journal article·2025-11

Electromagnetic field-controlled wire-arc directed energy deposition of 316L stainless steel: In-situ nitrogen alloying for enhanced strength-ductility and corrosion resistance

Yang Zhong, Liming Lei, Zhizhen Zheng, Jianjun Li

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Recent developments in stainless steels10.1016/j.mser.2009.03.001 ↗
2. Steels in additive manufacturing: a review of their microstructure and properties10.1016/j.msea.2019.138633 ↗
3. Microstructure and mechanical properties of the austenitic stainless steel 316L fabricated by gas metal arc additive manufacturing10.1016/j.msea.2017.05.024 ↗
4. Effects of linear heat input on microstructure and corrosion behavior of an austenitic stainless steel processed by wire arc additive manufacturing10.1016/j.vacuum.2019.109131 ↗
5. Microstructure evolution and mechanical properties of a wire-arc additive manufactured austenitic stainless steel: effect of processing parameter10.3390/ma14071681 ↗
6. Effect of heat treatment temperature on microstructure and tensile properties of austenitic stainless 316L using wire and arc additive manufacturing10.1016/j.msea.2021.142446 ↗
7. Effect of heat treatment on microstructure, mechanical and corrosion properties of austenitic stainless steel 316L using arc additive manufacturing10.1016/j.msea.2017.10.002 ↗
8. Oxygen-induced intergranular cracking of a Ni-base alloy at elevated temperatures—an example of dynamic embrittlement10.1016/S1359-6454(01)00005-2 ↗
9. Microstructural evolution in 316LN austenitic stainless steel during solidification process under different cooling rates10.1007/s10853-015-9565-0 ↗
10. Solidification mode and residual ferrite in low-Ni austenitic stainless steels10.1023/A:1004774130483 ↗
11. Weldability of high nitrogen stainless steel10.2355/isijinternational.42.1334 ↗
12. An exceptionally strong, ductile and impurity-tolerant austenitic stainless steel prepared by laser additive manufacturing10.1016/j.actamat.2023.118868 ↗
13. The effect of post-processing heat treatment on the microstructure, residual stress and mechanical properties of selective laser melted 316L stainless steel10.1016/j.msea.2021.141611 ↗
14. Multi-scale defects in powder-based additively manufactured metals and alloys10.1016/j.jmst.2022.02.015 ↗
15. The influence of oxygen additions on Argon-shielded gas metal arc welding processes
16. Study on microstructure and mechanical properties of 304 stainless steel joints by TIG, laser and laser-TIG hybrid welding10.1016/j.optlaseng.2009.08.009 ↗
17. Effects of Ar-N2-He shielding gas on microstructure, mechanical properties and corrosion resistance of the Laser-MIG additive manufacturing 316L stainless steel10.1016/j.jmatprotec.2022.117844 ↗
18. Review on field assisted metal additive manufacturing10.1016/j.ijmachtools.2023.104032 ↗
19. Investigation of weld formation and porosity in 5052 aluminium alloy laser-GMA hybrid welding assisted by magnetic field with different orientations10.1080/13621718.2022.2106022 ↗
20. Effect of magnetic field orientation on suppressing porosity in steady-magnetic-field-assisted aluminum alloy deep-penetration laser welding10.1016/j.jmatprotec.2022.117569 ↗
21. Effects of electromagnetic force on melt flow and porosity prevention in pulsed laser keyhole welding10.1016/j.ijheatmasstransfer.2006.10.040 ↗
22. Backward flowing molten metal in weld pool and its influence on humping bead in high-speed GMAW10.1016/j.jmatprotec.2016.06.028 ↗
23. Analysis of additional electromagnetic force for mitigating the humping bead in high-speed gas metal arc welding10.1016/j.jmatprotec.2015.09.014 ↗
24. Improvement of low-temperature impact toughness for 304 weld joint produced by laser-MIG hybrid welding under magnetic field10.1016/j.jmatprotec.2017.04.004 ↗
25. Effect of magnetic field applied during laser-arc hybrid welding in improving the pitting resistance of the welded zone in austenitic stainless steel10.1016/j.corsci.2017.07.019 ↗
26. Effect of transverse magnetic field on microstructure and mechanical properties of Ti-6Al-4V manufactured by Laser-MIG hybrid welding10.1007/s00170-022-09626-x ↗
27. Effect of magnetic field on the microstructure and mechanical properties of inconel 625 superalloy fabricated by wire arc additive manufacturing10.1016/j.jmapro.2021.01.008 ↗
28. Tailoring the surface finish, dendritic microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy by magnetic arc oscillation
29. Enhanced mechanical properties of Ti6Al4V alloy fabricated by laser additive manufacturing under static magnetic field10.1080/21663831.2022.2064195 ↗
30. Influence of the external magnetic field on fluid flow, temperature profile and humping bead in high speed gas metal arc welding10.1016/j.ijheatmasstransfer.2017.09.130 ↗
31. Effect of in-situ transverse magnetic field on microstructure, mechanical properties and corrosion resistance of the directed energy deposited 316L stainless steel
32. Shielding gas effects on flux cored arc welding of AISI 316L (N) austenitic stainless steel joints10.1016/j.matdes.2012.09.012 ↗
33. Suppression of humping bead in high speed GMAW with external magnetic field10.1179/1362171815Y.0000000074 ↗
34. Surface tension and thermal conductivity of NIST SRM 1155a (AISI 316L stainless steel)10.1007/s10765-022-02991-5 ↗
35. Visualizing the vibration effect on the tandem-pulsed gas metal arc welding in the presence of surface tension active elements10.1016/j.ijheatmasstransfer.2020.120310 ↗
