Improvement of Low‐Temperature zT in a Mg3Sb2–Mg3Bi2 Solid Solution via Mg‐Vapor Annealing
Source abstract
Abstract
Abstract Materials with high zT over a wide temperature range are essential for thermoelectric applications. n‐Type Mg3Sb2‐based compounds have been shown to achieve high zT at 700 K, but their performance at low temperatures (<500 K) is compromised due to their highly resistive grain boundaries. Syntheses and optimization processes to mitigate this grain‐boundary effect has been limited due to loss of Mg, which hinders a sample's n‐type dopability. A Mg‐vapor anneal processing step that grows a sample's grain size and preserves its n‐type carrier concentration during annealing is demonstrated. The electrical conductivity and mobility of the samples with large grain size follows a phonon‐scattering‐dominated T−3/2 trend over a large temperature range, further supporting the conclusion that the temperature‐activated mobility in Mg3Sb2‐based materials is caused by resistive grain boundaries. The measured Hall mobility of electrons reaches 170 cm2 V−1 s−1 in annealed 800 °C sintered Mg3 + δSb1.49Bi0.5Te0.01, the highest ever reported for Mg3Sb2‐based thermoelectric materials. In particular, a sample with grain size >30 mm has a zT 0.8 at 300 K, which is comparable to commercial thermoelectric materials used at room temperature (n‐type Bi2Te3) while reaching zT 1.4 at 700 K, allowing applications over a wider temperature scale.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal Radiation and Cooling Technologies · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Science & Engineering (MSE) Northwestern University Evanston IL 60208 USA
Funding
National Aeronautics and Space Administration · Materials Research Science and Engineering Center, Harvard University
References (33)
Show source-provided references
1. Snyder G. J. · 2011 · 101
2. 10.1039/C7EE02007D10.1039/C7EE02007D ↗
3. 10.1002/adma.20160395510.1002/adma.201603955 ↗
4. 10.1039/C7EE00098G10.1039/C7EE00098G ↗
5. 10.1038/ncomms1390110.1038/ncomms13901 ↗
6. 10.1039/C7EE03326E10.1039/C7EE03326E ↗
7. 10.1063/1.501648810.1063/1.5016488 ↗
8. 10.1016/j.joule.2017.11.00510.1016/j.joule.2017.11.005 ↗
9. May A. F. · 2017 · 11‐1
10. Marlow Industries private communication unpublished.
11. Warzecha M. · 2012 · 012004
12. 10.1063/1.172899010.1063/1.1728990 ↗
13. 10.1063/1.171275110.1063/1.1712751 ↗
14. 10.1016/j.jallcom.2004.11.01710.1016/j.jallcom.2004.11.017 ↗
15. 10.1007/s10853-011-5393-z10.1007/s10853-011-5393-z ↗
16. 10.1039/C8TA08975B10.1039/C8TA08975B ↗
17. 10.1103/PhysRev.88.86710.1103/PhysRev.88.867 ↗
18. 10.1063/1.32633410.1063/1.326334 ↗
19. 10.1073/pnas.171172511410.1073/pnas.1711725114 ↗
20. 10.1007/BF0286832010.1007/BF02868320 ↗
21. 10.1021/j150079a00510.1021/j150079a005 ↗
22. 10.1002/zaac.1930190010910.1002/zaac.19301900109 ↗
23. Grube G. · Z. Elektrochem. Angew. Phys. Chem. · 1934 · 40 · 143
24. 10.1007/BF0287118810.1007/BF02871188 ↗
25. 10.1016/B978-0-12-401682-8.00007-010.1016/B978-0-12-401682-8.00007-0 ↗
26. 10.1179/02670830110151031110.1179/026708301101510311 ↗
27. 10.1016/j.jallcom.2008.10.06110.1016/j.jallcom.2008.10.061 ↗
28. 10.31399/asm.tb.pdub.978162708310210.31399/asm.tb.pdub.9781627083102 ↗
29. Callister W. D. · 2007
30. 10.1063/1.353408010.1063/1.3534080 ↗
31. 10.1039/C4EE01320D10.1039/C4EE01320D ↗
32. 10.1063/1.360135810.1063/1.3601358 ↗
33. 10.1016/j.mtphys.2018.10.00110.1016/j.mtphys.2018.10.001 ↗