Performance criteria for concrete subjected to freezing and thawing conditions (−22°C to 24°C, with 3.0% sodium chloride freezing medium) using a scaling test method from a European technical specification were investigated. A total of 57 concretes were considered, covering various binder types (Portland cement (CEM I) and combinations with fly ash, ground granulated blast-furnace slag (GGBS) and limestone), binder proportions, strength classes and non-air-entrained (NAE) and air-entrained (AE) concretes. Reduced scaling was generally noted for the NAE concretes with increasing strength, and between comparable-strength concretes when air entrainment was used. While the GGBS concretes generally showed improved performance compared with the other concretes, it was difficult to identify consistent trends in the data between them. Increasing the air content also mainly led to improvements, while the reverse occurred (in AE concretes) with increasing addition level. Cast faces generally performed less well than cut surfaces (according to the method in the European technical specification), although the effect noticeably reduced with air entrainment. The data for 28 freeze–thaw cycles suggests that, for NAE concrete meeting current prescribed requirements, a scaling limit of around 1.0 kg/m2 would apply. For AE concrete, the corresponding limit is less than 0.5 kg/m2. Other practical issues associated with applying performance criteria for specifying concrete are discussed.
Source: crossref · Quality: baseline
Affiliations
University of Dundee Concrete Technology Unit, School of Science and Engineering, , Scotland
References (59)
Show source-provided references
1. Relationship between cement composition and the freeze–thaw resistance of concretes10.1680/jadcr.17.00138 ↗
2. Freeze–thaw field exposure and testing the reliability of performance test temperature cycle for concrete scaling in presence of de-icing salts10.1617/s11527-021-01831-6 ↗
3. The case for air-entrainment in high-performance concrete10.1680/stbu.2005.158.5.311 ↗
4. Bilodeau · 1997 · 121
5. BSI (British Standards Institution) (1990) BS 5328-1:1990: Concrete – Guide to specifying concrete. BSI, London, UK.
6. BSI (2002) BS EN 12620:2002+A1:2008: Aggregates for concrete. BSI, London, UK.
7. BSI (2006a) BS 8500-1:2006+A1:2012: Concrete. Complementary British Standard to BS EN 206-1. Method of specifying and guidance for the specifier, BSI, London, UK.
8. BSI (2006b) PD CEN/TR 15177:2006: Testing the freeze-thaw resistance of concrete. Internal structural damage. BSI, London, UK.
9. BSI (2006c) BS EN 15167-1:2006: Ground granulated blast furnace slag for use in concrete, mortar and grout. Definitions, specifications and conformity criteria. BSI, London, UK.
10. BSI (2009a) BS EN 1367-2:2009: Tests for thermal and weathering properties of aggregates. Magnesium sulfate test. BSI, London, UK.
11. BSI (2009b) BS EN 934-2:2009: Concrete admixture definitions, requirements, conformity, marking and labelling. BSI, London, UK.
12. BSI (2011) BS EN 197-1:2011: Cement. Composition, specifications and conformity criteria for common cements. BSI, London, UK.
13. BSI (2012) BS EN 450-1:2012: Fly ash for concrete. Definition, specifications and conformity criteria.
14. BSI (2013a) BS EN 206:2013+A2:2021: Concrete. Specification, performance, production and conformity.
15. BSI (2013b) BS 1881-125:2013: Testing concrete. Methods for mixing and sampling fresh concrete in the laboratory. BSI, London, UK.
16. BSI (2016a) PD CEN/TS 12390-9:2016: Testing hardened concrete. Freeze-thaw resistance with de-icing salts. Scaling. BSI, London, UK.
17. BSI (2016b) BS 7979:2016: Specification for limestone fines for use with Portland cement, BSI, London, UK.
18. BSI (2019a) BS EN 12350-2:2019: Testing fresh concrete. Slump test. BSI, London, UK.
19. BSI (2019b) BS EN 12350-7:2019: Testing fresh concrete – Air content. Pressure methods. BSI, London, UK.
20. BSI (2019c) BS EN 12390-3:2019: Testing hardened concrete. Compressive strength of test specimens. BSI, London, UK.
21. BSI (2020) BS EN 1097-2:2020: Tests for mechanical and physical properties of aggregates. Methods for the determination of resistance to fragmentation. BSI, London, UK.
