Epitaxial Ferroelectric Heterostructures Fabricated by Selective Area Epitaxy of SrRuO3 Using an MgO Mask

J. Karthik, Anoop R. Damodaran, Lane W. Martin

Advanced Materials· Volume 24· Issue 12

Abstract

Illustration of a new high-temperature hard-mask process based on traditional lithography and selective wet-etching of MgO. The hard mask is compatible with standard nano-lithography techniques and heat treatments in excess of 1000 °C. Here, this technique is applied to produce temperature-stable contacts that give rise to low leakage, improved fatigue properties, and excellent high-temperature stability in ferroelectric thin-film capacitors. Detailed facts of importance to specialist readers are published as ”Supporting Information”. Such documents are peer-reviewed, but not copy-edited or typeset. They are made available as submitted by the authors. Please note: The publisher is not responsible for the content or functionality of any supporting information supplied by the authors. Any queries (other than missing content) should be directed to the corresponding author for the article.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Electronic and Structural Properties of Oxides · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. 10.1007/978-3-662-04307-310.1007/978-3-662-04307-3 ↗
2. 10.1021/nl071804g10.1021/nl071804g ↗
3. 10.1557/mrs2008.22110.1557/mrs2008.221 ↗
4. 10.1103/RevModPhys.77.108310.1103/RevModPhys.77.1083 ↗
5. 10.1126/science.112956410.1126/science.1129564 ↗
6. 10.1063/1.34441910.1063/1.344419 ↗
7. 10.1126/science.116863610.1126/science.1168636 ↗
8. 10.1038/nnano.2009.45110.1038/nnano.2009.451 ↗
9. 10.1063/1.319724610.1063/1.3197246 ↗
10. 10.1126/science.118186210.1126/science.1181862 ↗
11. 10.1109/TCAD.2002.80438510.1109/TCAD.2002.804385 ↗
12. Huang W. · 2005
13. 10.1146/annurev.matsci.37.061206.11301610.1146/annurev.matsci.37.061206.113016 ↗
14. 10.1016/j.mser.2010.03.00110.1016/j.mser.2010.03.001 ↗
15. 10.1063/1.12593810.1063/1.125938 ↗
16. 10.1063/1.138154210.1063/1.1381542 ↗
17. 10.1143/JJAP.39.211010.1143/JJAP.39.2110 ↗
18. 10.1063/1.176574210.1063/1.1765742 ↗
19. 10.1103/PhysRevLett.96.10760310.1103/PhysRevLett.96.107603 ↗
20. 10.1063/1.217410010.1063/1.2174100 ↗
21. 10.1038/nmat242910.1038/nmat2429 ↗
22. 10.1063/1.36012210.1063/1.360122 ↗
23. 10.1063/1.162173110.1063/1.1621731 ↗
24. 10.1038/nature0150110.1038/nature01501 ↗
25. 10.1126/science.109825210.1126/science.1098252 ↗
26. 10.1063/1.11043610.1063/1.110436 ↗
27. 10.1063/1.137194710.1063/1.1371947 ↗
28. 10.1103/PhysRevB.75.10410310.1103/PhysRevB.75.104103 ↗
29. 10.1364/JOSAB.22.00009610.1364/JOSAB.22.000096 ↗
30. 10.1126/science.110321810.1126/science.1103218 ↗
31. 10.1038/nmat243210.1038/nmat2432 ↗
32. The films were grown at 630 °C with the SrRuO3bottom electrode and PbZr0.2Ti0.8O3layers being grown in 100 and 200 mTorr of oxygen laser repetition rates of 12 and 3 Hz and laser fluences of 1.75 and 2 J/cm2 respectively. Following growth films are cooled to room temperature at an oxygen pressure of 760 Torr.
33. 10.1063/1.302129310.1063/1.3021293 ↗
34. 10.1038/nnano.2008.16110.1038/nnano.2008.161 ↗
35. 10.1063/1.347496010.1063/1.3474960 ↗
36. 10.1007/s00339005004110.1007/s003390050041 ↗
37. 10.1080/1058458950801290610.1080/10584589508012906 ↗
38. 10.1103/PhysRevB.82.17412510.1103/PhysRevB.82.174125 ↗
39. 10.1063/1.187012610.1063/1.1870126 ↗
40. 10.1143/JJAP.42.594110.1143/JJAP.42.5941 ↗
41. 10.1063/1.12482010.1063/1.124820 ↗
42. 10.1063/1.12415810.1063/1.124158 ↗
43. 10.1063/1.132727910.1063/1.1327279 ↗
44. 10.1143/JJAP.39.545110.1143/JJAP.39.5451 ↗
45. 10.1063/1.33045510.1063/1.330455 ↗