journal article·2004-05

Relating the Morphology of Poly(p‐phenylene vinylene)/Methanofullerene Blends to Solar‐Cell Performance

J. K. J. van Duren, X. Yang, J. Loos, C. W. T. Bulle‐Lieuwma, A. B. Sieval, J. C. Hummelen, R. A. J. Janssen

Advanced Functional Materials· Volume 14· Issue 5
Publisher page

Abstract

Abstract The performance of bulk‐heterojunction solar cells based on a phase‐separated mixture of donor and acceptor materials is known to be critically dependent on the morphology of the active layer. Here we use a combination of techniques to resolve the morphology of spin cast films of poly(p‐phenylene vinylene)/methanofullerene blends in three dimensions on a nanometer scale and relate the results to the performance of the corresponding solar cells. Atomic force microscopy (AFM), transmission electron microscopy (TEM), and depth profiling using dynamic time‐of‐flight secondary ion mass spectrometry (TOF‐SIMS) clearly show that for the two materials used in this study, 1‐(3‐methoxycarbonyl)propyl‐1‐phenyl‐[6,6]‐methanofullerene (PCBM) and poly[2‐methoxy‐5‐(3′,7′‐dimethyloctyloxy)‐1,4‐phenylene vinylene] (MDMO‐PPV), phase separation is not observed up to 50 wt.‐% PCBM. Nanoscale phase separation throughout the film sets in for concentrations of more than 67 wt.‐% PCBM, to give domains of rather pure PCBM in a homogenous matrix of 50:50 wt.‐% MDMO‐PPV/PCBM. Electrical characterization, under illumination and in the dark, of the corresponding photovoltaic devices revealed a strong increase of power conversion efficiency when the phase‐separated network develops, with a sharp increase of the photocurrent and fill factor between 50 and 67 wt.‐% PCBM. As the phase separation sets in, enhanced electron transport and a reduction of bimolecular charge recombination provide the conditions for improved performance. The results are interpreted in terms of a model that proposes a hierarchical build up of two cooperative interpenetrating networks at different length scales.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Organic Electronics and Photovoltaics · Fullerene Chemistry and Applications · Conducting polymers and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. 10.1126/science.270.5243.178910.1126/science.270.5243.1789 ↗
2. 10.1038/376498a010.1038/376498a0 ↗
3. 10.1063/1.152124410.1063/1.1521244 ↗
4. 10.1002/anie.20035164710.1002/anie.200351647 ↗
5. 10.1126/science.258.5087.147410.1126/science.258.5087.1474 ↗
6. 10.1016/S0009-2614(01)00431-610.1016/S0009-2614(01)00431-6 ↗
7. 10.1063/1.151294310.1063/1.1512943 ↗
8. 10.1063/1.161994610.1063/1.1619946 ↗
9. 10.1063/1.134583410.1063/1.1345834 ↗
10. 10.1002/1616-3028(200112)11:6<420::AID-ADFM420>3.0.CO;2-K10.1002/1616-3028(200112)11:6<420::AID-ADFM420>3.0.CO;2-K ↗
11. 10.1002/1521-4095(20021203)14:23<1735::AID-ADMA1735>3.0.CO;2-O10.1002/1521-4095(20021203)14:23<1735::AID-ADMA1735>3.0.CO;2-O ↗
12. 10.1002/adfm.20039001110.1002/adfm.200390011 ↗
13. 10.1016/S0379-6779(02)01311-510.1016/S0379-6779(02)01311-5 ↗
14. 10.1021/ma010240e10.1021/ma010240e ↗
15. 10.1021/nl025741810.1021/nl0257418 ↗
16. 10.1002/adfm.20039000410.1002/adfm.200390004 ↗
17. 10.1016/S0169-4332(02)00756-010.1016/S0169-4332(02)00756-0 ↗
18. 10.1021/ma971692n10.1021/ma971692n ↗
19. 10.1021/ma981302c10.1021/ma981302c ↗
20. 10.1021/ja00333a00610.1021/ja00333a006 ↗
21. Zalm P. C. · Mikrochim. Acta · 2000 · 132 · 24310.1007/s006040050018 ↗
22. It should be noted that with increasing polymer concentration the overlap in mass between the isotope clusters13C1H with12C2H (= CD) and1H2with2H (= D) results in an increasing contribution of the non‐deuterium related isotopes to the ion yields of CD CHD and C2D from < 10 % for 100 wt.‐% d5‐PCBM to ∼ 30 % at 40 wt.‐% d5‐PCBM as can be concluded from comparison with the undeuterated composites.
