Vacuum brazing of TZM alloy to ZrC particle reinforced W composite using Ti-28Ni eutectic brazing alloy

G.H. Han, Y.F. Wang, H.Y. Zhao, X.G. Song, J. Cao, J.C. Feng

Publisher page

Abstract

Abstract Reliable brazing of TZM alloy and ZrC particle reinforced (ZrC p ) W composite was achieved in this study by using Ti-28Ni eutectic brazing alloy. The typical interfacial microstructure of TZM/Ti-28Ni/ZrC p -W brazed joint consisted of a Ti solid solution (Ti(s, s)) layer, a continuous Ti 2 Ni layer and a diffusion layer mainly composed of W particles and (Ti, Zr)C particles. With an increase of brazing temperature, more ZrC particles and W particles entered the molten brazing alloy, which broadened the brazing seam and diminished the Ti 2 Ni layer, resulting in the disappearance of the Ti 2 Ni layer eventually. Meanwhile, more Ti(s, s) stripes were observed on the TZM side. The presence of continuous Ti 2 Ni intermetallic phase and Ti(s, s) stripes structure in joints deteriorated the joining properties, which resulted in the formation of brittle fracture under shear test. In addition, the fracture path was related to the brazing temperature, and cracks initiate and propagate in the continuous Ti 2 Ni layer at lower temperatures. However, the fracture path tended to be located at the TZM substrate close to the interface between TZM and the brazing seam when the brazing temperature exceeded 1040 °C. The optimal room temperature shear strength reached 120.5 MPa when brazed at 1040 °C for 10 min and the fracture surface exhibited cleavage fracture characteristics, and the shear strength at high temperature of 800 °C for the specimens with highest shear strength at room temperature reached 77.5 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Effects of strain rate on tensile properties of TZM and Mo-5%Re10.1016/S0022-3115(02)01191-1 ↗
2. Preparation of nanostructured high-temperature TZM alloy by mechanical alloying and sintering10.1016/j.ijrmhm.2010.09.003 ↗
3. The mechanical properties and fracture mechanisms of wrought low carbon arc cast (LCAC), molybdenum-0.5pct titanium-0.1pct zirconium (TZM), and oxide dispersion strengthened (ODS) molybdenum flat products10.1016/j.msea.2005.11.030 ↗
4. The change in the hardness of LCAC, TZM, and ODS molybdenum in the post-irradiated and annealed conditions10.1016/j.jnucmat.2009.04.025 ↗
5. Preparation of TZM alloy by aluminothermic smelting and its characterization10.1016/j.jallcom.2004.09.055 ↗
6. Microstructure and mechanical properties of ZrCW matrix composite prepared by reactive infiltration at 1300°C10.1016/j.ijrmhm.2012.10.014 ↗
7. The comparison of W/Cu and W/ZrC composites fabricated through hot-press10.1016/j.ijrmhm.2010.04.006 ↗
8. Effect of heat treatment on microstructure and mechanical properties of ZrC particles reinforced tungsten-matrix composites10.1016/j.msea.2009.01.078 ↗
9. The mechanical and thermophysical properties of ZrC/W composites at elevated temperature10.1016/S0921-5093(01)01802-0 ↗
10. Near net-shape/net-dimension ZrC/W-based composites with complex geometries via rapid prototyping and displacive compensation of porosity10.1016/j.jeurceramsoc.2010.01.011 ↗
11. Brazing high Nb containing TiAl alloy using Ti–28Ni eutectic brazing alloy: interfacial microstructure and joining properties10.1016/j.msea.2015.03.108 ↗
12. Study of brazing Ti-6Al-4V and TZM alloy using pure silver10.1023/B:JMSL.0000004642.79837.d1 ↗
13. The microstructural observation of brazing Ti-6Al-4V and TZM using the BAg-8 braze alloy10.1016/j.ijrmhm.2003.11.002 ↗
14. Microstructural evolution of brazing Ti–6Al–4V and TZM using silver-based braze alloy10.1016/j.matlet.2003.09.007 ↗
15. Brazing of Mo and Nb using two active braze alloys10.1016/j.msea.2004.08.027 ↗
16. Brazing of Mo to a CuZr alloy for the production of bimetallic raw materials for the CLIC accelerating structures10.1016/j.jmatprotec.2010.01.010 ↗
17. Interfacial microstructure and joining properties of titanium-zirconium-molybdenum alloy joints brazed using Ti-28Ni eutectic brazing alloy10.1016/j.msea.2015.12.009 ↗
18. Infrared brazing of Mo using the 70Au–22Ni–8Pd alloy[J]10.1016/j.ijrmhm.2004.10.003 ↗
19. The active metal brazing of TZM-Mo and SiN ceramics10.1007/BF03221364 ↗
20. Analysis of the brazeability of W-W joints using a high temperature Ni-based alloy10.1016/j.matdes.2013.08.106 ↗
21. Investigation of brazing structure of bulk graphite to a W-Re substrate10.1016/S1044-5803(00)00062-0 ↗
22. Study of a novel brazing process for W-W joints in fusion applications10.1016/j.matdes.2016.09.067 ↗
23. Wettability study of a Cu-Ti alloy on tungsten and EUROFER substrates for brazing components of DEMO fusion reactor10.1016/j.matdes.2016.03.054 ↗
24. Interfacial reaction evolution of the ZrC ceramic joint diffusion bonded with Ni interlayer10.1016/j.ceramint.2014.04.163 ↗
25. Homogenization of the zirconium carbide-titanium interface domain10.1016/j.scriptamat.2015.09.006 ↗
26. Electroplating assisted diffusion bonding of ZrC-SiC composite for full ceramic joints10.1016/j.ceramint.2013.12.013 ↗
27. Microstructure evolution and its effect on the mechanical properties of the ZrC-SiC composite joint diffusion bonded with pure Ni foil10.1016/j.ceramint.2013.04.074 ↗
28. Massalski · 1990
29. Microstructure and mechanical properties of hot-pressed ZrC–Ti–CNTs composites10.1016/j.matdes.2016.06.070 ↗
30. The effect of low-dose neutron irradiation on mechanical properties, electrical resistivity and fracture of NiAl bronze for ITER10.1016/j.jnucmat.2007.03.262 ↗
31. Dislocation behavior in ZrC particles during elevated temperature compressive deformation of a 30vol.% ZrCp/W composite10.1016/S1005-0302(11)60107-2 ↗
32. Villars · 1995
33. Spark plasma sintering of TiC-ZrC composites10.1016/j.ceramint.2015.02.019 ↗
34. Mechanical properties of nanocrystalline TiC–ZrC solid solutions fabricated by spark plasma sintering10.1016/j.ceramint.2014.03.024 ↗