journal article·2026-07-31

Microstructures, Mechanical Properties and Corrosion Resistance of Mg-1.5Zn-0.3Mn-xY (0 ≤ x ≤ 4.0 wt.%) Alloys through Continuous Variable Cross-Section Extrusion

Huai Yao, Xueying Zhang, Yanchun Zhao, Yanfeng Zhu, Marko Huttula, Wei Cao

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. N. Zhang, M. Liu, Q. Li, X. Chen, and Z. Zheng, Effect of Long-period Stacking Ordered Phase on Dynamic Recrystallization in Mg-Y-Zn-Zr Alloy Processed by Backward Extrusion, J. Mater. Res. Technol., 2023, 26, p 2384–2393. https://doi.org/10.1016/j.jmrt.2023.08.08910.1016/j.jmrt.2023.08.089 ↗
2. M. Yamasaki, Z. Shi, A. Atrens, A. Furukawa, and Y. Kawamura, Influence of Crystallographic Orientation and Al Alloying on the Corrosion Behaviour of Extruded α-Mg/LPSO Two-Phase Mg-Zn-Y Alloys with Multimodal Microstructure, Corros. Sci., 2022, 200, p 110237. https://doi.org/10.1016/j.corsci.2022.11023710.1016/j.corsci.2022.110237 ↗
3. D. Zhao, X. Chen, W. Ci, C. Liu, and F. Pan, Effect of Al Element on Microstructure, Mechanical Properties and Damping Capacity of LPSO-Containing Mg-Y-Zn-Li Alloy, Mater Charact, 2024, 207, p 113542. https://doi.org/10.1016/j.matchar.2023.11354210.1016/j.matchar.2023.113542 ↗
4. G.G. Wang, G.S. Huang, X. Chen, Q.Y. Deng, A.T. Tang, B. Jiang, and F.S. Pan, Effects Zn Addition on the Mechanical Properties and Texture of Extruded Mg-Zn-Ca-Ce Magnesium Alloy Sheets, Mater. Sci. Eng. A, 2017, 705, p 46–54. https://doi.org/10.1016/j.msea.2017.08.03610.1016/j.msea.2017.08.036 ↗
5. T. Morishige, Y. Obata, T. Goto, T. Fukagawa, E. Nakamura, and T. Takenaka, Effect of Al Composition on the Corrosion Resistance of Mg-14 Mass% Li System Alloy, Mater. Trans., 2016, 57, p 1853–1856. https://doi.org/10.2320/matertrans.M201624710.2320/matertrans.M2016247 ↗
6. C.C. Li, Z.H. Xia, X.G. Qiao, I.S. Golovin, and M.Y. Zheng, Superior Ductility Mg-Mn Extrusion Alloys at Room Temperature Obtained by Controlling Mn Content, Mater. Sci. Eng. A, 2023, 869, p 144508. https://doi.org/10.1016/j.msea.2022.14450810.1016/j.msea.2022.144508 ↗
7. G.N. Zhu, Z. Wang, W.Y. Qiu, Y. Zhou, L. Zhou, F. Wang, Z. Liu, and P.L. Mao, Effect of Yttrium on Hot Tearing Susceptibility of Mg-6Zn-1Cu-0.6Zr Alloys, Int. J. Met., 2019, 14, p 179–190. https://doi.org/10.1007/s40962-019-00352-x10.1007/s40962-019-00352-x ↗
8. J. Tian, J.F. Deng, Y.C. Zhou, Y.Y. Chang, W. Liang, and J.Y. Ma, Slip Behavior during Tension of Rare Earth Magnesium Alloys Processed by Different Rolling Methods, J. Mater. Res. Technol., 2023, 22, p 473–488. https://doi.org/10.1016/j.jmrt.2022.11.10210.1016/j.jmrt.2022.11.102 ↗
