journal article·2019-09

Tensile properties of two-dimensional carbon fiber reinforced silicon carbide composites at temperatures up to 1800 ° C in air

Tianbao Cheng, Rubing Zhang, Yongmao Pei, Shigang Ai, Rujie He, Yunong Zhao, Daining Fang, Yazheng Yang

Publisher page

Abstract

Abstract Carbon fiber reinforced silicon carbide (C/SiC) composites usually serve in ultra-high-temperature extreme environments and are subjected to thermal-mechanical-oxidation coupled loads. However, the mechanical properties of C/SiC composites reported in the literature are mainly limited to room and moderate temperatures. In this work, the tensile properties of a two-dimensional plain-weave C/SiC composite are studied in air up to 1800 ° C for the first time. C/SiC composite shows linear deformation characteristic initially and then strong nonlinear deformation behavior under the tensile load at room temperature. This is because that the initial defects and cracks propagate and result in the interfacial debonding and sliding. The nonlinear deformation behavior decreases as temperature increases because of the reduced thermal residual stresses. The Young’s modulus increases up to 1000 ° C and then decreases as temperature increases. The tensile strength shows weaker temperature dependence than Young’s modulus because that oxidation reduces the strength at elevated temperatures. The failure mechanisms being responsible for the mechanical behavior are gained through macro and micro analysis. The results are useful for the applications of C/SiC composites in the thermal structure engineering.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Energetic Materials and Combustion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Progress in research work of new CMC-SiC
2. Processing and properties of self-healing C/SiC ceramic matrix composites
3. Zhang · 2009
4. Ablation behavior of C/SiC composites in plasma wind tunnel10.1016/j.carbon.2016.02.085 ↗
5. Carbon fiber reinforced silicon carbide composite-based sharp leading edges in high enthalpy plasma flows10.1016/j.compositesb.2017.09.060 ↗
6. Bansal · 2005
7. Krenkel · 2008
8. Bansal · 2015
9. Mechanical properties of two plain-woven chemical vapor infiltrated silicon carbide-matrix composites10.1111/j.1151-2916.2001.tb00788.x ↗
10. Damage characteristics and constitutive modeling of the 2D C/SiC composite: Part I – Experiment and analysis10.1016/j.cja.2014.10.026 ↗
11. Research of tensile performance of 2D weave C/SiC composites at high temperature
12. Comparison of tensile behavior of plain-woven carbon/silicon carbide composites at room temperature and high temperature
13. Tensile behavior of 2D-C/SiC composites at elevated temperatures: Experiment and modeling10.1016/j.jeurceramsoc.2016.11.011 ↗
14. Fracture behavior of C/SiC composites at elevated temperature10.1007/s12206-017-0702-3 ↗
15. Experimental investigation on the fatigue characteristics about high temperature of plain-woven C/SiC composite
16. The dynamic tensile properties of 2D-C/SiC composites at elevated temperatures10.1016/j.ijimpeng.2014.10.006 ↗
17. Compressive behavior of C/SiC composites over a wide range of strain rates and temperatures10.1016/j.carbon.2013.06.044 ↗
18. High-temperature flexural properties of SiBC modified C/SiC composites10.1016/j.ceramint.2013.11.072 ↗
19. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
20. Thermomechanical properties of carbon fibers at high temperatures (up to 2000 °C)10.1016/S0266-3538(01)00140-3 ↗
21. The tensile behavior of carbon fibers at high temperatures up to 2400 °C10.1016/j.carbon.2003.11.020 ↗
22. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