Enhanced strength-ductility synergy in Ag-1wt%Cu alloys via nano-precipitation

Xin Li, Qi Tang, Shiqi Li, Ke Tang, Jinghong Chen, Yunxiu Chao, Ming Wen, Xizhang Chen

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (85)

Show source-provided references
1. The tensile behaviors of Ag-Cu alloys with different cu contents: molecular dynamics simulations study
2. Microstructure evolution and multi-reinforcement mechanisms in Al-Cu-Ag alloys10.1016/j.jallcom.2024.174852 ↗
3. Oxidation behavior of Cu–Ag alloy in-situ manufactured via laser powder bed fusion
4. The competing crystalline and amorphous solid solutions in the Ag–Cu system10.1016/S1359-6454(01)00374-3 ↗
5. Introduction of pressure in binary phase diagram calculations. Application to the Ag–Cu system
6. Experimental investigation and modeling of the influence of microstructure on the resistive conductivity of a Cu–Ag–Nb in situ composite10.1016/S1359-6454(99)00026-9 ↗
7. Microstructural evolution and mechanical properties of a two-phase Cu–Ag alloy processed by high-pressure torsion to ultrahigh strains10.1016/j.actamat.2011.01.017 ↗
8. Microstructure evolution and properties of Cu–Ag microcomposites with different ag content10.1016/j.msea.2006.07.125 ↗
9. Competition between precipitation and dissolution in Cu–Ag alloys under high pressure torsion10.1016/j.actamat.2016.09.024 ↗
10. Influence of thermomechanical process and fe addition on microstructural evolution and properties of Cu-26 wt% ag composite10.1016/j.jallcom.2018.09.179 ↗
11. Microstructure and tensile properties of nanostructured Cu-25wt%10.1016/S1359-6454(02)00468-8 ↗
12. Annealing effects on the microstructure, strength, and electrical resistivity in a dual-phase Cu-15 wt% ag alloy10.1016/j.msea.2022.143004 ↗
13. Annealing behaviour of cold-rolled Cu–Ag alloy under mechanical loads10.1080/02670836.2017.1412006 ↗
14. Wear resistance of Cu/Ag multilayers: a microscopic study10.1021/acsami.8b03015 ↗
15. Microstructural evolution and current-carrying tribological performance of an Ag-Cu alloy subjected to surface severe plastic deformation10.1016/j.jmst.2025.01.053 ↗
16. Review of nano-phase effects in high strength and conductivity copper alloys10.1515/ntrev-2019-0034 ↗
17. Microstructural characteristics of a nanoeutectic Ag–Cu alloy processed by surface mechanical attrition treatment10.1016/j.scriptamat.2012.11.033 ↗
18. Production of copper and copper alloy powders
19. Cu–Ag alloy for engineering properties and applications based on the LSPR of metal nanoparticles10.1039/D0RA01474E ↗
20. Micro-structure and properties of Cu-0.5 wt% ag alloy fine wires with severe cold plastic deformation treatment
21. Influence of hot isostatic pressing and forging on the microstructure and mechanical properties of Cu-3Ag-1Zr alloys10.1016/j.matdes.2019.107676 ↗
22. Tensile deformation and fracture behaviours of cold rolled Cu-3wt% Ag-0.5 wt% zr thin sheets with different annealed microstructures10.1016/j.msea.2019.04.038 ↗
23. Aging properties studies in a Cu–Ag–Cr alloy10.1016/j.msea.2005.09.118 ↗
24. A new grain orientation spread approach to analyze the dynamic recrystallization behavior of a cast-homogenized Mg-Zn-Zr alloy using electron backscattered diffraction10.1016/j.msea.2017.10.062 ↗
25. An electron backscattered diffraction study on the dynamic recrystallization behavior of a nickel–chromium alloy (800H) during hot deformation10.1016/j.msea.2013.07.037 ↗
26. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
27. Strengthening mechanism of CrCoNi medium-entropy alloy from the partially recrystallized structure to the fully recrystallized heterogeneous structure10.1016/j.matchar.2022.111795 ↗
28. Aging induced segregation and nanoprecipitation in a severely deformed equiatomic high-entropy alloy10.1016/j.matchar.2020.110369 ↗
29. Hierarchical microstructure design to tune the mechanical behavior of an interstitial TRIP-TWIP high-entropy alloy10.1016/j.actamat.2018.10.017 ↗
