Source abstract
Abstract
Polyurethane is an important biomaterial with wide applications in biomedical engineering. Here, we report a new method to make an azido-functionalized polyurethane prepolymer with no need of postmodification. This prepolymer can easily form stable porous elastomers through click chemistry for cross-linking, instead of using a toxic polyisocyanate. The mechanical properties can be modulated by simply adjusting either the prepolymer concentrations or azido/alkyne ratios for cross-linking. Young's modulus therefore varies from 0.52 to 2.02 MPa for the porous elastomers. When the azido-functionalized polyurethane elastomer is made with a compact structure, Young's modulus increases up to 28.8 MPa at 0-15% strain. The strain at break reaches 150% that is comparable to the commercially resourced Nylon-12. Both the porous and compact elastomers could undergo reversible elastic deformations for at least 200 and 1000 cycles, respectively, within 20% strain without failure. The material showed a considerable stability against erosion in a basic solution. In vivo biocompatibility study demonstrated no degradation by subcutaneous implantation in mice over 2 months. The implant induced only a mild inflammatory response and fibrotic capsule. This material might be useful to make elastomeric components of biomedical devices.
Source: openalex_inverted_index · Quality: baseline
Affiliations
Nancy E. and Peter C. Meining School of Biomedical Engineering, Cornell University, 277 Kimball Hall, Hollister Drive 134, Ithaca, New York 14853, United States
School of Dental Medicine, University of Pittsburgh, 335 Sutherland Drive, 522 Salk Pavilion, Pittsburgh, Pennsylvania 15260, United States
Department of Chemical Engineering, Arizona State University, 501 E. Tyler Mall, Tempe, Arizona 85287, United States
Department of Chemical and Petroleum Engineering, University of Pittsburgh, 940 Benedum Hall, 3700 O’Hara Street, Pittsburgh, Pennsylvania 15261, United States
Funding
Cornell University