journal article·2025

Analysis of Sintering Curves, Microstructure, and Microhardness of the Cu-WC Composite

A.C. Marques, T.Q. Silva, K.F. Araújo, M.J. Lima, P.S. Vieira, C.S. Lourenço, M. Mashhadikarimi, U.U. Gomes

Materials Research· Volume 28· Issue suppl 1
Publisher page

Abstract

Composite materials have gained prominence due to their tailored properties for various applications. Cu-WC composites, combining a copper matrix with tungsten carbide reinforcement, are particularly valuable for electrical conductors and heat sinks. This study examined the sintering behavior of Cu-WC composite powder (10%WC) produced via High-Energy Ball Milling (HEBM) at 400 RPM for 2, 10, and 20 hours. The powders were compacted at 150 MPa and sintered at 900°C with a 1-hour isothermal hold. Sintering curves, microstructure, and Vickers microhardness were analyzed. The results showed that longer milling times led to significant powder expansion up to 750°C, followed by greater shrinkage due to diffusion mechanisms. Sintered samples milled for 10 hours displayed improved carbide distribution in the copper matrix. The highest microhardness was achieved at 20 hours of milling, attributed to refined microstructure. Extended milling times enhanced atomic diffusion during sintering, resulting in a more homogeneous structure and increased hardness.
Source: crossref · Quality: baseline

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Universidade Federal do Rio Grande do Norte, Brasil

References (51)

