Creep crack initiation prediction considering constraint effect for pressurized pipelines with circumferential surface cracks
Source abstract
Abstract
Abstract Theoretical 2‐parameter C*‐Q* approaches and numerical simulation were conducted to investigate the creep crack initiation (CCI) time and the effect of constraints induced by the geometrical sizes of pipelines with circumferential surface cracks. The theoretical enhancement model of the C*‐Q* approaches under the transient creep condition, which considered the load‐independent constraint parameter Q*, was proposed to predict the CCI time around the crack front. The results revealed that the distribution regulation of Q* along the crack front for circumferential internal surface cracks and external surface cracks was similar. The maximum constraint level occurred near the deepest crack front part for cracks with small a/c (a/c < 0.4), while it occurred near the free surface for cracks with large a/c (a/c > 0.4). The constraint values at the same position (2Φ/π) increased with the increasing of the crack depth when a/c kept constant. In addition, the circumferential internal surface cracks of pipelines were proved more dangerous than the external surface cracks with the same geometrical size. Furthermore, the CCI times were decided by the peak values of constraint, or the CCI firstly occurred at the position where the constraint level was maximum. Additionally, the variation of hydrostatic stresses, triaxiality, and multiaxial strain factor considering the constraint parameter Q* was discussed. The suitability of the analytical C*‐Q* approaches was verified to predict CCI. The comparison of CCI times between the analytical approach and the BS 7910 as well as the finite element results demonstrated that the solutions under stress intensity factor–Riedel‐Rice control (initially by stress intensity factor and then by transient creep stress or Riedel‐Rice conditions)—were more accurate when internal pressure P < 18 MPa, but the solutions under Hutchinson‐Rice‐Rosengren–Riedel‐Rice control (initially by plastic Hutchinson‐Rice‐Rosengren control and then by Riedel‐Rice conditions) were more appropriate when P > 18 MPa. Finally, the accuracy of C*‐Q* 2‐parameter approaches and the suitability of finite element simulation were validated.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Material Properties and Failure Mechanisms · Fire effects on concrete materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Tianjin University Tianjin 300072 China
Tianjin Key Laboratory of Advanced Joining Technology Tianjin 300072 China
Funding
National Natural Science Foundation of China
References (62)
Show source-provided references
1. 10.1016/j.engfracmech.2008.08.00110.1016/j.engfracmech.2008.08.001 ↗
2. 10.1016/j.engfracmech.2010.04.02410.1016/j.engfracmech.2010.04.024 ↗
3. 10.1016/j.engfracmech.2010.04.02310.1016/j.engfracmech.2010.04.023 ↗
4. 10.1016/j.msea.2012.07.09410.1016/j.msea.2012.07.094 ↗
5. 10.1016/j.ijsolstr.2009.11.01810.1016/j.ijsolstr.2009.11.018 ↗
6. The influence of test duration and geometry on the creep crack initiation and growth behavior of 316H steel
7. 10.1016/j.engfracmech.2011.11.01410.1016/j.engfracmech.2011.11.014 ↗
8. 10.1111/j.1460-2695.2012.01722.x10.1111/j.1460-2695.2012.01722.x ↗
9. 10.1016/j.engfracmech.2006.10.00410.1016/j.engfracmech.2006.10.004 ↗
10. 10.1016/j.matdes.2013.07.05810.1016/j.matdes.2013.07.058 ↗
11. 10.1016/j.ijpvp.2014.05.00610.1016/j.ijpvp.2014.05.006 ↗
12. 10.1016/S0020-7683(00)00255-910.1016/S0020-7683(00)00255-9 ↗
13. 10.1080/09603409.1992.1168941010.1080/09603409.1992.11689410 ↗
14. 10.1016/j.ijsolstr.2006.08.03610.1016/j.ijsolstr.2006.08.036 ↗
15. British Standards Institution. BS 7910.Guide to methods for assessing the acceptability of flaws in metallic structures [D].British 2005.
