Effect of shot peening intensity on the corrosion behavior of 321 stainless steel in liquid lead-bismuth eutectic
Source abstract
Abstract
The influence of shot peening (SP)-induced surface deformation on the liquid lead–bismuth eutectic (LBE) corrosion behavior of metastable 321 stainless steel (321 SS) was systematically investigated at 500 °C for 1000 h in oxygen-controlled LBE (~10⁻⁶ wt.% O). Particular attention was paid to the role of strain-induced martensitic transformation (SIMT) and defect evolution in regulating oxide formation and liquid metal penetration. The results show that corrosion resistance strongly depends on SP intensity. Insufficient deformation introduced by 0.3 mmA SP produced heterogeneous martensitic transformation and coarse planar deformation structures, which promoted localized LBE penetration and resulted in a discontinuous oxide scale. In contrast, 0.5 mmA SP generated a more uniformly refined deformation layer with a higher martensite fraction, facilitating the formation of a compact duplex oxide layer composed primarily of Fe–Cr spinel and magnetite, thereby effectively suppressing liquid metal ingress. Microstructural characterization revealed significant elemental redistribution and phase evolution beneath the oxide layer during corrosion. The deformation-induced martensite underwent compositional partitioning and phase decomposition, accompanied by Cr enrichment and the formation of nanoscale σ phase precipitates after prolonged exposure. The enhanced corrosion resistance obtained under higher SP intensity is attributed to the synergistic effects of refined defect structures, accelerated protective oxide formation, and reduced preferential penetration pathways. These findings provide insight into the coupling between mechanically induced metastable microstructures and liquid metal corrosion behavior in austenitic stainless steels.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Overview of lead-cooled fast reactor activities10.1016/j.pnucene.2013.11.011 ↗
2. Further insights into the mechanisms involved in the corrosion of 316L(N) austenitic steel in oxygenated liquid sodium at 550 °C10.1016/j.corsci.2019.108399 ↗
3. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
4. Dissolution mechanism of 316L in lead–bismuth eutectic at 500 °C10.1016/j.corsci.2011.05.031 ↗
5. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450 °
6. Effect of silicon contents on the microstructures and mechanical properties of heat affected zones for 9Cr2WVTa steels10.1016/j.jnucmat.2015.11.055 ↗
7. Enhancing LBE corrosion resistance of T91 steel by yttrium-aluminide coating
8. Effect of Si on suppressing dissolution corrosion of AFA steel exposed to LBE at 600 °C with 10−6 wt% oxygen for up to 6000h via modification of internal oxidation zone
9. Effects of Al and Y elements on mechanical properties and LEB resistance of FeCrAl(Y) coatings prepared by HiPIMS10.1016/j.surfcoat.2025.132733 ↗
10. Corrosion tests on austenitic samples with alumina and alumina-forming coatings in oxygen-containing stagnant Pb and turbulently flowing PbBi10.1016/j.jnucmat.2024.155121 ↗
11. Corrosion investigations of Al-Fe-coated steels, high Cr steels, refractory metals and ceramics in lead alloys at 700 °C10.1016/j.jnucmat.2009.10.025 ↗
12. Corrosion and radiation resistant nanoceramic coatings for lead fast reactors10.1016/j.corsci.2017.05.011 ↗
13. Preparation of Cr-N coatings on 316H stainless steel via pack chromizing and gas nitriding, and their resistance to liquid metal corrosion in early stages10.1016/j.surfcoat.2024.130665 ↗
14. Unexpected promoter: thermokinetic role of sigma phase in accelerating stainless steel chromizing10.1016/j.actamat.2026.122088 ↗
15. Effect of high energy shot peening pressure on the stress corrosion cracking of the weld joint of 304 austenitic stainless steel10.1016/j.msea.2015.03.088 ↗
16. Enhanced corrosion resistance of 15-15Ti austenitic steel in liquid lead-bismuth eutectic at 550 °C by shot peening processing10.1016/j.corsci.2023.111640 ↗
17. Microstructure and corrosion property evolution of a surface-nanostructured 15-15Ti austenitic steel during immersion in liquid LBE at 550 °C10.1016/j.jnucmat.2024.155475 ↗
