journal article·2026-01Open access

Self‐Evolving Gradient Alloy Layer Enables Stable Al Foil Anode for High Energy Lithium Batteries

Sihai Bi, Ruopeng Li, Serhii Kuksenko, Penghui Ren, Meiyan Sun, Yaqiang Li, Xiaona Pan, Guangzhao Wang, Jiang Qin, Anmin Liu, Jinqiu Zhang, Maozhong An, Peixia Yang, Yuanpeng Liu

Advanced Materials· Volume 38· Issue 6

Abstract

Abstract Aluminum (Al) foil anodes, alloyed with lithium (Li), offer a theoretical capacity of 993 mAhg −1 and are considered promising candidates for next‐generation high‐energy‐density lithium‐ion batteries (LIBs). However, their practical application is hindered by non‐uniform alloying processes initiated by the native Al 2 O 3 passivation layer, leading to severe structural degradation and electrode pulverization. Here, a self‐evolving gradient alloy strategy is proposed that enables uniform Li alloying through the in situ construction of a lithiophilic zinc (Zn) interfacial layer on commercial Al foil via a scalable electroless plating process. The Zn interlayer initiates a low‐barrier, sequential alloying pathway—from LiZn to LiAl—thereby promoting uniform lithium infusion, suppressing stress accumulation, and stabilizing the solid–electrolyte interphase (SEI). As a result, the Al@Zn anode achieves an ultralong cycling lifespan with a high Coulombic efficiency of 99.92% over 11 800 cycles, and powers full cells delivering an energy density of 452 Wh kg −1 . Comprehensive structural, electrochemical, and theoretical analyses confirm that the Zn‐guided interfacial gradient effectively mitigates mechanical failure and interfacial instability. This work presents a practical and scalable interfacial engineering approach toward stable, high‐performance alloy‐type anodes, paving the way for the next generation of lithium‐ion batteries.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

MIIT Key Laboratory of Critical Materials Technology for New Energy Conversion and Storage School of Chemistry and Chemical Engineering Harbin Institute of Technology Harbin Heilongjiang 150001 P. R. China

Zhengzhou Research Institute Harbin Institute of Technology Zhengzhou 450000 P. R. China

Shandong Laboratory of Advanced Materials and Green Manufacturing at Yantai Yantai 264000 P. R. China

College of Chemistry Institute of Molecular Engineering Plus Fuzhou University Fuzhou Fujian 350116 P. R. China

School of Chemistry and Chemical Engineering State Key Laboratory of Crystal Materials Shandong University Jinan 250100 P. R. China

Key Laboratory of Extraordinary Bond Engineering and Advanced Materials Technology of Chongqing School of Electronic Information Engineering Yangtze Normal University Chongqing 408100 P. R. China

School of Energy Science and Engineering, Harbin Institute of Technology Harbin 150001 P. R. China

School of Chemical Engineering Ocean and Life Sciences Leicester International Institute Dalian University of Technology 2 Dagong Road Liaodongwan New District Panjin Liaoning 124221 P. R. China

National Key Laboratory of Science and Technology on Advanced Composites in Special Environments, and Center for Composite Materials and Structures Harbin 150001 P. R. China

Funding

National Natural Science Foundation of China

References (48)

Show source-provided references
1. 10.1038/3510464410.1038/35104644 ↗
2. 10.1038/451652a10.1038/451652a ↗
3. 10.1038/s41586-021-03772-010.1038/s41586-021-03772-0 ↗
4. 10.1126/science.121274110.1126/science.1212741 ↗
5. 10.1038/s41560-019-0474-310.1038/s41560-019-0474-3 ↗
6. 10.1038/s41467-020-15452-010.1038/s41467-020-15452-0 ↗
7. 10.1002/adfm.20231634110.1002/adfm.202316341 ↗
8. 10.1016/j.actamat.2007.12.00210.1016/j.actamat.2007.12.002 ↗
9. 10.1149/2.038201jes10.1149/2.038201jes ↗
10. 10.1021/nn204476h10.1021/nn204476h ↗
11. 10.1002/adma.20240262610.1002/adma.202402626 ↗
12. 10.1021/acsenergylett.1c0246110.1021/acsenergylett.1c02461 ↗
13. 10.1038/nnano.2007.41110.1038/nnano.2007.411 ↗
14. 10.1021/ja906261c10.1021/ja906261c ↗
15. 10.1021/ja103199710.1021/ja1031997 ↗
16. 10.1038/nnano.2012.3510.1038/nnano.2012.35 ↗
17. 10.1039/C5EE01363A10.1039/C5EE01363A ↗
18. 10.1038/nchem.180210.1038/nchem.1802 ↗
19. 10.1016/S0167-2738(00)00362-310.1016/S0167-2738(00)00362-3 ↗
20. 10.1002/aenm.20110038010.1002/aenm.201100380 ↗
21. 10.1016/j.msea.2012.08.10610.1016/j.msea.2012.08.106 ↗
22. 10.1007/s42114-019-00115-610.1007/s42114-019-00115-6 ↗
23. 10.1016/j.msea.2018.08.06010.1016/j.msea.2018.08.060 ↗
24. 10.1016/j.mtadv.2025.10058110.1016/j.mtadv.2025.100581 ↗
25. 10.1002/adma.20240111410.1002/adma.202401114 ↗
26. 10.1002/adma.20240764810.1002/adma.202407648 ↗
27. Wang S. · Nat. Mater. · 2025
28. 10.1016/j.cej.2021.13357210.1016/j.cej.2021.133572 ↗
29. 10.1021/acsenergylett.3c0045510.1021/acsenergylett.3c00455 ↗
30. 10.1002/anie.20230497810.1002/anie.202304978 ↗
31. 10.1039/D0TA06694J10.1039/D0TA06694J ↗
32. 10.1021/acsami.9b0281310.1021/acsami.9b02813 ↗
33. 10.1016/j.ssi.2022.11608110.1016/j.ssi.2022.116081 ↗
34. 10.1002/anie.20200659510.1002/anie.202006595 ↗
35. 10.1002/adma.20190082610.1002/adma.201900826 ↗
36. 10.1038/s41586-025-09153-110.1038/s41586-025-09153-1 ↗
37. 10.1038/s41467-023-39685-x10.1038/s41467-023-39685-x ↗
38. 10.1038/s41467-024-45613-410.1038/s41467-024-45613-4 ↗
39. 10.1002/anie.20250209110.1002/anie.202502091 ↗
40. 10.1016/j.joule.2023.11.01210.1016/j.joule.2023.11.012 ↗
41. 10.1002/anie.20242353110.1002/anie.202423531 ↗
42. 10.1038/s41557-024-01689-510.1038/s41557-024-01689-5 ↗
43. 10.1038/s41467-019-13436-310.1038/s41467-019-13436-3 ↗
44. Li S. · Angew. Chem.‐Int. Edit. · 2025
45. 10.1007/s40820-025-01751-y10.1007/s40820-025-01751-y ↗
46. 10.1016/j.joule.2025.10193010.1016/j.joule.2025.101930 ↗
47. 10.1039/C9TA01708A10.1039/C9TA01708A ↗
48. 10.1093/nsr/nwaf12410.1093/nsr/nwaf124 ↗