23. 10.1002/1521-4095(200009)12:18<1367::AID-ADMA1367>3.0.CO;2-Z10.1002/1521-4095(200009)12:18<1367::AID-ADMA1367>3.0.CO;2-Z ↗
24. 10.1002/1616-3028(20021016)12:10<665::AID-ADFM665>3.0.CO;2-J10.1002/1616-3028(20021016)12:10<665::AID-ADFM665>3.0.CO;2-J ↗
25. T. J. Savenije J. E. Kroeze M. M. Wienk J. M. Kroon J. M. Warman unpublished.
26. The spectral overlap between the light source and the absorption spectrum of the 80 wt.‐% PCBM film is shown in the inset of Figure 7b.
27. The fill factor is defined as: FF = (JmaxVmax)/(JscVoc) whereJmaxandVmaxare current density and voltage at the maximum power point respectively.
28. The power conversion efficiency is defined as ηpc[%] = (JscVoc×FF)/ILP with ILP the incident light power.
29. The standard deviation of the short‐circuit current density (Jsc) and power conversion efficiency (ηpc) is below 10 % of the average. The light source has a deviation of 3 % in light power. The open‐circuit voltage (Voc) has a standard deviation of ∼ 1 % for every composition except for the pure MDMO‐PPV and 2 wt.‐% PCBM devices whose standard deviation forVocis somewhat larger (∼ 7 %). TheVocfor these low fullerene concentrations is very sensitive to film thickness and shorts density as a result of the photocurrent and leakage current being of the same order of magnitude. The fill factor (FF) has a standard deviation of ∼ 1 % for every composition.
30. Due to poor film‐forming properties of pure PCBM the ∼ 100 nm spin‐cast films contain tiny holes (as observed with AFM) making reproducibility of the solar cell results poor and the influence of leakage current extremely large. Therefore no data of photocurrents coming from pure PCBM are included.
31. M. Sahimi Applications of Percolation Theory Taylor & Francis London1994.10.1201/9781482272444 ↗
32. 10.1002/1616-3028(200110)11:5<374::AID-ADFM374>3.0.CO;2-W10.1002/1616-3028(200110)11:5<374::AID-ADFM374>3.0.CO;2-W ↗
33. 10.1002/polb.1064710.1002/polb.10647 ↗
34. 10.1063/1.156273910.1063/1.1562739 ↗
35. 10.1016/S0039-6028(01)01554-010.1016/S0039-6028(01)01554-0 ↗
36. The work functions for PEDOT–PSS (5.2 eV) and LiF/Al (∼ 3.7 eV) match with the HOMO level of MDMO‐PPV (5.3 ± 0.1 eV) and the LUMO level of PCBM (3.7 eV) see reference [37].
37. 10.1063/1.162068310.1063/1.1620683 ↗
38. A. L. Fahrenbruch R. H. Bube Fundamentals of Solar Cells Academic Press New York1983.10.1016/B978-0-12-247680-8.50013-X ↗
39. 10.1016/S0040-6090(01)01589-910.1016/S0040-6090(01)01589-9 ↗
40. Fitting is performed over the upper part of the measured range (three orders of magnitude R &#62; 0.999) where bothVocand FF are clearly beyond their threshold value. When fitted over the full range (five orders of magnitude) the trend in the slope with varying composition is unaffected but statistics deteriorate.
41. Dyakonov V. · Mater. Res. Soc. Symp. Proc. · 2002 · 665 · 235
42. 10.1126/science.106915610.1126/science.1069156 ↗
43. The incident photon to current conversion efficiency (or external quantum efficiency) is defined as: IPCE [%] = (1.24 × 105 × Jsc)/(ILP × λ) withJsc[mA cm–2] ILP [mW cm–2] and λ [nm] the wavelength of the monochromatic light.
44. 10.1021/ja00106a06810.1021/ja00106a068 ↗
45. 10.1103/PhysRevB.55.R65610.1103/PhysRevB.55.R656 ↗
46. 10.1063/1.36822710.1063/1.368227 ↗
47. 10.1103/PhysRevB.49.1748010.1103/PhysRevB.49.17480 ↗
48. 10.1002/1439-7641(20020916)3:9<795::AID-CPHC795>3.0.CO;2-A10.1002/1439-7641(20020916)3:9<795::AID-CPHC795>3.0.CO;2-A ↗
49. V0 ≈ Voc + 0.2 V for 0 and 2 wt.‐% whereasV0 ≈ Voc + 0.05 V for all other concentrations.
50. For current densities larger than 100 mA cm–2 the applied voltage should be corrected for the voltage drop across the indium tin oxide (ITO) series resistanceVRS which typically amounts to 25 Ω in our substrates.
51. 10.1002/(SICI)1521-4095(200001)12:1<42::AID-ADMA42>3.0.CO;2-F10.1002/(SICI)1521-4095(200001)12:1<42::AID-ADMA42>3.0.CO;2-F ↗