16. 10.1016/S0013-7944(99)00127-710.1016/S0013-7944(99)00127-7 ↗
17. 10.1016/j.engfracmech.2012.08.00910.1016/j.engfracmech.2012.08.009 ↗
18. 10.1016/j.ijmecsci.2015.02.00910.1016/j.ijmecsci.2015.02.009 ↗
19. 10.1016/j.engfracmech.2013.01.01710.1016/j.engfracmech.2013.01.017 ↗
20. 10.1023/A:101830591962210.1023/A:1018305919622 ↗
21. 10.1115/1.130482310.1115/1.1304823 ↗
22. 10.1016/j.ijpvp.2012.06.00710.1016/j.ijpvp.2012.06.007 ↗
23. 10.1016/j.engfracmech.2015.06.03210.1016/j.engfracmech.2015.06.032 ↗
24. 10.1016/j.ijsolstr.2009.09.01510.1016/j.ijsolstr.2009.09.015 ↗
25. 10.1016/j.engfracmech.2010.11.01710.1016/j.engfracmech.2010.11.017 ↗
26. 10.1016/j.engfracmech.2013.12.01510.1016/j.engfracmech.2013.12.015 ↗
27. 10.1016/j.engfracmech.2015.10.00910.1016/j.engfracmech.2015.10.009 ↗
28. 10.1016/j.engfracmech.2015.05.04410.1016/j.engfracmech.2015.05.044 ↗
29. 10.1016/j.engfracmech.2016.01.01710.1016/j.engfracmech.2016.01.017 ↗
30. 10.1023/A:101242471167210.1023/A:1012424711672 ↗
31. 10.1016/j.ijmecsci.2016.11.00210.1016/j.ijmecsci.2016.11.002 ↗
32. 10.1557/jmr.2011.1110.1557/jmr.2011.11 ↗
33. 10.1016/j.engfracmech.2015.01.01810.1016/j.engfracmech.2015.01.018 ↗
34. 10.1016/j.engfracmech.2016.01.00910.1016/j.engfracmech.2016.01.009 ↗
35. 10.1016/j.engfracmech.2017.11.03210.1016/j.engfracmech.2017.11.032 ↗
36. 10.1016/j.engfracmech.2015.09.01210.1016/j.engfracmech.2015.09.012 ↗
37. Characterization of creep crack‐tip constraint levels for pressurized pipelines with axial surface cracks
38. 10.1016/j.advengsoft.2017.08.01310.1016/j.advengsoft.2017.08.013 ↗
39. 10.1016/j.engfracmech.2017.02.02110.1016/j.engfracmech.2017.02.021 ↗
40. 10.1016/j.ijsolstr.2016.07.03910.1016/j.ijsolstr.2016.07.039 ↗
41. 10.1016/S0308-0161(01)00085-010.1016/S0308-0161(01)00085-0 ↗
42. Kaguchi H · 1994
43. 10.1016/j.tafmec.2017.10.00410.1016/j.tafmec.2017.10.004 ↗
44. 10.1016/j.engfracmech.2012.10.02010.1016/j.engfracmech.2012.10.020 ↗
45. 10.1016/j.tafmec.2018.02.01410.1016/j.tafmec.2018.02.014 ↗
46. 10.1016/j.tafmec.2018.03.01010.1016/j.tafmec.2018.03.010 ↗
47. 10.1016/j.euromechsol.2018.03.01110.1016/j.euromechsol.2018.03.011 ↗
48. 10.1016/j.matdes.2011.05.00910.1016/j.matdes.2011.05.009 ↗
49. 10.1016/j.msea.2003.09.01410.1016/j.msea.2003.09.014 ↗
50. O'DowdNP KamranMN BiglariFR.Creep crack initiation in a weld steel: effects of residual stress. In: Proc. 2005 ASME pressure vessels and piping division conf 2005 Denver Colorado USA.10.1115/PVP2005-71566 ↗
51. 10.1016/j.actamat.2008.03.04510.1016/j.actamat.2008.03.045 ↗
52. 10.1179/03063458079044118710.1179/030634580790441187 ↗
53. 10.1007/s10338-008-0836-z10.1007/s10338-008-0836-z ↗
54. 10.1007/BF0264656610.1007/BF02646566 ↗
55. 10.1002/maco.1994045111110.1002/maco.19940451111 ↗
56. 10.1016/S0013-7944(97)00030-110.1016/S0013-7944(97)00030-1 ↗
57. Ilyushin AA · 1973
58. 10.1111/j.1460-2695.1990.tb00598.x10.1111/j.1460-2695.1990.tb00598.x ↗
59. 10.1016/j.nucengdes.2003.09.00510.1016/j.nucengdes.2003.09.005 ↗
60. KumarV GermanMD ShihCF.An engineering approach for elastic‐plastic fracture analysis. EPRI EPRI Report1981; NP‐1931.
61. 10.1115/1.401145410.1115/1.4011454 ↗
62. 10.1016/0022-5096(68)90021-510.1016/0022-5096(68)90021-5 ↗