Investigation of Crystallographic Influences on Small Fatigue Crack Growth in Powder Metallurgy Superalloy FGH96
Source abstract
Abstract
ABSTRACT In situ small fatigue crack growth experiments at 500°C, combined with pretest and posttest electron backscatter diffraction analysis, were conducted to investigate the growth behavior of FGH96. High‐temperature fatigue loading reduced the average texture intensity and induced a pronounced {111} plane normal alignment along the loading direction, forming a localized strong texture. Significant local lattice rotations and geometrically necessary dislocation accumulation occurred in the crack region, both decreasing with distance. Crack growth was predominantly transgranular and strongly influenced by crystallographic orientation. Intragranular crack path deflection occurred with similar frequencies toward slip systems of higher and lower Schmid factors. The experimental results demonstrated that under certain conditions, high‐angle grain boundaries substantially impeded transgranular crack propagation. Three types of crack growth resumption behaviors induced by grain boundaries were identified. Overall, crystallographic orientation and grain boundaries jointly govern the small crack growth. These findings enable high‐precision life prediction of small fatigue cracks.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · High Temperature Alloys and Creep · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Aircraft/Engine Integrated System Safety Beijing Key Laboratory, School of Energy and Power Engineering Beihang University Beijing China
Tianmushan Laboratory Hangzhou China
Civil Aviation University of China Tianjin China
Research Institute of Aero‐Engine Beihang University Beijing China
Funding
National Natural Science Foundation of China
References (56)
Show source-provided references
1. Reed R. C. · 2008
2. 10.2514/1.1823910.2514/1.18239 ↗
3. 10.1016/j.actamat.2015.05.05010.1016/j.actamat.2015.05.050 ↗
4. Fatigue Crack Initiation and Propagation Relation of Notched Specimens With Welded Joint Characteristics
5. 10.1016/j.commatsci.2020.10996210.1016/j.commatsci.2020.109962 ↗
6. 10.1115/1.163102610.1115/1.1631026 ↗
7. 10.1016/j.ijfatigue.2023.10773110.1016/j.ijfatigue.2023.107731 ↗
8. 10.1115/1.365690010.1115/1.3656900 ↗
9. 10.1016/0025-5416(88)90547-210.1016/0025-5416(88)90547-2 ↗
10. 10.1520/STP32032S10.1520/STP32032S ↗
11. 10.1016/j.msea.2008.04.05010.1016/j.msea.2008.04.050 ↗
12. 10.1179/imtr.1984.29.1.44510.1179/imtr.1984.29.1.445 ↗
13. 10.1016/0013-7944(91)90151-P10.1016/0013-7944(91)90151-P ↗
14. 10.1111/ffe.1372510.1111/ffe.13725 ↗
15. 10.1016/j.ijfatigue.2020.10588710.1016/j.ijfatigue.2020.105887 ↗
16. 10.1016/j.msea.2019.03.10210.1016/j.msea.2019.03.102 ↗
17. 10.1017/CBO978051180657510.1017/CBO9780511806575 ↗
18. 10.1016/S0167-577X(03)00423-310.1016/S0167-577X(03)00423-3 ↗
19. 10.1016/1359-6454(95)00147-910.1016/1359-6454(95)00147-9 ↗
20. 10.1016/j.proeng.2010.03.24510.1016/j.proeng.2010.03.245 ↗
21. 10.1016/S1359-6454(00)00214-710.1016/S1359-6454(00)00214-7 ↗
22. 10.1016/j.msea.2018.11.04010.1016/j.msea.2018.11.040 ↗
23. 10.1016/j.ijfatigue.2020.10559410.1016/j.ijfatigue.2020.105594 ↗
24. 10.1016/j.ijfatigue.2022.10686110.1016/j.ijfatigue.2022.106861 ↗
25. 10.1111/ffe.1463510.1111/ffe.14635 ↗
26. 10.1016/j.ijfatigue.2014.04.00310.1016/j.ijfatigue.2014.04.003 ↗
27. 10.1016/j.actamat.2019.07.02510.1016/j.actamat.2019.07.025 ↗
28. 10.1016/j.ijfatigue.2022.10689410.1016/j.ijfatigue.2022.106894 ↗
29. 10.1016/j.ijfatigue.2019.10536510.1016/j.ijfatigue.2019.105365 ↗
30. 10.1016/j.ijfatigue.2020.10595310.1016/j.ijfatigue.2020.105953 ↗
31. Standardization Administration of the People's Republic of China (SAC) · 2021
32. Standardization Administration of the People's Republic of China (SAC) · 2015
33. 10.1016/j.ijfatigue.2022.10737210.1016/j.ijfatigue.2022.107372 ↗
34. 10.1016/j.engfracmech.2022.10878610.1016/j.engfracmech.2022.108786 ↗
35. 10.1111/ffe.1462010.1111/ffe.14620 ↗
36. Comparison of Surface Pretreatments Effects on Fatigue Damage Behavior Identification of Metals Under In‐Situ SEM Tests
37. 10.3390/ma1706135610.3390/ma17061356 ↗
38. 10.1016/j.ijfatigue.2010.02.00110.1016/j.ijfatigue.2010.02.001 ↗
39. 10.1016/j.msea.2015.05.06510.1016/j.msea.2015.05.065 ↗
40. 10.1016/j.jmps.2012.02.00110.1016/j.jmps.2012.02.001 ↗
41. 10.1016/j.ijfatigue.2010.11.02410.1016/j.ijfatigue.2010.11.024 ↗
42. 10.1016/j.ijfatigue.2020.10573910.1016/j.ijfatigue.2020.105739 ↗
43. 10.1007/s10704-010-9512-710.1007/s10704-010-9512-7 ↗
44. 10.1016/j.engfracmech.2024.10985010.1016/j.engfracmech.2024.109850 ↗
45. 10.1016/j.matdes.2024.11311710.1016/j.matdes.2024.113117 ↗
46. 10.3390/ma1617588310.3390/ma16175883 ↗
47. In Situ Synchrotron HEXRD Study on the Deformation Mechanism of a Nickel‐Based Superalloy During Medium‐Temperature Compression
48. 10.1016/j.ijfatigue.2023.10757310.1016/j.ijfatigue.2023.107573 ↗
49. 10.1016/j.ijfatigue.2023.10775510.1016/j.ijfatigue.2023.107755 ↗
50. 10.1016/j.ijfatigue.2022.10715810.1016/j.ijfatigue.2022.107158 ↗
51. 10.1016/j.msea.2013.05.05310.1016/j.msea.2013.05.053 ↗
52. 10.1126/sciadv.ado211810.1126/sciadv.ado2118 ↗
53. 10.1016/j.cma.2019.01.01410.1016/j.cma.2019.01.014 ↗
54. 10.1038/s41598-020-59405-510.1038/s41598-020-59405-5 ↗
55. 10.1007/s10704-020-00467-x10.1007/s10704-020-00467-x ↗
56. 10.1016/j.matlet.2004.05.06310.1016/j.matlet.2004.05.063 ↗