journal article·2018-06

Experimental and simulation studies on fatigue behavior of laminated glass having polyvinyl butyral and ethyl vinyl acetate interlayers

A. Vedrtnam, S.J. Pawar

Publisher page

Abstract

Abstract Cyclic fatigue strength (CFS) of laminated glasses (LGs) with different interlayers and their different nominal thicknesses were compared. The effect of interlayer thickness, cyclic bending fatigue load, and interlayer type on CFS is clearly observed from this brief study. It was found that the LG‐PVB has comparatively lower CFS than LG‐EVA. There is an increment in CFS with an increment in critical interlayer thickness (significantly for an increment from 0.38 to 0.76 mm) in both LG‐EVA (prominent) and LG‐PVB. The maximum deformation at failure load at the corresponding number of cycles is obtained using the finite element model. The strain‐life relations for LG samples were established and shown by surface plots. The results of finite element analysis previously established fracture models were used to explain the fracture patterns of the LG samples. The conclusions of the study are useful for the selection of LG in fatigue prone LG structures.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Structural Analysis of Composite Materials · Civil and Structural Engineering Research · Silicone and Siloxane Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Applied Mechanics Motilal Nehru National Institute of Technology Allahabad Allahabad UP 211004 India

Department of Mechanical Engineering Invertis University Bareilly UP 243001 India

Funding

Technical Education Quality Improvement Programme

References (38)

Show source-provided references
1. 10.1016/j.engfracmech.2017.10.02010.1016/j.engfracmech.2017.10.020 ↗
2. 10.13036/17533546.58.6.00510.13036/17533546.58.6.005 ↗
3. VedrtnamA PawarSJ.Experimental and simulation studies on flexural strength of laminated glass using ring‐on‐ring and three‐point bending test Accepted In press Proc IMechE Part C: J Mechanical Engineering Science published online: November 24 2017.10.1177/0954406217744815 ↗
4. 10.1016/j.matdes.2014.05.03010.1016/j.matdes.2014.05.030 ↗
5. Ferry J · 1980
6. 10.1021/ja01619a00810.1021/ja01619a008 ↗
7. 10.1061/(ASCE)0733-9399(1999)125:4(435)10.1061/(ASCE)0733-9399(1999)125:4(435) ↗
8. 10.1016/0020-7403(73)90012-X10.1016/0020-7403(73)90012-X ↗
9. 10.1061/(ASCE)0733-9445(1993)119:1(202)10.1061/(ASCE)0733-9445(1993)119:1(202) ↗
10. EdelM.The effect of temperature on the bending of laminated glass units. PhD thesis Texas A&M University Department of Civil Engineering College Station Texas;1997.
11. 10.1061/(ASCE)0733-9399(1998)124:1(46)10.1061/(ASCE)0733-9399(1998)124:1(46) ↗
12. 10.1016/j.compstruc.2005.02.02010.1016/j.compstruc.2005.02.020 ↗
13. Long‐term laminated glass four point bending test with PVB, EVA and SG inter‐layers at different temperatures
14. 10.1016/j.conbuildmat.2011.07.04610.1016/j.conbuildmat.2011.07.046 ↗
15. 10.1016/j.engstruct.2013.02.00210.1016/j.engstruct.2013.02.002 ↗
16. 10.1016/j.engfailanal.2008.09.02310.1016/j.engfailanal.2008.09.023 ↗
17. 10.1016/S1359-6454(02)00255-010.1016/S1359-6454(02)00255-0 ↗
18. 10.1016/j.conbuildmat.2009.09.00710.1016/j.conbuildmat.2009.09.007 ↗
19. 10.1016/j.ijsolstr.2006.02.01410.1016/j.ijsolstr.2006.02.014 ↗
20. 10.1016/j.compositesb.2013.05.02510.1016/j.compositesb.2013.05.025 ↗
21. NhamoinesuS OverendM.Simple model for predicting the post‐fracture behavior of laminated glass XXV A.T.I.V 2010 International Conference Parma Italy 2010.
22. CalderoneI DaviesPS BennisonSJ XiaokunH GangL.Effective laminate thickness for the design of laminated glass. Glass Processing Days2009 Tampere Finland
23. SerafinavičiusT LebetJP LouterC LenkimasT KuranovasA.Long‐term laminated glass four point bending test with PVB EVA and SG inter‐layers at different temperatures. 11th International Conference on Modern Building Materials Structures and Techniques MBMST2013 Procedia Engineering 57 996–1004.10.1016/j.proeng.2013.04.126 ↗
24. 10.1016/j.compositesb.2014.04.01810.1016/j.compositesb.2014.04.018 ↗
25. 10.1016/j.proeng.2011.04.03310.1016/j.proeng.2011.04.033 ↗
26. 10.1016/j.engstruct.2015.08.02110.1016/j.engstruct.2015.08.021 ↗
27. 10.1617/s11527-015-0661-z10.1617/s11527-015-0661-z ↗
28. 10.1016/j.engstruct.2013.12.01210.1016/j.engstruct.2013.12.012 ↗
29. 10.1016/j.engstruct.2014.05.00310.1016/j.engstruct.2014.05.003 ↗
30. 10.1680/stbu.13.0011310.1680/stbu.13.00113 ↗
31. 10.1016/j.compstruct.2006.04.04110.1016/j.compstruct.2006.04.041 ↗
32. 10.1016/j.compstruct.2016.02.02410.1016/j.compstruct.2016.02.024 ↗
33. 10.1016/j.compositesa.2011.11.00810.1016/j.compositesa.2011.11.008 ↗
34. 10.1177/002199830505108410.1177/0021998305051084 ↗
35. Hilcken J · 2014
36. Factors affecting the strength of the glass (review)
37. 10.1063/1.312078410.1063/1.3120784 ↗
38. 10.1007/s11661-999-0173-y10.1007/s11661-999-0173-y ↗