Influence of Contact Load on the Dry Sliding Wear Performance of 7075 Aluminum Alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Williamson J (1981) Steve, Casing wear: the effect of contact pressure. J. Pet. Technol. 33(12):2382–238810.2118/10236-PA ↗
2. White JP, Dawson R (1987) Casing wear: laboratory measurements and field predictions. SPE Drill. Eng. 2(01):56–6210.2118/14325-PA ↗
3. Hao Y, Lian Z, Lin T, Xu X (2016) Experimental and numerical study on casing wear in highly deviated drilling for oil and gas. Adv. Mech. Eng. 8(7)10.1177/1687814016656535 ↗
4. Shen Z, Beck FE (2012) Intermediate casing collapse induced by casing wear in high-temperature and high-pressure wells. Soc. Pet. Eng.10.2118/155973-MS ↗
5. Chu S, Zhang L, Fan J, Yu H (2009) Experimental study of casing wear under impact-sliding conditions. Pet. Sci. 04:445–45010.1007/s12182-009-0068-y ↗
6. Mao L, Cai M, Liu Q, Wang X, Fan Y, He Y, Wang G (2020) Effects of nano-SiO2 addition in drilling fluid on wear behavior of 2Cr13 steel casing. Tribol. Let. 68(1):1–1610.1007/s11249-019-1243-y ↗
7. Hao Y, Taleghani AD, Lian Z (2018) Modelling casing wear at doglegs by incorporating alternate accumulative wear. J. Pet. Sci. Eng. 168:273–28210.1016/j.petrol.2018.05.009 ↗
8. Bol GM (1986) Effect of mud composition on wear and friction of casing and tool joints. SPE Drill. Eng. 1(2005):369–37610.2118/13457-PA ↗
9. Xu QC, Liu QL, Hou W, Gang PU, Wang WD (2007) Discussion on Sichuan gas drilling technology. NGI 27:60–62
10. Jiao AY, Zhang LL, Liu XL, Chen Y (2019) Experimental study of deburring in Al 7075 cross-hole edge based on magnetic particles grinding. Surf. Technol. 48:302–309
11. Yin JH, Lin XX, Meng XX, Zuo JY (2019) Formation mechanism of a sawtooth chip in highspeed milling of aeronautical aluminum alloy 7075-T651, Surf. Technol
12. Wu J, Cheng XQ, Xia QX, Li JY (2017) Experimental research on the influence of restraint layer materials on surface strengthening of 7075 aluminum alloy laser shot peening. Surf. Technol. 46(3):124–129
13. Yuan R, Yang S, Zhao C, Dong G (2015) Mechanics analysis on hot granule medium pressure forming process for AA7075-T6 cylindrical parts, China. Mech. Eng. 26:3240–3248
14. Santus C (2008) Fretting fatigue of aluminum alloy in contact with steel in oil drill pipe connections, modeling to interpret test results. Int. J. Fatigue 30(4):677–68810.1016/j.ijfatigue.2007.05.006 ↗
15. Baradeswaran A, Perumal AE (2015) Effect of graphite on tribological and mechanical properties of AA7075 composites. Tribol. Trans. 58(1):1–610.1080/10402004.2014.947663 ↗
16. Venkataraman B, Sundararajan G (2000) Correlation between the characteristics of the mechanically mixed layer and wear behaviour of aluminium, Al-7075 alloy and Al-MMCs. Wear 245(1-2):22–3810.1016/S0043-1648(00)00463-4 ↗
17. Lu J, Song YL, Hua L, Zhou P, Xie GJ (2019) Effect of temperature on friction and galling behavior of 7075 aluminum alloy sheet based on ball-on-plate sliding test. Tribol. Int. 140:10587210.1016/j.triboint.2019.105872 ↗
18. Avcu E (2017) The influences of ECAP on the dry sliding wear behaviour of AA7075 aluminium alloy. Tribol. Int. 110:173–18410.1016/j.triboint.2017.02.023 ↗
19. Mao L, Cai M, Liu Q, He Y (2019) Effects of sliding speed on the tribological behavior of AA 7075 petroleum casing in simulated drilling environment. Tribol. Int. 145:10619410.1016/j.triboint.2020.106194 ↗
20. Mao L, Cai M, Wang G (2018) Effect of rotation speed on the abrasive-erosive-corrosive wear of steel pipes against steel casings used in drilling for petroleum. Wear 410–411:1–1010.1016/j.wear.2018.06.002 ↗
