journal article·2014-06

Surface Energy Engineering in the Solvothermal Deoxidation of Graphene Oxide

Liangxu Lin, Xuelin Zheng, Shaowei Zhang, Dan A. Allwood

Advanced Materials Interfaces· Volume 1· Issue 3
Publisher page

Abstract

A route to achieving high yields of monodisperse, deeply deoxidized graphene oxide (GO) in solution is presented. It overcomes many of the problems of dispersibility and inefficient reduction of GO in solvothermal deoxidation that are usually observed, despite the previous use of strong reducing agents (e.g. Fe2+, S or hydrazine). It is shown that the incomplete deoxidation is most likely due to agglomeration/self‐assembly of partially reduced GO, which also creates poor dispersibility. GO deoxidation is found to be highly sensitive to the solvent surface energy and, through experiments and empirical calculations, tuning the solvent surface energy to around 85.6 mJ/m2 (at 100 °C) leads to fully deoxidized GO. These calculations also allow appropriate solvent surface energies to be calculated for other temperatures for deep deoxidation of GO. This approach makes solvothermal deoxidation of GO a potential route to large scale, economic production of highly disperse monolayered graphene.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Graphene research and applications · Graphene and Nanomaterials Applications · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering University of Sheffield Sheffield S1 3JD UK

College of Chemistry and Chemical Engineering Fujian Normal University Fuzhou 350007 China

College of Engineering, Mathematics and Physical Sciences University of Exeter Exeter EX4 4QF UK

Funding

University of Sheffield and The National Natural Science Foundation of China

References (41)

Show source-provided references
1. 10.1038/nmat184910.1038/nmat1849 ↗
2. 10.1021/nl802484w10.1021/nl802484w ↗
3. 10.1038/nmat196710.1038/nmat1967 ↗
4. 10.1002/admi.20130004310.1002/admi.201300043 ↗
5. 10.1038/nnano.2010.13210.1038/nnano.2010.132 ↗
6. 10.1021/jp900360k10.1021/jp900360k ↗
7. 10.1038/nnano.2009.6710.1038/nnano.2009.67 ↗
8. 10.1126/science.112592510.1126/science.1125925 ↗
9. 10.1038/nnano.2008.21510.1038/nnano.2008.215 ↗
10. 10.1021/ja203725d10.1021/ja203725d ↗
11. 10.1016/j.carbon.2007.02.03410.1016/j.carbon.2007.02.034 ↗
12. 10.1002/adfm.20090016710.1002/adfm.200900167 ↗
13. 10.1002/adma.20080130610.1002/adma.200801306 ↗
14. 10.1038/nnano.2007.45110.1038/nnano.2007.451 ↗
15. 10.1039/c2jm31940c10.1039/c2jm31940c ↗
16. 10.1021/nn101187z10.1021/nn101187z ↗
17. Liu S. · Int. J. Electrochem. Sci. · 2010 · 7 · 35410.1016/S1452-3981(23)13344-X ↗
18. Given byIAPWS(The International Association for the Properties of Water and Steam) anddataphysics.
19. 10.1039/C0JM02790A10.1039/C0JM02790A ↗
20. 10.1016/S0927-7757(99)00100-410.1016/S0927-7757(99)00100-4 ↗
21. 10.1016/S0009-2614(97)01466-810.1016/S0009-2614(97)01466-8 ↗
22. 10.1016/0008-6223(73)90075-410.1016/0008-6223(73)90075-4 ↗
23. 10.1016/S0009-2614(01)01339-210.1016/S0009-2614(01)01339-2 ↗
24. 10.1103/PhysRevB.69.15540610.1103/PhysRevB.69.155406 ↗
25. 10.1021/la901402f10.1021/la901402f ↗
26. 10.1016/j.carbon.2005.07.03610.1016/j.carbon.2005.07.036 ↗
27. 10.1016/0008-6223(91)90025-E10.1016/0008-6223(91)90025-E ↗
28. 10.1063/1.55574610.1063/1.555746 ↗
29. Gerhartz W. · 1993 · 458
30. 1994 · 968
31. 10.1063/1.55568810.1063/1.555688 ↗
32. Adam N. K. · 1941
33. Atkins P. W. · 1982
34. 10.1021/je020132310.1021/je0201323 ↗
35. 10.1016/j.jct.2005.10.00810.1016/j.jct.2005.10.008 ↗
36. 10.1002/pssb.20100033910.1002/pssb.201000339 ↗
37. 10.1021/ac00178a00110.1021/ac00178a001 ↗
38. 10.1007/BF0064720410.1007/BF00647204 ↗
39. 10.1002/aic.69044102110.1002/aic.690441021 ↗
40. Tahery R. · Iran J. Sci. Technol. B · 2005 · 29 · 501
41. 10.1021/ja01539a01710.1021/ja01539a017 ↗