Enabling Stable Lithium Metal Anode through Electrochemical Kinetics Manipulation
Source abstract
Abstract
Abstract The surface morphology of Li metal anode significantly dictates the stability and safety of Li metal batteries. The key parameters for morphological control and causes for dendritic growth of Li anode are still not clear. Although the plating kinetics is generally believed to be associated with Li growth habits, the detailed models are still not well defined. In this work, the temperature effect on the stability and efficiency of Li anode is systematically investigated in a variety of electrolyte composition for Li metal batteries. A dendrite‐free growth mechanism is observed, and a high Coulombic efficiency up to ≈99.4% in Li||Cu cells is achieved by tuning the deposition behaviors at elevated temperatures. The results provide insights into the Li dendrite growth mechanism and general principle for developing stable Li anode.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Hefei National Laboratory for Physical Science at the Microscale CAS Key Laboratory of Materials for Energy Conversion Department of Materials Science and Engineering University of Science and Technology of China Hefei 230026 China
School of Environmental and Materials Engineering Yantai University Yantai 264005 China
Funding
National Basic Research Program of China · National Natural Science Foundation of China
References (40)
Show source-provided references
1. 10.1039/C3EE40795K10.1039/C3EE40795K ↗
2. 10.1038/nnano.2017.1610.1038/nnano.2017.16 ↗
3. 10.1002/adma.20170000710.1002/adma.201700007 ↗
4. 10.1021/acs.chemrev.7b0011510.1021/acs.chemrev.7b00115 ↗
5. 10.1016/j.ensm.2017.12.00210.1016/j.ensm.2017.12.002 ↗
6. 10.1002/batt.20180002410.1002/batt.201800024 ↗
7. 10.1038/s41560-017-0047-210.1038/s41560-017-0047-2 ↗
8. 10.1016/S0167-2738(02)00080-210.1016/S0167-2738(02)00080-2 ↗
9. 10.1038/s41557-018-0166-910.1038/s41557-018-0166-9 ↗
10. 10.1016/j.ensm.2018.03.00110.1016/j.ensm.2018.03.001 ↗
11. 10.1016/j.nanoen.2017.08.05610.1016/j.nanoen.2017.08.056 ↗
12. 10.1073/pnas.170822411410.1073/pnas.1708224114 ↗
13. 10.1021/acs.nanolett.6b0475510.1021/acs.nanolett.6b04755 ↗
14. 10.1002/anie.20170209910.1002/anie.201702099 ↗
15. 10.1103/PhysRevA.42.735510.1103/PhysRevA.42.7355 ↗
16. 10.1149/2.028309jes10.1149/2.028309jes ↗
17. 10.1016/j.jpowsour.2014.03.02910.1016/j.jpowsour.2014.03.029 ↗
18. 10.1016/j.electacta.2014.05.12010.1016/j.electacta.2014.05.120 ↗
19. 10.1016/j.elecom.2014.11.00210.1016/j.elecom.2014.11.002 ↗
20. 10.1002/celc.20180165210.1002/celc.201801652 ↗
21. 10.1126/science.aap878710.1126/science.aap8787 ↗
22. 10.1149/1.145413810.1149/1.1454138 ↗
23. 10.1073/pnas.161573311410.1073/pnas.1615733114 ↗
24. 10.1021/acsenergylett.8b0200310.1021/acsenergylett.8b02003 ↗
25. 10.1039/C4CP05786D10.1039/C4CP05786D ↗
26. 10.1021/acsenergylett.9b0043310.1021/acsenergylett.9b00433 ↗
27. 10.1149/1.183756310.1149/1.1837563 ↗
28. 10.1016/j.electacta.2012.12.13110.1016/j.electacta.2012.12.131 ↗
29. 10.1038/s41467-019-09924-110.1038/s41467-019-09924-1 ↗
30. 10.1021/acs.nanolett.5b0243210.1021/acs.nanolett.5b02432 ↗
31. 10.1149/1.314872110.1149/1.3148721 ↗
32. 10.1021/jp068691u10.1021/jp068691u ↗
33. 10.1038/s41586-018-0397-310.1038/s41586-018-0397-3 ↗
34. 10.1007/s10008-017-3610-710.1007/s10008-017-3610-7 ↗
35. 10.1021/ja203983r10.1021/ja203983r ↗
36. 10.1039/C3EE42351D10.1039/C3EE42351D ↗
37. 10.1038/ncomms736210.1038/ncomms7362 ↗
38. 10.1002/crat.217025081410.1002/crat.2170250814 ↗
39. 10.1134/S102319350806004910.1134/S1023193508060049 ↗
40. 10.1063/1.33220910.1063/1.332209 ↗