Calcium Oxalate Protective Interphase for Regulated Zinc Deposition in Aqueous Batteries
Source abstract
Abstract
Interfacial instability of Zn metal anodes, including nonuniform deposition, parasitic reactions, hydrogen evolution, corrosion, and by-product accumulation, remains a major challenge for aqueous zinc-ion batteries. Herein, we report a facile calcium oxalate (CaC2O4) protective coating to regulate the Zn/electrolyte interface. Owing to its low solubility and inorganic stability, the CaC2O4 layer serves as a persistent ion-regulating interphase that reduces direct water contact and promotes more uniform Zn2+ transport and deposition. Structural characterization confirms a continuous coating, while XPS indicates interfacial electronic interaction. In situ Raman spectroscopy shows that the perturbed oxalate-related νs(COO-) band remains detectable and evolves in intensity during initial Zn plating, supporting both persistence of the oxalate-containing framework and perturbation of its local interfacial environment. Electrochemical kinetic analyses show that the apparent activation energy for interfacial Zn2+ transport decreases from 17.58 to 10.04 kJ mol-1 after CaC2O4 modification, accompanied by reduced charge-transfer resistance and nucleation overpotential. These improvements suppress corrosion, hydrogen evolution, and zinc hydroxide sulfate by-product formation, enabling approximately 1450 h of Zn∥Zn cycling at 5 mA cm-2 and 1 mAh cm-2. Moreover, CaC2O4@Zn∥MnO2 full cells retain 60% capacity after 600 cycles at 1 A g-1. This work demonstrates a low-cost inorganic interphase for stabilizing Zn anodes through persistent protection and interfacial Zn2+ transport regulation.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.