Holey Graphene Nanomanufacturing: Structure, Composition, and Electrochemical Properties
Source abstract
Abstract
Topology is critical for properties and function of 2D nanomaterials. Membranes and films from 2D nanomaterials usually suffer from large tortuosity as a result from dense restacking of the nanosheets and thus have limited utility in applications such as electrodes for supercapacitor and batteries, which require ion transport through the nanosheet thickness. In comparison with conventional porous 2D nanomaterials, introducing holes through the nanosheets to create holey 2D nanomaterials with retention of the 2D‐related properties is a more viable approach to improve molecular transport. Here, graphene is used as a model to study the fundamental structure‐property relationship as a result from defect‐enabled hole creation. Specifically, the correlation of electrochemical capacitive properties with structure and composition for holey graphene materials is prepared using a highly scalable controlled air oxidation process. The presence of holes on graphene sheets is not sufficient to account for the observed capacitance improvement. Rather, the improvement is achieved through the combination of an enhanced mesopore fraction with simultaneous oxygen doping while retaining the graphitic carbon network with minimal damage. The detailed understanding might be further applied to other 2D materials toward a broader range of both energy‐related and other applications.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Supercapacitor Materials and Fabrication · Graphene research and applications · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Institute of Aerospace 100 Exploration Way Hampton VA 23666 USA
Department of Applied Science The College of William and Mary Williamsburg VA 23185 USA
Department of Materials Science and Engineering University of Maryland College Park MD 20742 USA
Advanced Materials and Processing Branch NASA Langley Research Center Hampton VA 23681‐2199 USA
References (24)
Show source-provided references
1. 10.1021/cr900070d10.1021/cr900070d ↗
2. 10.1021/cr300263a10.1021/cr300263a ↗
3. 10.1039/C3NR04555B10.1039/C3NR04555B ↗
4. 10.1002/adma.20130311510.1002/adma.201303115 ↗
5. 10.1039/C4NR04584J10.1039/C4NR04584J ↗
6. 10.1021/nn502635y10.1021/nn502635y ↗
7. 10.1038/ncomms555410.1038/ncomms5554 ↗
8. 10.1038/nnano.2010.810.1038/nnano.2010.8 ↗
9. 10.1021/nl100750v10.1021/nl100750v ↗
10. 10.1021/ja105426h10.1021/ja105426h ↗
11. 10.1038/srep0123810.1038/srep01238 ↗
12. 10.1021/ja205693t10.1021/ja205693t ↗
13. 10.1021/nn202710s10.1021/nn202710s ↗
14. 10.1038/srep0199610.1038/srep01996 ↗
15. 10.1126/science.120077010.1126/science.1200770 ↗
16. 10.1039/c3nr02135a10.1039/c3nr02135a ↗
17. 10.1039/c4ee00106k10.1039/c4ee00106k ↗
18. 10.1021/ar300106h10.1021/ar300106h ↗
19. 10.1021/nn401794k10.1021/nn401794k ↗
20. A similar relative enhancement factor was observed for Cmof h‐Graphene versus starting graphene with 0.5mH2SO4as the electrolyte (Figure S5 Supporting Information) but that in an ionic liquid electrolyte was much less (<15%).[6]The latter could be attributed to both the bulky sizes of the ionic liquid electrolyte ions and less pronounced effect of oxygen doping in ion liquid versus aqueous electrolytes.
21. 10.1021/ja01288a03210.1021/ja01288a032 ↗
22. The temperature‐dependent series of samples were conducted on a different tube furnace (MTI Corporation OTF‐1200X‐80‐II; no thermal block used) from the time‐dependent series discussed in the earlier sections of this manuscript (Thermolyne Model 21100; no thermal block used). Despite careful cross‐calibration there were still slight temperature differences (≈10–15 °C) in order to achieve the same carbon yield.
23. Because of the low densities of the materials each nitrogen adsorption–desorption experiment was conducted on only ≈10–20 mg of a given sample that could be fit in the sample bulb. The error margin for the measured absolute values from multiple experiments was thus found to be as large as 5%–10% even with the same calibrated sample bulb. However the shapes of BJH pore distribution plots were highly repeatable despite the absolute pore volume differences in multiple experiments.
24. 10.1021/ar200306b10.1021/ar200306b ↗