30. Rollett, Anthony, Rohrer, G.S., Humphreys, Recrystallization and Related Annealing Phenomena, Elsevier Science.
31. The role of disconnections in deformation-coupled grain boundary migration10.1016/j.actamat.2014.05.062 ↗
32. Ultrafine-grained dual phase Al0. 45CoCrFeNi high-entropy alloys10.1016/j.matdes.2019.107910 ↗
33. Microstructure tailoring of Al0. 5CoCrFeMnNi to achieve high strength and high uniform strain using severe plastic deformation and an annealing treatment10.1016/j.jmst.2020.07.017 ↗
34. Microstructure and properties of Ag-1.33% Mg-0.54% ni alloy after severe plastic deformation and internal oxidation10.1016/S1875-5372(13)60033-8 ↗
35. Mechanistic insights into cluster strengthening and grain refinement toughening in fully oxidized AgMgNi alloys10.1016/j.jmst.2024.10.030 ↗
36. Concurrent toughening and hardening in AgMgNi alloys by internal oxidation
37. Bulk eutectic Cu–Ag alloys with abundant twin boundaries10.1016/j.scriptamat.2011.09.024 ↗
38. Microstructures, strengthening mechanisms and fracture behavior of Cu–Ag alloys processed by high-pressure torsion10.1016/j.actamat.2011.09.058 ↗
39. Simultaneously increasing strength and electrical conductivity in nanostructured Cu–Ag composite10.1016/j.msea.2015.11.067 ↗
40. Effect of ag content and drawing strain on microstructure and properties of directionally solidified Cu-Ag alloy10.1016/j.vacuum.2018.05.010 ↗
41. Microstructural evolution and properties of Cu–20 wt% ag alloy wire by multi-pass continuous drawing10.1515/ntrev-2020-0108 ↗
42. Mechanical and electrical responses of nanostructured Cu–3 wt% ag alloy fabricated by ECAP and cold rolling10.1016/j.jallcom.2010.02.198 ↗
43. Microstructure and properties of Cu-Ag alloy prepared by continuously directional solidification10.1016/j.jallcom.2021.160769 ↗
44. Comparison of microstructures and mechanical properties of a Cu–Ag alloy processed using different severe plastic deformation modes10.1016/j.msea.2011.01.057 ↗
45. Evolution of microstructure and properties of Cu-4.5 wt% ag alloy prepared by vacuum horizontal continuous casting in solid solution and aging treatment10.1088/2053-1591/abd217 ↗
46. Effects of route on microstructural evolution and mechanical properties of Cu-8 wt pct ag alloy processed by equal channel angular pressing10.1007/s11661-010-0313-4 ↗
47. An intrinsic construction model of BN Cu-Ag alloy for predicting its mechanical properties10.1007/s11837-022-05606-4 ↗
48. Effect of large deformation on microstructure and properties of copper alloy wire10.1016/j.jmrt.2024.02.153 ↗
49. Effects of strain rates on dynamic deformation behavior of Cu-20Ag alloy10.1016/j.jmst.2020.11.043 ↗
50. Mechanisms for high strength and ultra-high electrical conductivity of Cu-3.5 wt% ag alloy prepared by thermomechanical treatment
51. Microstructural stability and mechanical response of Cu–Ag microcomposite wires10.1016/S1359-6454(98)00106-2 ↗
52. Mechanical stability and electrical conductivity of Cu–Ag filamentary microcomposites10.1016/S0921-5093(98)01097-1 ↗
53. Evolution of microstructure and property alterations in Cu-Ag-Cr alloy under rolling deformation10.1016/j.msea.2024.147768 ↗
54. Effect of cr addition on the microstructure evolution, precipitation behavior and properties of Cu–Ag alloy10.1016/j.msea.2024.146186 ↗
55. Optimizing mechanical and electrical properties of a nanostructured Cu-Ag alloy by aging at low temperatures10.1016/j.msea.2024.147588 ↗
56. Refinement of eutectic structure and precipitates of Cu–20Ag alloy due to y microalloying10.1016/j.jmrt.2024.10.179 ↗
57. Effect of la addition on Ag-rich phase formation and mechanical properties of Cu-2Ag alloys10.1016/j.jmrt.2022.03.020 ↗
58. Mechanisms of primary phase refinement and toughness improvement of Cu–2 wt% Ag–0.15 wt% la alloy through continuous extrusion forming10.1016/j.msea.2021.141521 ↗