9. J.W. Dai, Q.S. Dong, Y.J. Nie, Y.Q. Jia, C.L. Chu, and X.B. Zhang, Insight into the Role of Y Addition in the Microstructures, Mechanical and Corrosion Properties of As-Cast Mg-Gd-Y-Zn-Ca-Zr Alloys, Mater. Des., 2022, 221, p 110980. https://doi.org/10.1016/j.matdes.2022.11098010.1016/j.matdes.2022.110980 ↗
10. Y.Q. Li, F. Li, F.W. Kang, H.Q. Du, and Z.Y. Chen, Recent Research and Advances in Extrusion Forming of Magnesium Alloys: A Review, J. Alloy. Compd., 2023, 953, p 170080. https://doi.org/10.1016/j.jallcom.2023.17008010.1016/j.jallcom.2023.170080 ↗
11. Y.J. Ma, C.M. Liu, Y.J. Huang, S.N. Jiang, Y.H. Gao, Y.C. Wan, and Z.Y. Chen, Effect of Extrusion Parameters on Microstructure, Mechanical Properties and Damping Capacities of Mg-Y-Zn-Zr Alloy, J. Alloy. Compd., 2023, 935, p 168122. https://doi.org/10.1016/j.jallcom.2022.16812210.1016/j.jallcom.2022.168122 ↗
12. T.S. Zhao, Q.Y.T. Zhang, R. Wang, J.L. Wu, Y.B. Hu, B. Jiang, and F.S. Pan, Achieving High Strength-Ductility Synergy in Mg-Gd-Zn-Zr Alloy by Controlling Extrusion Processes Parameters, Mater. Sci. Eng. A, 2024, 916, p 147342. https://doi.org/10.1016/j.msea.2024.14734210.1016/j.msea.2024.147342 ↗
13. F.N. Xu, L.A. Tian, N. Li, N. Ding, L. Liu, H.X. Xu, and J.X. Zhou, Effect of Extrusion Temperature on Microstructure and Mechanical Properties of ZTM631 Magnesium Alloy, Mater. Today Commun., 2024, 39, p 108845. https://doi.org/10.1016/j.mtcomm.2024.10884510.1016/j.mtcomm.2024.108845 ↗
14. Y.H. Guo, X.C. He, Y.B. Dai, H.F. Xiang, Q.H. Zang, F.J. Shi, X.G. Dong, and Z.Y. Zhang, Microstructures and Mechanical Properties of Mg-5LI-4Sn-2Al-1Zn Alloy After Hot Extrusion, Mater. Sci. Eng. A, 2022, 860, p 144329. https://doi.org/10.1016/j.msea.2022.14432910.1016/j.msea.2022.144329 ↗
15. Z. Zeng, N. Stanford, C.H.J. Davies, J. Nie, and N. Birbilis, Davies, Magnesium Extrusion Alloys: A Review of Developments and Prospects, Int. Mater. Rev., 2019, 64, p 27–62. https://doi.org/10.1080/09506608.2017.142143910.1080/09506608.2017.1421439 ↗
16. H. Zengin and Y. Turen, Effect of Y Addition on Microstructure and Corrosion Behavior of Extruded Mg-Zn-Nd-Zr Alloy, J. Magnes. Alloy., 2020, 8, p 640–653. https://doi.org/10.1016/j.jma.2020.06.00410.1016/j.jma.2020.06.004 ↗
17. N. Uemura, S. Singhaneka, and R. Matsumoto, First-Principles Study of Generalized Stacking Fault Energy in Mg-Zn-Y Alloy with Long-Period Stacking-Ordered Structures, Mater. Trans., 2024, 65, p 1080–1088. https://doi.org/10.2320/matertrans.MT-M202405610.2320/matertrans.MT-M2024056 ↗
18. M.S. Geshani, P.M. Kalayeh, A.H. Asadi, H. Mirzadeh, M. Malekan, and M. Emamy, A Review of Mg Alloys Containing Long-Period Stacking Ordered (LPSO) Structures with Insight into the Application of Friction Stir Processing, J. Mater. Res. Technol., 2023, 24, p 4945–4966. https://doi.org/10.1016/j.jmrt.2023.04.10510.1016/j.jmrt.2023.04.105 ↗
