Microtubule‐Templated Biomimetic Mineralization of Lepidocrocite
Source abstract
Abstract
Abstract Protein microtubules (MTs) 25 nm in diameter and tens of micrometers long have been used as templates for the biomimetic mineralization of FeOOH. Exposure of MTs to anaerobic aqueous solutions of Fe2+ buffered to neutral pH followed by aerial oxidation leads to the formation of iron oxide coated MTs. The iron oxide layer was found to grow via a two‐step process: initially formed 10–30 nm thick coatings were found to be amorphous in structure and comprised of several iron‐containing species. Further growth resulted in MTs coated with highly crystalline layers of lepidocrocite with a controllable thickness of up to 125 nm. On the micrometer size scale, these coated MTs were observed to form large, irregular bundles containing hundreds of individually coated MTs. Iron oxide grew selectively on the MT surface, a result of the highly charged MT surface that provided an interface favorable for iron oxide nucleation. This result illustrates that MTs can be used as scaffolds for the in‐situ production of high‐aspect‐ratio inorganic nanowires.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Characterization and Applications of Magnetic Nanoparticles · Micro and Nano Robotics · Iron oxide chemistry and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Biomimetic Materials Chemistry(Ed: S. Mann) VCH New York1996.
2. 10.1021/cm010165m10.1021/cm010165m ↗
3. 10.1021/cm011068w10.1021/cm011068w ↗
4. 10.1126/science.264.5155.4810.1126/science.264.5155.48 ↗
5. 10.1021/ja027954510.1021/ja0279545 ↗
6. 10.1002/1521-3773(20001002)39:19<3392::AID-ANIE3392>3.0.CO;2-M10.1002/1521-3773(20001002)39:19<3392::AID-ANIE3392>3.0.CO;2-M ↗
7. 10.1146/annurev.matsci.31.1.23710.1146/annurev.matsci.31.1.237 ↗
8. 10.1021/cm010110k10.1021/cm010110k ↗
9. 10.1002/anie.20039028410.1002/anie.200390284 ↗
10. 10.1126/science.163608610.1126/science.1636086 ↗
11. 10.1016/S0965-9773(97)00133-510.1016/S0965-9773(97)00133-5 ↗
12. 10.1109/20.90865810.1109/20.908658 ↗
13. 10.1021/ic991269q10.1021/ic991269q ↗
14. 10.1126/science.269.5220.5410.1126/science.269.5220.54 ↗
15. 10.1002/(SICI)1521-4095(199903)11:3<253::AID-ADMA253>3.0.CO;2-710.1002/(SICI)1521-4095(199903)11:3<253::AID-ADMA253>3.0.CO;2-7 ↗
16. 10.1038/3021110.1038/30211 ↗
17. 10.1002/(SICI)1521-4095(199906)11:8<679::AID-ADMA679>3.0.CO;2-J10.1002/(SICI)1521-4095(199906)11:8<679::AID-ADMA679>3.0.CO;2-J ↗
18. 10.1002/1521-4095(20020318)14:6<415::AID-ADMA415>3.0.CO;2-W10.1002/1521-4095(20020318)14:6<415::AID-ADMA415>3.0.CO;2-W ↗
19. 10.1016/S0040-6090(97)00131-410.1016/S0040-6090(97)00131-4 ↗
20. 10.1002/1521-4095(20021118)14:22<1621::AID-ADMA1621>3.0.CO;2-D10.1002/1521-4095(20021118)14:22<1621::AID-ADMA1621>3.0.CO;2-D ↗
21. M. Schliwa The Cytoskeleton: An Introductory Survey Springer‐Verlag; New York1986.
22. Our standard procedure for forming MTs involves the polymerization of 5 mg mL–1α/β‐tubulin solutions in BRB80 (80 mM PIPES 1 mM EGTA 1 mM MgCl2 pH 6.9) containing 1 mM GTP and 10 % glycerol at 37 °C for 20 min followed by stabilization with BRB80 containing 2 μM taxol.
23. J. Howard Mechanics of the Motor Proteins and the Cytoskeleton Sinauer Associates Inc. Sunderland MA2001.
24. 10.1002/(SICI)1521-4095(200004)12:7<507::AID-ADMA507>3.0.CO;2-G10.1002/(SICI)1521-4095(200004)12:7<507::AID-ADMA507>3.0.CO;2-G ↗
25. 10.1002/1521-4095(200112)13:23<1793::AID-ADMA1793>3.0.CO;2-V10.1002/1521-4095(200112)13:23<1793::AID-ADMA1793>3.0.CO;2-V ↗
26. 10.1126/science.107124710.1126/science.1071247 ↗
27. 10.1021/nl03401610.1021/nl034016 ↗
28. 10.1038/3446510.1038/34465 ↗
29. 10.1016/S0092-8674(00)80961-710.1016/S0092-8674(00)80961-7 ↗
30. 10.1016/S0006-291X(02)00251-610.1016/S0006-291X(02)00251-6 ↗
31. The Diatoms(Ed: J. P. Smol) Cambridge University Press Cambridge UK1999.
32. 10.1021/nl025636y10.1021/nl025636y ↗
33. 10.1088/0957-4484/10/3/30210.1088/0957-4484/10/3/302 ↗
34. 10.1021/la026155x10.1021/la026155x ↗
35. U. Schwertmann R. M. Cornell Iron Oxides in the Laboratory VCH New York1991.
36. Full synthetic details can be found in the Supporting Information.
37. The overall length of the coated MTs observed by TEM on the order of a few micrometers was far shorter than that observed in fluorescence microscopy. This may be due to fracturing of the coated tubes while the solution they were cast from dried on the TEM sample grid.
38. Networks resulting from high iron content coating solutions were too thick to be imaged by TEM.
39. These films are likely comprised of the salts contained in the buffer solutions used to prepare the coated MTs and form as part of the sample drying process after deposition onto TEM grids.