Mode I fracture toughness of the thermally pretreated red Verona marble by means of the two‐parameter model
Source abstract
Abstract
Abstract The paper aims to analyse the effects of pretreatment thermal cycles on both mechanical and fracture parameters of the red Verona marble, which is a natural stone of sedimentary formation. The effects of the thermal pretreatment, consisting of freeze/thaw cycles and simulating the atmospheric ageing on the material, are evaluated in terms of changes of the aforementioned parameters. Note that a wide variety of both specimen types and methods to determine mode I plain strain fracture toughness of rocks are available in the literature. The two‐parameter model originally proposed for plain concrete is herein adopted. Such a method, based on the experimental data obtained from three‐point bending tests on single edge‐notched specimens, is able to take into account the slow nonlinear crack growth occurring before the peak load, typical of quasibrittle materials, and presents the advantages of easy specimens preparation and simple test configuration.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Rock Mechanics and Modeling · Geophysical Methods and Applications · Numerical methods in engineering
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Civil and Environmental Engineering and Architecture University of Parma Parco Area delle Scienze 181/A 43124 Parma Italy
References (47)
Show source-provided references
1. 10.1111/ffe.1204310.1111/ffe.12043 ↗
2. ASTM E 399‐90 · 2001
3. Whittaker B. N. · 1992
4. 10.1016/0148-9062(88)91871-210.1016/0148-9062(88)91871-2 ↗
5. Three point bending test investigation of the fracture behaviour of siltstone after thermal treatment10.1016/j.ijrmms.2014.04.005 ↗
6. 10.1201/978148226558310.1201/9781482265583 ↗
7. 10.1111/ffe.1212210.1111/ffe.12122 ↗
8. UNI 11186(2008)Beni culturali ‐ materiali lapidei naturali ed artificiali ‐ metodologia per l'esposizione a cicli di gelo e disgelo.
9. 10.1007/s11771-007-0311-x10.1007/s11771-007-0311-x ↗
10. SEM in situ investigations on thermal cracking behaviour of Pingdingshan sandstone at elevated temperature
11. 10.1016/S1365-1609(00)00051-410.1016/S1365-1609(00)00051-4 ↗
12. 10.1016/S1365-1609(00)00003-410.1016/S1365-1609(00)00003-4 ↗
13. 10.1007/s11431-007-0081-610.1007/s11431-007-0081-6 ↗
14. Experimental determination of the coupled thermal‐mechanical effects on fracture toughness of sandstone10.1520/JTE101542 ↗
15. 10.1016/j.ijrmms.2004.02.00810.1016/j.ijrmms.2004.02.008 ↗
16. ISRM · 2006
17. ISRM · 2015
18. 10.1007/BF0232114810.1007/BF02321148 ↗
19. Review of fracture toughness testing of rock
20. 10.1007/BF0115755510.1007/BF01157555 ↗
21. 10.1016/0013-7944(93)90030-V10.1016/0013-7944(93)90030-V ↗
22. Fracture toughness measurement using chevron notched semi‐circular bend specimen
23. 10.1016/0013-7944(77)90028-510.1016/0013-7944(77)90028-5 ↗
24. 10.1520/JTE10764J10.1520/JTE10764J ↗
25. 10.1007/BF0004706310.1007/BF00047063 ↗
26. 10.1115/1.344346810.1115/1.3443468 ↗
27. 10.1016/0013-7944(80)90025-910.1016/0013-7944(80)90025-9 ↗
28. Fracture toughness of ceramics measured by a chevron‐notched diametral‐compression test
29. Thiercelin M.andRoegiers J. C.(1986)Fracture toughness determination with the modified ring test. In: Proceedings of the International Symposium on Engineering in Complex Rock Formations Beijing 1–8.
30. 10.1016/S0013-7944(99)00065-X10.1016/S0013-7944(99)00065-X ↗
31. Method for determination of dynamic fracture toughness of rock using holed‐cracked flattened disk specimen
32. 10.1016/j.ijrmms.2006.10.00110.1016/j.ijrmms.2006.10.001 ↗
33. 10.1016/j.engfracmech.2010.03.00910.1016/j.engfracmech.2010.03.009 ↗
34. 10.1016/j.ijrmms.2012.01.01710.1016/j.ijrmms.2012.01.017 ↗
35. 10.5267/j.esm.2013.10.00110.5267/j.esm.2013.10.001 ↗
36. 10.1007/s00603-014-0665-y10.1007/s00603-014-0665-y ↗
37. 10.5267/j.esm.2015.7.00110.5267/j.esm.2015.7.001 ↗
38. Kuruppu M. D. · 2015 · 107
39. 10.1007/s10704-008-9280-910.1007/s10704-008-9280-9 ↗
40. 10.1111/j.1460-2695.2009.01402.x10.1111/j.1460-2695.2009.01402.x ↗
41. 10.1016/j.ijrmms.2011.09.01910.1016/j.ijrmms.2011.09.019 ↗
42. 10.1016/j.ijrmms.2012.02.00410.1016/j.ijrmms.2012.02.004 ↗
43. 10.1061/(ASCE)EM.1943-7889.000065110.1061/(ASCE)EM.1943-7889.0000651 ↗
44. 10.1016/j.engfracmech.2014.12.01010.1016/j.engfracmech.2014.12.010 ↗
45. 10.1061/(ASCE)0733-9399(1985)111:10(1227)10.1061/(ASCE)0733-9399(1985)111:10(1227) ↗
46. 10.1111/j.1460-2695.2010.01477.x10.1111/j.1460-2695.2010.01477.x ↗
47. UNI EN 12371(2010)Natural stone test methods: determination of frost resistance.