19. S. Najafi, Y. Palizdar, A. Sheikhani, M.S.A. Nezhad, F. Abdiyan, S.M. Banijamali, and H. Torkamani, The Effect of Y Addition on the Microstructure and Work Hardening Behavior of Mg-Zn-Zr Alloys, J. Mater. Eng. Perform., 2021, 30, p 2574–2585. https://doi.org/10.1007/s11665-021-05592-910.1007/s11665-021-05592-9 ↗
20. W.Z. Chen, W.C. Zhang, L.X. Zhang, and E.D. Wang, Property Improvements in Fine-Grained Mg-Zn-Zr Alloy Sheets Produced by Temperature-Step-Down Multi-pass Rolling, J. Alloy. Compd., 2015, 646, p 195–203. https://doi.org/10.1016/j.jallcom.2015.06.11210.1016/j.jallcom.2015.06.112 ↗
21. S. Liu, K. Zhang, C. Wang, D.W. Wang, M.X. Li, Y.J. Yang, K. Guan, A. Volochko, and H.Y. Wang, Dramatic Enhancement of the Corrosion Resistance of Dilute Mg-Al-Mn-Ca Alloy through Gd Alloying, Corros. Sci., 2024, 238, p 112351. https://doi.org/10.1016/j.corsci.2024.11235110.1016/j.corsci.2024.112351 ↗
22. Z.L. Li, Z.Z. Shi, W.L. Cai, J.Y. Wang, X.J. Ji, F.Z. Dai, X.F. Gu, and L.N. Wang, Novel Cast Mg-Ga-Li Alloys with Excellent Strength-Ductility Balance and Corrosion Resistance, J. Alloy. Compd., 2025, 1026, p 180460. https://doi.org/10.1016/j.jallcom.2025.18046010.1016/j.jallcom.2025.180460 ↗
23. W.J. Ci, Q. Tao, X.H. Chen, C. Blawert, M. Serdechnova, C. Song, S. Yuan, F.S. Pan, and M.L. Zheludkevich, Enhancing Corrosion Resistance of Mg-Nd-Zr-In Alloys via the Development of a Triple‑Layered In (Indium) Rich Corrosion Product Film, Corros. Sci., 2025, 250, p 112905. https://doi.org/10.1016/j.corsci.2025.11290510.1016/j.corsci.2025.112905 ↗
24. Y.C. Shi, C.Q. Peng, Y. Feng, R.C. Wang, and N.G. Wang, Microstructure and Electrochemical Corrosion Behavior of Extruded Mg-Al-Pb-La Alloy as Anode for Seawater‑Activated Battery, Mater. Des., 2017, 124, p 24–33. https://doi.org/10.1016/j.matdes.2017.03.05810.1016/j.matdes.2017.03.058 ↗
25. Y. Liu, J.B. Wen, J.G. He, and H. Li, Enhanced Mechanical Properties and Corrosion Resistance of Biodegradable Mg-Zn-Zr-Gd Alloy by Y Microalloying, J. Mater. Sci., 2020, 55, p 1813–1825. https://doi.org/10.1007/s10853-019-04026-110.1007/s10853-019-04026-1 ↗
26. P.F. Fei, Z.K. Qu, and R.Z. Wu, Microstructure and Hardness of Mg-9Li-6Al-xLa (x=0, 2, 5) Alloys during Solid Solution Treatment, Mater. Sci. Eng. A, 2015, 625, p 169–176. https://doi.org/10.1016/j.msea.2014.12.01410.1016/j.msea.2014.12.014 ↗
27. K. Huang and R.E. Logé, A Review of Dynamic Recrystallization Phenomena in Metallic Materials, Mater. Des., 2016, 111, p 548–574. https://doi.org/10.1016/j.matdes.2016.09.01210.1016/j.matdes.2016.09.012 ↗
28. B. Smola, I. Stulíková, J. Pelcová, and B.L. Mordike, Significance of Stable and Metastable Phases in High Temperature Creep Resistant Magnesium-Rare Earth Base Alloys, J. Alloy. Compd., 2004, 378, p 196–201. https://doi.org/10.1016/j.jallcom.2023.10.09910.1016/j.jallcom.2023.10.099 ↗