18. Understanding shot peening-enhanced corrosion resistance in AFA steel exposed to LBE with 10−6 wt% oxygen at 600 °C: precipitation-recrystallization interaction in deformation layer10.1016/j.corsci.2025.113439 ↗
19. The effects of cold working on the corrosion behavior of an austenitic stainless steel in liquid lead-bismuth eutectic under vacuum at 873 K10.1016/j.jnucmat.2018.07.034 ↗
20. Effect of deformation twinning on the early oxidation behaviour of 316L steel exposed to liquid lead-bismuth eutectic10.1016/j.vacuum.2024.113387 ↗
21. Corrosion behavior of cold-worked austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.jnucmat.2014.02.006 ↗
22. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
23. Development of Ultra-Fine-Grained structure in AISI 321 austenitic stainless steel10.1007/s11661-017-4361-x ↗
24. Enhancing AISI 321 stainless steel's high-temperature oxidation resistance at 600 °C through surface nanocrystallization and pre-oxidation synergy10.1016/j.surfcoat.2024.130747 ↗
25. The effect of temperature and oxygen content on the flowing liquid metal corrosion of structural steels in the Pb-Bi eutectic10.1016/j.nucengdes.2006.02.003 ↗
26. MAUD (Material Analysis Using Diffraction) v2.9997 [software]
27. Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2018.08.030 ↗
28. X-ray line profile analysis of the deformation microstructure in a medium-grained Fe-Mn-Al-C austenitic steel10.1016/j.matchar.2020.110833 ↗
29. Improving the oxidation resistance of SIMP steel to liquid Pb-Bi eutectic by shot peening treatments10.1016/j.apsusc.2021.151910 ↗
30. Microstucture evolution and interfacial properties in the Fe-Pb system10.1016/S1359-6454(02)00129-5 ↗
31. Research results on the corrosion effects of liquid heavy metals Pb, Bi and Pb-Bi on structural materials with and without corrosion inhibitors10.1016/S0029-5493(02)00158-9 ↗
32. fourth ed., Butterworth-Heinemann, Oxford
33. Effect of spinodal decomposition on the mechanical behavior of Fe–Cr alloys10.1016/j.msea.2010.01.020 ↗
34. Humphreys · 2017
35. High-Chromium Ferritic and
36. Effect of 475 °C embrittlement on the mechanical properties of duplex stainless steel10.1016/j.msea.2009.01.039 ↗
37. On the significance of nature of strain-induced martensite on phase-reversion-induced nanograined/ultrafine-grained austenitic stainless steel10.1007/s11661-009-0072-2 ↗
38. Reversion mechanism from deformation induced martensite to austenite in metastable austenitic stainless steels10.2355/isijinternational.31.1431 ↗
39. Effect of initial microstructure on superplasticity in ultrafine grained 18Cr-9Ni stainless steel10.2320/matertrans.45.2259 ↗
40. Enhanced mechanical properties through reversion in metastable austenitic stainless steels10.1007/s11661-008-9723-y ↗
41. On the role of dislocations in bulk diffusion10.1016/0001-6160(57)90127-X ↗
42. High Temperature Oxidation
43. Insights into the preferential intergranular oxidation mechanism of 316L austenitic stainless steel exposed to oxygen saturated lead-bismuth eutectic (LBE)10.1016/j.actamat.2026.121962 ↗
44. On oxidation film structure of SIMP steel exposed in stagnant oxygen-saturated LBE at 600 °C10.1016/j.corsci.2024.111927 ↗
45. Mechanistic insight into the ferritization of austenite in Pb via a discontinuous reaction governed by a migrating liquid film10.1016/j.corsci.2025.113398 ↗
46. A refined oxidation mechanism proposed for ferritic-martensitic steels exposed to oxygen-saturated liquid lead-bismuth eutectic at 400 °C for 500h10.1016/j.jnucmat.2021.152852 ↗
47. Corrosion scales on various steels after exposure to liquid lead-bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
48. Quantification of the long-term performance of steels T91 and 316L in oxygen-containing flowing lead-bismuth eutectic at 550 °C10.1115/1.4000364 ↗
49. Oxidation mechanism of T91 in liquid lead-bismuth eutectic: with consideration of internal oxidation10.1038/srep35268 ↗
50. Spectroscopic and microscopic investigation of the corrosion of 316/316L stainless steel by lead-bismuth eutectic (LBE) at elevated temperatures: importance of surface preparation10.1016/j.jnucmat.2004.03.006 ↗