Show source-provided references
1. Study characteristics of (epoxy–bentonite doped) composite materials10.1016/j.egypro.2017.07.094 ↗
2. Correction to: a comparative study of mechanical properties, thermal conductivity, residual stresses, and wear resistance of aluminum-alumina composites obtained by squeeze casting and powder metallurgy10.1007/s11661-021-06436-w ↗
3. Microstructure and mechanical properties of aluminium metal matrix composites with addition of bamboo leaf ash by stir casting method10.1016/S1003-6326(17)60284-X ↗
4. An experimental analysis of tensile, hardness and wear properties of aluminium metal matrix composite through stir casting process10.1007/s42452-020-2657-8 ↗
5. Trinh SN · 2016
6. Preparation of 6061Al-Al 2 O 3 MMC’s by stir casting and evaluation of mechanical and wear properties10.1016/j.mspro.2014.07.151 ↗
7. Effect of nano-size Al2O3 reinforcement on the mechanical behavior of synthesis 7075 aluminum alloy composites by mechanical alloying10.1016/j.matchemphys.2012.12.015 ↗
8. Reinforcements, manufacturing techniques, and respective property changes of Al2O3/SiC based composites: a review10.1007/s12633-021-01108-1 ↗
9. In situ tungsten carbide formation in nanostructured copper matrix composite using mechanical alloying and sintering10.3390/ma15072340 ↗
10. Modulating the microstructural and mechanical characteristics of copper-tungsten carbide composite powders by WC content and milling time
11. Synergistic performance evaluation of copper–WC-graphene composites: Microstructure, mechanical properties, corrosion, and wear behavior under microwave sintering10.1016/j.matchemphys.2024.129202 ↗
12. Thermal, electrical and wear behavior of sintered Cu–W nanocomposite10.1016/j.matdes.2012.09.055 ↗
13. Well-dispersion of nanoscale WC particles in WC–Cu composites prepared by molecular level mixing and spark plasma sintering10.1007/s11106-022-00270-4 ↗
14. Synthesis of tungsten carbides in a copper matrix by spark plasma sintering: microstructure formation mechanisms and properties of the consolidated materials10.3390/ma16155385 ↗
15. Raimundo RA · 2016
16. W–Cu composite with high W content prepared by grading rounded W powder with narrow particle size distribution10.3390/ma15051904 ↗
17. Ceramic particles reinforced copper matrix composites manufactured by advanced powder metallurgy: preparation, performance, and mechanisms
18. High‐strength wear‐resistant Cu/tungsten carbide/diamond composites fabricated by powder metallurgy10.1002/adem.202302142 ↗
19. Brophy JE · 1972
20. WC – (Cu: AISI304) composites processed from high energy ball milled powders10.1016/j.ijrmhm.2019.104990 ↗
21. WC-Cu thermal barriers for fusion applications10.1016/j.surfcoat.2018.02.086 ↗
22. New WC-Cu thermal barriers for fusion applications: high temperature mechanical behaviour10.1016/j.jnucmat.2017.10.071 ↗
23. Silva TQ · 2022
24. Effects of ball size on the grinding behavior of talc using a high-energy ball mill10.3390/min9110668 ↗
25. Microstructure and properties of NiCoCrAlTi high entropy alloy prepared using MA-SPS technique10.3390/ma16052082 ↗
26. 2018
27. 2017
28. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
29. High-entropy high-hardness metal carbides discovered by entropy descriptors10.1038/s41467-018-07160-7 ↗
30. Phenomenological model of anisotropic peak broadening in powder diffraction10.1107/S0021889898006001 ↗
31. Rietveld texture analysis from synchrotron diffraction images. I. Calibration and basic analysis10.1017/S0885715613001346 ↗
32. Properties and microstructure evaluation in NiAl-xWC (x = 0 − 90 wt.%) intermetallic-based composites prepared by mechanical alloying10.3390/ma16052048 ↗
33. Understanding anisotropic microstrain broadening in Rietveld refinement10.1524/zkri.2011.1413 ↗
34. Synthesis of tungsten carbides in a copper matrix by spark plasma sintering: microstructure formation mechanisms and properties of the consolidated materials10.3390/ma16155385 ↗
35. 2022
36. Microstructural evolution and mechanical properties of AlCrFeNiCoC high entropy alloy produced via spark plasma sintering10.1080/00325899.2019.1576389 ↗
37. Effect of C and milling parameters on the synthesis of WC powders by mechanical alloying10.1016/j.ijrmhm.2009.09.006 ↗
38. Phase analysis of mechanically alloyed in situ copper-tungsten carbide composite
39. Effect of milling time and reinforcement volume fraction on microstructure and mechanical properties of SiCp-reinforced AA2017 composite powder produced by high-energy ball milling10.3390/ma17020435 ↗
40. Ultrafine-grained stainless steels after severe plastic deformation10.3390/met13040674 ↗
41. Impact of the SiC addition on the morphological, structural and mechanical properties of Cu-SiC composite powders prepared by high energy milling10.1016/j.apt.2021.06.006 ↗
42. The influence of ball milling conditions on the powder characteristics and sintering densification of Mo Cu alloy10.1016/j.ijrmhm.2024.106914 ↗
43. Micro-/nano-scale WC particle-reinforced Cu-based composite preparation and property study10.1063/5.0160981 ↗
44. A review on the additive manufacturing of W-Cu composites10.3390/met15020197 ↗
45. Investigation of the effect of sintering process parameters on the corrosion, wear and hardness of W–Cu composite10.1007/s12046-024-02559-z ↗
46. Influence of sintering time on microstructure and properties of hot oscillatory pressing sintered W–Cu refractory alloys10.1007/s42864-023-00224-2 ↗
47. Effect of grain refinement on the comprehensive mechanical performance of W–Cu composites10.3390/nano13030386 ↗
48. Microstructure and mechanical properties of WC–TiC–Co cemented carbides produced by spark plasma sintering (SPS) method10.1007/s42452-023-05510-9 ↗
49. Investigation of WC reinforced CuNiSi composites produced by mechanical alloying method
50. Fabrication and characterization of W Cu composite coatings with different W contents by cold spraying10.1016/j.surfcoat.2019.04.034 ↗
51. Tribological and electrochemical corrosion behaviors of Cu-based powder metallurgy composites reinforced by in-situ WC with different morphology10.1016/j.jmrt.2022.11.031 ↗