29. W.T. Sun, X.G. Qiao, M.Y. Zheng, C. Xu, N. Gao, and M.J. Starink, Microstructure and Mechanical Properties of a Nanostructured Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr Supersaturated Solid Solution Prepared by High Pressure Torsion, Mater. Des., 2017, 135, p 366–376. https://doi.org/10.1016/j.matdes.2017.09.04810.1016/j.matdes.2017.09.048 ↗
30. H.Y. Yu, H.G. Yan, J.H. Chen, B. Su, Y. Zheng, Y.J. Shen, and Z.J. Ma, Effect of Minor Gd Addition on Microstructures and Mechanical Properties of the High Strain-Rate Rolled Mg-Zn-Zr Alloys, J. Alloy. Compd., 2014, 586, p 757–765. https://doi.org/10.1016/j.jallcom.2013.10.00510.1016/j.jallcom.2013.10.005 ↗
31. R.Q. Lu, Z.M. Xu, F.L. Jiang, S.W. Xu, D.F. Fu, H. Zhang, and J. Teng, Revealing the Grain Size Dependent Hot Workability and Deformation Mechanisms in a Mg-Zn-Y Alloy, J. Magnes. Alloy., 2023, 11, p 1461–1471. https://doi.org/10.1016/j.jma.2021.08.00110.1016/j.jma.2021.08.001 ↗
32. J. Luo, H. Yan, R.S. Chen, and E.H. Han, Effects of Gd Concentration on Microstructure, Texture and Tensile Properties of Mg-Zn-Gd Alloys Subjected to Large Strain Hot Rolling, Mater. Sci. Eng. A, 2014, 614, p 88–95. https://doi.org/10.1016/j.msea.2014.06.11010.1016/j.msea.2014.06.110 ↗
33. W.H. Liu, J.X. Bao, M.L. Qiao, S.Q. Yin, Z.K. Wang, J.Z. Cui, and Z.Q. Zhang, Microstructures and Mechanical Properties of Mg-6Zn-1Y-0.85Zr Alloy Prepared at Different Extrusion Temperatures and Speeds, J. Mater. Res. Technol., 2022, 21, p 1042–1052. https://doi.org/10.1016/j.jmrt.2022.09.09610.1016/j.jmrt.2022.09.096 ↗
34. Z.N. Ma, M. Jiang, and L. Wang, First-Principles Study of Electronic Structures and Phase Stabilities of Ternary Intermetallic Compounds in the Mg-Y-Zn Alloys, Acta Phys. Sin., 2015, 64, p 187102. https://doi.org/10.7498/aps.64.18710210.7498/aps.64.187102 ↗
35. J.W. Seong and W.J. Kim, Development of Biodegradable Mg-Ca Alloy Sheets with Enhanced Strength and Corrosion Properties through the Refinement and Uniform Dispersion of the Mg2Ca Phase by High-Ratio Differential Speed Rolling, Acta Biomater., 2015, 11, p 531–542. https://doi.org/10.1016/j.actbio.2014.09.02910.1016/j.actbio.2014.09.029 ↗
36. R. Labusch, A Statistical Theory of Solid Solution Hardening, Phys. Status Solidi, 1970, 41, p 659–669. https://doi.org/10.1002/PSSB.1970041022110.1002/PSSB.19700410221 ↗
37. X.Y. Qian, Y. Zeng, B. Jiang, Q.R. Yang, Y.J. Wan, G.F. Quan, and F.S. Pan, Grain Refinement Mechanism and Improved Mechanical Properties in Mg-Sn Alloy with Trace Y Addition, J. Alloy. Compd., 2020, 820, p 153122. https://doi.org/10.1016/j.jallcom.2019.15312210.1016/j.jallcom.2019.153122 ↗
