Effects of Photo‐oxidation on the Performance of Poly[2‐methoxy‐5‐(3′,7′‐dimethyloctyloxy)‐1,4‐phenylene vinylene]:[6,6]‐Phenyl C61‐Butyric Acid Methyl Ester Solar Cells
Source abstract
Abstract
Abstract A study of the photo‐oxidation of films of poly[2‐methoxy‐5‐(3′,7′‐dimethyloctyloxy)‐1,4‐phenylene vinylene] (MDMO‐PPV) blended with [6,6]‐phenyl C61‐butyric acid methyl ester (PCBM), and solar cells based thereon, is presented. Solar‐cell performance is degraded primarily through loss in short‐circuit current density, JSC. The effect of the same photodegradation treatment on the optical‐absorption, charge‐recombination, and charge‐transport properties of the active layer is studied. It is concluded that the loss in JSC is primarily due to a reduction in charge‐carrier mobility, owing to the creation of more deep traps in the polymer during photo‐oxidation. Recombination is slowed down by the degradation and cannot therefore explain the loss in photocurrent. Optical absorption is reduced by photo‐bleaching, but the size of this effect alone is insufficient to explain the loss in device photocurrent.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. 10.1063/1.152124410.1063/1.1521244 ↗
2. 10.1063/1.186112310.1063/1.1861123 ↗
3. 10.1016/j.solmat.2006.06.04110.1016/j.solmat.2006.06.041 ↗
4. 10.1016/j.solmat.2004.02.02810.1016/j.solmat.2004.02.028 ↗
5. 10.1063/1.151483110.1063/1.1514831 ↗
6. 10.1016/S0927-0248(99)00094-X10.1016/S0927-0248(99)00094-X ↗
7. 10.1016/S0040-6090(01)01589-910.1016/S0040-6090(01)01589-9 ↗
8. 10.1007/s00339-003-2499-410.1007/s00339-003-2499-4 ↗
9. 10.1016/j.solmat.2004.02.03110.1016/j.solmat.2004.02.031 ↗
10. 10.1021/jp960322i10.1021/jp960322i ↗
11. 10.1063/1.162105410.1063/1.1621054 ↗
12. 10.1002/adfm.20030504910.1002/adfm.200305049 ↗
13. 10.1002/adfm.20040034510.1002/adfm.200400345 ↗
14. 10.1002/1616-3028(200110)11:5<374::AID-ADFM374>3.0.CO;2-W10.1002/1616-3028(200110)11:5<374::AID-ADFM374>3.0.CO;2-W ↗
15. 10.1063/1.151294310.1063/1.1512943 ↗
16. 10.1021/jp027101z10.1021/jp027101z ↗
17. 10.1063/1.162463610.1063/1.1624636 ↗
18. 10.1002/adfm.20040033710.1002/adfm.200400337 ↗
19. 10.1103/PhysRevB.67.15520910.1103/PhysRevB.67.155209 ↗
20. 10.1103/PhysRevB.64.19520610.1103/PhysRevB.64.195206 ↗
21. 10.1021/ja00146a00410.1021/ja00146a004 ↗
22. 10.1103/PhysRevLett.73.74410.1103/PhysRevLett.73.744 ↗
23. 10.1002/(SICI)1097-4628(19980919)69:12<2451::AID-APP16>3.0.CO;2-#10.1002/(SICI)1097-4628(19980919)69:12<2451::AID-APP16>3.0.CO;2-# ↗
24. 10.1063/1.161994610.1063/1.1619946 ↗
25. 10.1002/pssb.222175010210.1002/pssb.2221750102 ↗
26. 10.1016/S0379-6779(00)01445-410.1016/S0379-6779(00)01445-4 ↗
27. It could be argued that the decrease in hole mobility and increase in charge lifetime could together lead to no change in the charge‐collection efficiency. However the reduction in the darkJ–Vof the photovoltaic device shows that the overall efficiency of charge collection is reduced. Moreover observations on other molecular solar cells have shown that reductions in mobility of around one order can lead to similar reductions in the darkJ–VandJSCas those seen here [26].
28. 10.1038/nmat157410.1038/nmat1574 ↗
29. 10.1007/s10853-005-0572-410.1007/s10853-005-0572-4 ↗
30. 10.1103/PhysRevB.65.12532410.1103/PhysRevB.65.125324 ↗
31. 10.1002/adfm.20030515610.1002/adfm.200305156 ↗
32. A. J. Chatten S. M. Tuladhar J. Nelson Conference Records of 31st IEEE Photovoltaic Specialists Conference IEEE Piscataway NJ2005.
33. Owing to computer time and memory constraints a film thickness of 1 μm was assumed for both the fresh and degraded films whereas the experimental films were 1.6 and 3 μm thick respectively. This difference in thickness of the simulated and experimental films is one reason why the region of sigmoidal decay is shorter for the simulation of the fresh film than the experiment. In a thicker film the carriers arrive at the counter electrode over a broader time distribution leading to a longer decay in the transient.
34. 10.1063/1.145911410.1063/1.1459114 ↗