Toward Design Rules for Multilayer Ferroelectric Energy Storage Capacitors – A Study Based on Lead‐Free and Relaxor‐Ferroelectric/Paraelectric Multilayer Devices
Source abstract
Abstract
Abstract Future pulsed‐power electronic systems based on dielectric capacitors require the use of environment‐friendly materials with high energy‐storage performance that can operate efficiently and reliably in harsh environments. Here, a study of multilayer structures, combining paraelectric‐like Ba0.6Sr0.4TiO3 (BST) with relaxor‐ferroelectric BaZr0.4Ti0.6O3 (BZT) layers on SrTiO3‐buffered Si substrates, with the goal to optimize the high energy‐storage performance is presented. The energy‐storage properties of various stackings are investigated and an extremely large maximum recoverable energy storage density of ≈165.6 J cm−3 (energy efficiency ≈ 93%) is achieved for unipolar charging–discharging of a 25‐nm‐BZT/20‐nm‐BST/910‐nm‐BZT/20‐nm‐BST/25‐nm‐BZT multilayer structure, due to the extremely large breakdown field of 7.5 MV cm−1 and the lack of polarization saturation at high fields in this device. Strong indications are found that the breakdown field of the devices is determined by the outer layers of the multilayer stack and can be increased by improving the quality of these layers. Authors are also able to deduce design optimization rules for this material combination, which can be to a large extend justify by structural analysis. These rules are expected also to be useful for optimizing other multilayer systems and are therefore very relevant for further increasing the energy storage density of capacitors.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Acoustic Wave Resonator Technologies · Ferroelectric and Piezoelectric Materials · Innovative Energy Harvesting Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
MESA+ Institute for Nanotechnology University of Twente P.O. Box 217, 7500 AE Enschede The Netherlands
International Training Institute for Materials Science (ITIMS) Hanoi University of Science and Technology 1 Dai Co Viet Road Hanoi 100000 Vietnam
Funding
University of Twente
References (70)
Show source-provided references
1. 10.1143/JPSJ.7.510.1143/JPSJ.7.5 ↗
2. 10.1143/JPSJ.7.1210.1143/JPSJ.7.12 ↗
3. 10.1038/s41598-020-67651-w10.1038/s41598-020-67651-w ↗
4. 10.1063/1.304032610.1063/1.3040326 ↗
5. 10.1063/5.009012010.1063/5.0090120 ↗
6. 10.1063/5.003551510.1063/5.0035515 ↗
7. 10.1039/C3EE42540A10.1039/C3EE42540A ↗
8. 10.35848/1347-4065/abbfa010.35848/1347-4065/abbfa0 ↗
9. 10.1063/5.000662010.1063/5.0006620 ↗
10. 10.1002/ente.20190063810.1002/ente.201900638 ↗
11. 10.1021/acsami.1c1404810.1021/acsami.1c14048 ↗
12. 10.1116/6.000092310.1116/6.0000923 ↗
13. 10.1038/s41563-020-0725-510.1038/s41563-020-0725-5 ↗
14. 10.1016/j.jallcom.2015.12.26010.1016/j.jallcom.2015.12.260 ↗
15. 10.1039/C6RA11744A10.1039/C6RA11744A ↗
16. 10.1007/s10854-021-06542-w10.1007/s10854-021-06542-w ↗
17. 10.1063/1.500098010.1063/1.5000980 ↗
18. 10.1111/jace.1780810.1111/jace.17808 ↗
19. 10.1007/s10854-017-7521-210.1007/s10854-017-7521-2 ↗
20. 10.1063/5.005604110.1063/5.0056041 ↗
21. 10.1038/s41598-018-21305-010.1038/s41598-018-21305-0 ↗
22. 10.1103/PhysRevLett.103.25760210.1103/PhysRevLett.103.257602 ↗
23. 10.1021/acsami.6b1647010.1021/acsami.6b16470 ↗
24. 10.1002/adfm.20180719610.1002/adfm.201807196 ↗