38. N. Su, Q.Y. Wu, C.Y. Ding, Y.J. Wu, and L.M. Peng, Effect of Y and Gd Solutes on Grain Refinement of the As-Extruded Mg-Gd-(-Y)-Zn-Mn Alloys, J. Alloy. Compd., 2023, 968, p 171804. https://doi.org/10.1016/j.jallcom.2023.17180410.1016/j.jallcom.2023.171804 ↗
39. S.C. Jin, J.W. Cha, H.J. Kim, J.H. Lee, H. Yu, and S.H. Park, Improved Mechanical Properties of High-Speed Extruded BA53 Alloy through Long-Range Water-Cooling System, J. Mater. Res. Technol., 2024, 28, p 4363–4369. https://doi.org/10.1016/j.jmrt.2024.01.02810.1016/j.jmrt.2024.01.028 ↗
40. H.C. Pan, R. Kang, J.R. Li, H.B. Xie, Z.R. Zeng, Q.Y. Huang, C.L. Yang, Y.P. Ren, and G.W. Qin, Mechanistic Investigation of a Low-Alloy Mg-Ca–Based Extrusion Alloy with High Strength-Ductility Synergy, Acta Mater., 2020, 186, p 278–290. https://doi.org/10.1016/j.actamat.2020.01.01710.1016/j.actamat.2020.01.017 ↗
41. J.F. Nie, Effects of Precipitate Shape and Orientation on Dispersion Strengthening in Magnesium Alloys, Scripta Mater., 2003, 48, p 1009–1015. https://doi.org/10.1016/S1359-6462(02)00497-910.1016/S1359-6462(02)00497-9 ↗
42. L. Li, Y. Wang, C.C. Zhang, T. Wang, and H. Lv, Effect of Yb Concentration on Recrystallization, Texture and Tensile Properties of Extruded ZK60 Magnesium Alloys, Mater. Sci. Eng. A, 2020, 788, p 139609. https://doi.org/10.1016/j.msea.2020.13960910.1016/j.msea.2020.139609 ↗
43. D.H. Bae, S.H. Kim, D.H. Kim, and W.T. Kim, Deformation Behavior of Mg-Zn-Y Alloys Reinforced by Icosahedral Quasicrystalline Particles, Acta Mater., 2002, 50, p 2343–2356. https://doi.org/10.1016/S1359-6454(02)00067-810.1016/S1359-6454(02)00067-8 ↗
44. X.Y. Liu, X.W. Li, Q.B. Liu, Q.L. Ren, Y.F. Liu, and J.H. Wang, Investigation of the Impact of Trace Y Addition on Mechanical Properties, Microstructure and Fracture Behavior of Mg-4Al-2.5Ce-1.5La-0.3Mn-xY (x=0, 0.1, 0.2, 0.5 wt.%) Alloys, Mater. Today Commun., 2024, 38, p 108153. https://doi.org/10.1016/j.mtcomm.2024.10815310.1016/j.mtcomm.2024.108153 ↗
45. P.L. Jiang, C. Blawert, R.Q. Hou, N. Scharnagl, J. Bohlen, and M.L. Zheludkevich, Microstructural Influence on Corrosion Behavior of MgZnGe Alloy in NaCl Solution, J. Alloy. Compd., 2019, 783, p 179–192. https://doi.org/10.1016/j.jallcom.2018.12.29610.1016/j.jallcom.2018.12.296 ↗
46. D.X. Liu, C.G. Guo, L.Q. Chai, V.R. Sherman, X.Q. Qin, Y.T. Ding, and M.A. Meyers, Mechanical Properties and Corrosion Resistance of Hot Extruded Mg-2.5Zn-1Ca Alloy, Mater. Sci. Eng. B, 2015, 195, p 50–58. https://doi.org/10.1016/j.mseb.2015.02.00110.1016/j.mseb.2015.02.001 ↗
47. Z.M. Shi, M. Liu, and A. Atrens, Measurement of the Corrosion Rate of Magnesium Alloys using Tafel Extrapolation, Corros. Sci., 2010, 52, p 579–588. https://doi.org/10.1016/j.corsci.2009.10.01610.1016/j.corsci.2009.10.016 ↗