36. Recent progress in welding technology under external magnetic fields
37. Phase instabilities during high temperature exposure of 316 austenitic stainless steel10.1007/BF02647659 ↗
38. Thermal stability of dislocation structure and its effect on creep property in austenitic 316L stainless steel manufactured by directed energy deposition10.1016/j.msea.2023.144981 ↗
39. Origin of dislocation structures in an additively manufactured austenitic stainless steel 316L10.1016/j.actamat.2020.07.063 ↗
40. Theory of dislocations10.1115/1.3167075 ↗
41. Real-time observations of TRIP-induced ultrahigh strain hardening in a dual-phase CrMnFeCoNi high-entropy alloy10.1038/s41467-020-14641-1 ↗
42. Reconfiguring dual-phase structure with equal micro-hardness to achieve double strength with slight ductility sacrifice10.1016/j.jmst.2022.09.019 ↗
43. Effect of initial dislocation density on the plastic deformation response of 316L stainless steel manufactured by directed energy deposition10.1016/j.msea.2022.143591 ↗
44. Dislocation structure evolution and its effects on cyclic deformation response of AISI 316L stainless steel10.1016/j.msea.2011.01.015 ↗
45. Fabrication of 316L nuclear nozzles on the main pipeline with large curvature by CMT wire arc additive manufacturing and self-developed slicing algorithm10.1016/j.msea.2021.141539 ↗
46. Multi-physics simulation of dendritic growth in magnetic field assisted solidification10.1016/j.ijheatmasstransfer.2019.118673 ↗
47. Thermo-electromagnetic effect on weld microstructure in magnetically assisted laser welding of austenite steel10.1016/j.jmapro.2019.03.033 ↗
48. Three-dimensional transient thermoelectric currents in deep penetration laser welding of austenite stainless steel10.1016/j.optlaseng.2016.12.001 ↗
49. Effect of external applied magnetic field on microstructures and mechanical properties of laser welding joint of medium-Mn nanostructured steel10.1016/j.msea.2020.139787 ↗
50. In-situ fabrication of graded material with the application of a horizontal magnetic field during directional solidification10.1016/j.matchar.2018.05.007 ↗
51. Effect of a weak transverse magnetic field on solidification structure during directional solidification10.1016/j.actamat.2013.10.050 ↗
52. Molten pool behavior and solidification characterization in steady magnetic field assisted laser-MIG hybrid welding of aluminum alloy10.1016/j.jmapro.2022.10.041 ↗
53. The contribution of constitutional cupercooling to cucleation and grain formation10.1007/s11661-015-2960-y ↗
54. Manufacturing of metals: microstructure evolution and multistage control10.1016/j.jmst.2021.06.011 ↗
55. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
56. Refinement of Ti-6Al-4V prior-β grain structure in the as-deposited condition via process control during wire-direct energy deposition
57. 2003
58. Effect of processing parameters on microstructure and tensile properties of austenitic stainless steel 304L made by directed energy deposition additive manufacturing10.1016/j.actamat.2016.03.019 ↗
59. Study on microstructure and tensile properties of 316L stainless steel fabricated by CMT wire and arc additive manufacturing10.1016/j.msea.2020.140006 ↗
60. Study of mechanical properties of AISI 316 stainless steel processed by “selective laser melting”10.1007/s00170-010-2631-5 ↗
61. Wire and arc additive manufacturing: a comparison between CMT and TopTIG processes applied to stainless steel10.1007/s40194-018-0606-6 ↗
62. Damage evolution and failure mechanisms in additively manufactured stainless steel10.1016/j.msea.2015.10.073 ↗
63. Overview: high-nitrogen alloying of stainless steels10.1016/0921-5093(95)09991-3 ↗
64. Effects of processing and manufacturing of high nitrogen-containing stainless steels on their mechanical10.1016/S0924-0136(01)00804-4 ↗
65. Some theoretical aspects on designing nickel free high nitrogen austenitic stainless steels10.2355/isijinternational.41.1018 ↗
66. Nickel and chromium-based high nitrogen alloys10.1081/AMP-120027518 ↗
67. Enhanced wear and corrosion resistance of the laser direct metal deposited AISI 316L stainless steel by in-situ interstitial N alloying10.1016/j.optlastec.2023.110381 ↗
68. Processing of gas-nitrided AISI 316L steel powder by laser powder bed fusion – microstructure and properties
69. Validation of corrosion rates measured by the Tafel extrapolation method10.1016/j.corsci.2005.05.046 ↗
70. Effect of cold deformation on the corrosion behaviour of UNS S31803 duplex stainless steel in simulated concrete pore solution10.1016/j.corsci.2017.05.021 ↗
71. Crystallization-dependent transition of corrosion resistance of an Fe-based bulk metallic glass under hydrostatic pressures10.1016/j.corsci.2020.109098 ↗
72. Technical note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
73. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
74. Effect of solution concentration on semiconducting properties of passive films formed on austenitic stainless steels10.1016/j.corsci.2009.09.003 ↗
75. Corrosion mechanism of amorphous alloy strengthened stainless steel composite fabricated by selective laser melting
76. Effects of dissolved oxygen on electrochemical and semiconductor properties of 316L stainless steel10.1016/j.jnucmat.2010.10.010 ↗
77. Effect of annealing temperature on the pitting corrosion resistance of super duplex stainless steel UNS S3275010.1016/j.matchar.2009.04.009 ↗