59. Microstructural evolution and strengthening mechanisms in cold-rolled Cu–Ag alloys10.1016/j.jallcom.2020.156893 ↗
60. High tensile ductility via enhanced strain hardening in ultrafine-grained cu10.1016/j.msea.2011.10.070 ↗
61. Microstructure, mechanical properties and electrical conductivity of industrial Cu–0.5% cr alloy processed by severe plastic deformation10.1016/j.msea.2010.10.059 ↗
62. Fabrication of ultrafine-grained Cu-Mn alloy with uniform microstructure and high mechanical properties10.1016/j.matchar.2023.113270 ↗
63. Effect of deformation methods on microstructure, texture, and properties of a Cu–Mg alloy10.1016/j.msea.2023.145126 ↗
64. Deformation microstructures, strengthening mechanisms, and electrical conductivity in a Cu–Cr–Zr alloy10.1016/j.msea.2015.01.065 ↗
65. Grain refinement kinetics and strengthening mechanisms in Cu–0.3 Cr–0.5 zr alloy subjected to intense plastic deformation10.1016/j.msea.2015.12.038 ↗
66. Effect of friction-stir processing and subsequent aging treatment on microstructure and service properties of Cu-Cr-Zr alloy10.1016/j.matchar.2024.114225 ↗
67. Enhanced electrical, mechanical and tribological properties of Cu-Cr-Zr alloys by continuous extrusion forming and subsequent aging treatment10.1016/j.jmst.2021.10.012 ↗
68. Enhancing the strength and conductivity of commercialized Cu-Cr-Zr plate through simple high strain cold rolling and aging10.1016/j.matchar.2023.113213 ↗
69. Effect mechanism of nb addition on grain refinement and inhibition of discontinuous precipitation of Cu–15Ni–8Sn alloy10.1016/j.jmrt.2024.08.209 ↗
70. Effects of rare earth ce addition on microstructure and mechanical properties of impure copper containing pb10.1016/S1003-6326(20)65320-1 ↗
71. Excellent mechanical properties and high electrical conductivity of Cu-Co-Si-Ti alloy due to multiple strengthening10.1016/j.msea.2021.141639 ↗
72. Influence of thermomechanical treatment on recrystallization and softening resistance of cu− 6.5 fe− 0.3 mg alloy10.1016/S1003-6326(24)66584-2 ↗
73. Grain size control method for enhancing high-temperature durability of Al–Cu–Mg–Ag alloy10.1016/j.jmrt.2024.06.017 ↗
74. Improved stress relaxation stability of a heat-resistant Al-Cu-Mg-Ag alloy with good mechanical properties by a pre-annealing/solution-aging treatment10.1016/j.jallcom.2023.171145 ↗
75. Insights into precipitation characteristics and strengthening mechanisms in a low Cu/Mg ratio Al-Cu-Mg-Ag alloy10.1016/j.matdes.2024.112836 ↗
76. Effect of v additions on the microstructure and mechanical properties of Al-Cu-Mg-Ag alloy
77. Minimizing porosity and optimizing microstructure of hot-wire arc additive manufactured Al-Cu-Mg-Ag alloy for strength increment10.1016/j.jmapro.2024.03.053 ↗
78. On the precipitation behaviour in Al–Cu-Mg-(Ag) alloys processed by equal-channel angular pressing10.1016/j.msea.2024.147650 ↗
79. Effect of small sn addition on the initial strengthening and microstructural evolution of an Al-Cu-Mg-Ag alloy10.1016/j.jallcom.2023.169167 ↗
80. Development of ternary Ti-Ag-Cu alloys with excellent mechanical properties and antibiofilm activity10.3390/ma15249011 ↗
81. Strengthening mechanisms in a high-strength bulk nanostructured Cu–Zn–Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
82. Multi-component solid solution hardening: part 2 agreement with experimental results10.1007/BF00540988 ↗
83. A statistical theory of solid solution hardening10.1002/pssb.19700410221 ↗
84. Hierarchical grain size and nanotwin gradient microstructure for improved mechanical properties of a non-equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.jmst.2021.02.059 ↗
85. Designing ultra-strong and ductile hierarchical titanium alloys via interstitial solute-mediated multi-morphologic α-nanoprecipitates10.1016/j.actamat.2023.119082 ↗