21. Gao D, Sun L, Lian J (2010) Prediction of casing wear in extended-reach drilling. Pet. Sci. 7(4):494–50110.1007/s12182-001-0098-6 ↗
22. Hall R, Malloy K (2005) Contact pressure threshold: an important new aspect of casing Wear10.2118/94300-MS ↗
23. Kato H, Todaka Y, Umemoto M, Haga M, Sentoku E (2015) Sliding wear behavior of sub-microcrystalline pure iron produced by high-pressure torsion straining. Wear 336–337:58–6810.1016/j.wear.2015.04.014 ↗
24. Zhang Q, Chen K, Wang L, Cui X, Wang S (2013) Characteristics of oxidative wear and oxidative mild wear. Tribol Int 61:214–22310.1016/j.triboint.2013.01.003 ↗
25. Podgornik B, Hogmark S, Pezdirnik J (2004) Comparison between different test methods for evaluation of galling properties of surface engineered toolsur-faces. Wear 257(7–8):843–85110.1016/j.wear.2004.05.005 ↗
26. Mahammad AS, Brahma RG (2019) Development of highly wear resistant Cu-Al alloys processed via powder metallurgy. Tribol Int 136:127–13910.1016/j.triboint.2019.03.055 ↗
27. Chen M, Shi XH, Yang H, Liaw PK, Gao MC, Hawk JA, Jeffrey A, Qiao J (2018) Wear behavior of Al0.6CoCrFeNi high-entropy alloys: effect of environments. Mater. Res. 33(19):1–1110.1557/jmr.2018.279 ↗
28. Wang S, Li X, Zhou Y, Ji X, Li Y (2015) Effects of sliding velocity on tribo-oxides and wear behavior of Ti-6Al-4V alloy. Tribol. Int. 91:228–23410.1016/j.triboint.2015.02.009 ↗
29. Bowden FP, Tabor D (1996) Friction, Lubrication and wear: a survey of work during the last decade. Br. J. Appl. Phys. 17(12):152110.1088/0508-3443/17/12/301 ↗
30. Wang LL, Li XX, Zhou Y, Zhang QY, Chen KM, Wang SQ (2015) Relations of counterface materials with stability of tribo-oxide layer and wear behavior of Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy. Tribol. Int. 91:246–25710.1016/j.triboint.2015.01.028 ↗
31. Dwivedi DK (2010) Adhesive wear behavior of cast aluminum–silicon alloys: Overview. Mate. Des. 31(5):2517–253110.1016/j.matdes.2009.11.038 ↗
32. Xu Z, Shi X, Zhang Q, Zhai W, Li X, Chen L, Zhu Q, Xiao Y (2014) Effect of sliding speed and applied load on dry siding tribological performance of TiAl matrix self-lubricating composites. Tribol. Lett. 55(3):393–40410.1007/s11249-014-0367-3 ↗
33. Alidokht SA, Abdollah-zadeh A, Assadi H (2013) Effect of applied load on the dry sliding wear behavior and the subsurface deformation on hybrid metal matrix composite. Wear 35(1-2):291–29810.1016/j.wear.2012.11.043 ↗
34. Kim DW, Kim KW (2013) Effects of sliding velocity and normal load on friction and wear characteristics of multi-layered diamond-like carbon (DLC) coating prepared by reactive sputtering. Wear 297(1-2):722–73010.1016/j.wear.2012.10.009 ↗
35. Rigney DA (1997) Comments on the sliding wear of metals. Tribol Int 30(5):361–36710.1016/S0301-679X(96)00065-5 ↗
36. Wang L, He Y, Zhou J, Duszczyk J (2010) Effect of temperature on the frictional behavior of an aluminum alloy sliding against steel during ball-on-disc tests. Tribol Int 43:299–30610.1016/j.triboint.2009.06.009 ↗
37. Gali OA, Riahi AR, Alpas AT (2013) The tribological behavior of AA5083 alloy plastically deformed at warm forming temperatures. Wear 302:1257–126710.1016/j.wear.2012.12.048 ↗
38. Wang J, Liu Y, Liu B, Yan W, Cao Y, Li T, Rui Z (2017) Flow behavior and microstructures of powder metallurgical CrFeCoNiMo0.2 high entropy alloy during high-temperature deformation. Mater. Sci. Eng. 689(Mar 24):233–24210.1016/j.msea.2017.02.064 ↗