25. 10.1016/j.ensm.2019.10.01510.1016/j.ensm.2019.10.015 ↗
26. 10.1002/aenm.20180304810.1002/aenm.201803048 ↗
27. 10.1007/s40820-023-01036-210.1007/s40820-023-01036-2 ↗
28. 10.1016/j.nanoen.2023.10845810.1016/j.nanoen.2023.108458 ↗
29. 10.1038/s41560-023-01300-010.1038/s41560-023-01300-0 ↗
30. 10.1038/s41563-022-01274-610.1038/s41563-022-01274-6 ↗
31. 10.1038/s41467-022-30821-710.1038/s41467-022-30821-7 ↗
32. 10.1111/j.1551-2916.2008.02442.x10.1111/j.1551-2916.2008.02442.x ↗
33. 10.1142/S2010135X1550002210.1142/S2010135X15500022 ↗
34. 10.1016/j.cplett.2020.13800810.1016/j.cplett.2020.138008 ↗
35. 10.1088/1361-648X/aba38410.1088/1361-648X/aba384 ↗
36. 10.1016/j.ceramint.2019.09.20810.1016/j.ceramint.2019.09.208 ↗
37. 10.1016/j.jmat.2021.01.01210.1016/j.jmat.2021.01.012 ↗
38. 10.1016/j.materresbull.2020.11107210.1016/j.materresbull.2020.111072 ↗
39. 10.1103/PhysRevB.81.21411910.1103/PhysRevB.81.214119 ↗
40. 10.1039/C7TA10271B10.1039/C7TA10271B ↗
41. 10.1002/adma.20160442710.1002/adma.201604427 ↗
42. 10.1016/j.nanoen.2020.10486210.1016/j.nanoen.2020.104862 ↗
43. 10.1039/C9RA10030J10.1039/C9RA10030J ↗
44. 10.1021/acsami.1c0127510.1021/acsami.1c01275 ↗
45. 10.1016/j.ensm.2021.04.01010.1016/j.ensm.2021.04.010 ↗
46. 10.1002/adma.20230255410.1002/adma.202302554 ↗
47. 10.1002/aenm.20220051710.1002/aenm.202200517 ↗
48. 10.1039/C8TA09396B10.1039/C8TA09396B ↗
49. 10.1177/002199831244902910.1177/0021998312449029 ↗
50. 10.1143/JPSJ.7.52810.1143/JPSJ.7.528 ↗
51. 10.1016/S1369-7021(07)70349-810.1016/S1369-7021(07)70349-8 ↗
52. 10.1021/acsami.6b0642510.1021/acsami.6b06425 ↗
53. 10.1021/acs.inorgchem.7b0120510.1021/acs.inorgchem.7b01205 ↗
54. 10.1107/S056773947600155110.1107/S0567739476001551 ↗
55. In the Supporting Information we analyzed the polarization values at 2 MV cm−1and modeled this interface effect by introducing zero‐polarization interfacial layers adjacent to layers with bulk polarization values (i.e. equal to that in the single layer films see Section 4 Supporting Information). The zero‐polarization interfacial layers could be estimated to be 31 nm and 82 nm thick for the BZT respectively BST layers at 2 MV cm−1. This reflects the above‐deduced strain relaxation layer thicknesses in these materials in the multilayer.
56. Note that the breakdown field is slightly lower for bipolar cycling than for the lowest unipolar cycling measurement method. We speculate that the positive half of the cycle enhances the breakdown field of the top electrode interface by displacing trapped charges at that interface.
57. 10.1038/s41598-020-64451-010.1038/s41598-020-64451-0 ↗
58. 10.1039/c3ee43526a10.1039/c3ee43526a ↗
59. 10.1088/2631-7990/abba1210.1088/2631-7990/abba12 ↗
60. 10.1021/acsami.8b0534710.1021/acsami.8b05347 ↗
61. 10.1016/j.ceramint.2015.09.12210.1016/j.ceramint.2015.09.122 ↗
62. 10.1016/j.jallcom.2014.02.13710.1016/j.jallcom.2014.02.137 ↗
63. 10.1016/j.jallcom.2023.17183710.1016/j.jallcom.2023.171837 ↗
64. 10.1021/acsami.6b1001610.1021/acsami.6b10016 ↗
65. 10.1016/j.nanoen.2018.10.02810.1016/j.nanoen.2018.10.028 ↗
66. 10.1038/srep4091610.1038/srep40916 ↗
67. 10.1021/acsenergylett.1c0031310.1021/acsenergylett.1c00313 ↗
68. 10.1126/science.abi768710.1126/science.abi7687 ↗
69. 10.1016/j.jmat.2020.01.01010.1016/j.jmat.2020.01.010 ↗
70. 10.1016/j.jmat.2023.03.00710.1016/j.jmat.2023.03.007 ↗