22. BSI (2023a) BS EN 1992-1-1:2023: Eurocode 2: Design of concrete structures – General rules and rules for buildings, bridges and civil engineering structures. BSI, London, UK.
23. BSI (2023b) BS 8500-1:2023: Concrete. Complementary British Standard to BS EN 206. Method of specifying and guidance for the specifierBSI, London, UK.
24. BSI (2023c) BS 8500-2:2023: Concrete. Complementary British Standard to BS EN 206. Specification for constituent materials and concrete. BSI, London, UK.
25. Influence of GGBS on durability and corrosion behavior of reinforced concrete10.1016/j.matchemphys.2005.03.043 ↗
26. British Standard for concrete
27. Concrete Society · 2019
28. Effect of the addition of GGBS on the frost scaling and chloride migration resistance of concrete10.3390/app10113940 ↗
29. The wet and stormy UK winter of 2019/202010.1002/wea.3955 ↗
30. Evaluation of Portland limestone cements for use in concrete construction10.1617/s11527-006-9143-7 ↗
31. A comprehensive review of concrete durability in freeze-thaw conditions: mechanisms, prevention, and mitigation strategies10.1016/j.istruc.2025.108804 ↗
32. Damage mechanism and modeling of concrete in freeze–thaw cycles: a review10.3390/buildings12091317 ↗
33. Harrison · 2001
34. Frost resistance of concrete with high contents of fly ash-A study on how hollow fly ash particles distort the air void analysis10.1016/j.cemconres.2019.02.013 ↗
35. Hawkins · 2005
36. Hooton RD , NokkenM and ThomasMDA (2007) Portland-Limestone Cement: State-of-the-Art Report and Gap Analysis for CSA A 3000. Cement Association of Canada, Ottawa, Canada.
37. Hynard C (2021) Evaluating CEN/TS 12390-9 to Assess Concrete for UK Freeze-Thaw Exposure Conditions. PhD thesis, University of Dundee, Dundee, UK.
38. Water-binder ratio influence on de-icing salt scaling of fly ash concretes10.1016/j.proeng.2013.04.104 ↗
39. Salt scaling resistance of variable w/c ratio air-entrained concretes modified with polycarboxylates as a proper consequence of air void system10.3390/ma15175839 ↗
40. Effect of fly ash on Portland cement systems part I. Low-calcium fly ash10.1016/S0008-8846(99)00153-2 ↗
41. Surface and internal deterioration of concrete due to saline and non-saline freeze–thaw loads10.1016/j.cemconres.2005.10.007 ↗
42. Surface microstructure and scaling resistance of concrete10.1016/0008-8846(96)00138-X ↗
43. Price · 2000
44. Blended cement according to ENV 197 and experiences in Germany10.1520/CCA10603J ↗
45. Setzer · 1997 · 3
46. Freeze–thaw damage and chemical change of a Portland cement concrete in the presence of diluted deicers10.1617/s11527-009-9557-0 ↗
47. Siebel · 1998
48. SIS (Swedish Institute for Standards) · 2019
49. Stark · 1997 · 123
50. Tang · 2004 · 754
51. Thomas · 1997 · 21
52. Thomas · 2017 · 121
53. Properties and behavior of limestone cement concrete and mortar10.1016/S0008-8846(00)00372-0 ↗
54. Mechanism for salt scaling of a cementitious surface10.1617/s11527-006-9104-1 ↗
55. A review of salt scaling: I. Phenomenology10.1016/j.cemconres.2007.03.005 ↗
56. Water UK (2021) Freeze-thaw 2020/21: Recommendations from an unprecedented winter. See Link to the cited article (accessed04/06/2026).
57. Scaling resistance and air void characteristics in concrete containing ggbs10.1515/ace-2015-0115 ↗
58. Global assessment of concrete specimens subjected to freeze-thaw damage10.1016/j.cemconcomp.2022.104716 ↗
59. De-icing salt scaling of concrete incorporating different types & percentages of fly ash