Rich Phase Behavior in a Supramolecular Conducting Material Derived from an Organogelator
Source abstract
Abstract
Abstract Organic conducting fiber‐like materials hold great promise for the development of nanowires that can act as connections in miniature electronic devices, as an alternative to inorganic nanometer scale structures. This article presents a conducting organic tetrathiafulvalene‐based supramolecular material which possesses a rich phase behavior with different packing of the molecules in the different forms, evidenced by electron spin resonance (ESR) spectroscopy. The distinct phases of conducting nanofibers can be easily fabricated through the temperature control of their preparation process from a xerogel by doping with iodine vapors. A total of four conducting phases have been identified conclusively using ESR spectroscopy as the key analytical tool. Three of the phases show a good long‐term stability and areas in which the I–V curves have ohmic behavior when studied by current sensing (conducting) AFM. They offer promise for applications where electrical nanometer scale connections are required.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Organic and Molecular Conductors Research · Conducting polymers and applications · Luminescence and Fluorescent Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. 10.1109/TMAG.1987.106500110.1109/TMAG.1987.1065001 ↗
2. 10.1126/science.257.5070.64210.1126/science.257.5070.642 ↗
3. 10.1109/TED.2003.82247110.1109/TED.2003.822471 ↗
4. 10.1038/375767a010.1038/375767a0 ↗
5. 10.1126/science.267.5205.179310.1126/science.267.5205.1793 ↗
6. 10.1126/science.106092810.1126/science.1060928 ↗
7. 10.1002/adma.20040164810.1002/adma.200401648 ↗
8. 10.1002/adfm.20060010610.1002/adfm.200600106 ↗
9. 10.1002/smll.20070024510.1002/smll.200700245 ↗
10. 10.1039/b800289d10.1039/b800289d ↗
11. 10.1002/(SICI)1521-3773(19990517)38:10<1393::AID-ANIE1393>3.0.CO;2-H10.1002/(SICI)1521-3773(19990517)38:10<1393::AID-ANIE1393>3.0.CO;2-H ↗
12. 10.1016/j.eurpolymj.2004.01.04010.1016/j.eurpolymj.2004.01.040 ↗
13. 10.1021/cr030070z10.1021/cr030070z ↗
14. 10.1002/chem.20060132010.1002/chem.200601320 ↗
15. 10.1002/adfm.20070054910.1002/adfm.200700549 ↗
16. 10.1002/anie.20070526010.1002/anie.200705260 ↗
17. 10.1088/0964-1726/6/5/00410.1088/0964-1726/6/5/004 ↗
18. Yurish S. Y. · Sensors Traducers Magazine · 2005 · 62 · 456
19. Reimers J. · 2003
20. 10.1557/mrs2003.14410.1557/mrs2003.144 ↗
21. 10.1071/CH0330710.1071/CH03307 ↗
22. 10.1016/j.synthmet.2004.08.00610.1016/j.synthmet.2004.08.006 ↗
23. 10.1039/b501804h10.1039/b501804h ↗
24. 10.1021/cr970028210.1021/cr9700282 ↗
25. 10.1081/E-ESMC-12001387910.1081/E-ESMC-120013879 ↗
26. 10.1002/chem.20050024110.1002/chem.200500241 ↗
27. 10.1039/b417081b10.1039/b417081b ↗
28. Smith D. K. · 2008
29. 10.1021/jo00099a01210.1021/jo00099a012 ↗
30. 10.1021/ja055203810.1021/ja0552038 ↗
31. 10.1021/ja055800u10.1021/ja055800u ↗
32. 10.1021/ja053496z10.1021/ja053496z ↗
33. 10.1002/anie.20060248310.1002/anie.200602483 ↗
34. 10.1002/anie.20070486410.1002/anie.200704864 ↗
35. 10.1021/cr030664210.1021/cr0306642 ↗
36. 10.1246/bcsj.80.110.1246/bcsj.80.1 ↗
37. 10.1039/B703825A10.1039/B703825A ↗
38. 10.1002/chem.20060108910.1002/chem.200601089 ↗
39. 10.1002/cphc.20070019810.1002/cphc.200700198 ↗
40. 10.1021/ja028012310.1021/ja0280123 ↗
41. Williams J. M. · 1992
42. The melting temperature of the powder form of compound1is 377.4 K. However the xerogel does not display such a sharp melting temperature. It is a liquid at this melting point for the powder but no differential scanning calorimetric or optical micrographic evidence indicated any sharp phase change or obvious change in morphology between room temperature and the powder melting point. At 353 K the lowest temperature at which the delta phase was formed and which is 20 K below the melting temperature of the powder there is no evidence in the xerogel of melt behavior. Once the doped form (a salt) is created the melting temperature is over 423 K. The nature of the mechanism of formation of the doped material at high temperature will be the subject of further work.
43. 10.1103/PhysRevB.35.250110.1103/PhysRevB.35.2501 ↗
44. 10.1021/ic00126a02710.1021/ic00126a027 ↗
45. 10.1039/b102786g10.1039/b102786g ↗
46. 10.1039/b008735l10.1039/b008735l ↗
47. 10.1021/cm034866q10.1021/cm034866q ↗
48. 10.1103/PhysRevB.71.08520210.1103/PhysRevB.71.085202 ↗
49. 10.1016/0379-6779(89)90779-010.1016/0379-6779(89)90779-0 ↗
50. Buravov L. I. · Mater. Sci. · 1988 · 14 · 17
51. 10.1016/S0010-8545(98)00238-010.1016/S0010-8545(98)00238-0 ↗
52. 10.1080/1058725010802367010.1080/10587250108023670 ↗
53. 10.1039/B716533A10.1039/B716533A ↗