journal article·2025-02Open access

Constructing Quasi‐Localized High‐Concentration Solvation Structures to Stabilize Battery Interfaces in Nonflammable Phosphate‐Based Electrolyte

Chenyang Shi, Mengran Wang, Zari Tehrani, Bo Hong, Mengnan Wang, Rui Tan, Serena Margadonna, Yanqing Lai, Maria Magdalena Titirici

Advanced Science· Volume 12· Issue 6

Abstract

Abstract Flame‐retardant phosphate‐based electrolytes effectively enhance lithium‐ion battery safety but suffer from poor compatibility with graphite anodes and high‐voltage cathodes, hindering scalability. Fluorinated phosphates, though widely used, increase interfacial resistance at the anode, degrading performance. In this work, carbonate solvents with strong polarity are introduced to prevent tris(2,2,2‐trifluoroethyl) phosphate (TFEP) from participating in the solvation structure of lithium ions. This strategy forms a quasi‐localized high‐concentration solvation structure, thereby restricting the reduction of TFEP and its impact on the graphite anode. The LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NCM811) | Graphite (Gr) pouch cell with optimized electrolyte exhibits a capacity retention rate of 80.1% after 370 cycles at 0.5C, which is much more stable than the electrolyte with TFEP‐involved solvation structure (capacity retention rate: 47.1% after 300 cycles). The corresponding pouch cell with cut‐off voltage to 4.5 V exhibits a capacity retention rate of 82.8% after 125 cycles, significantly outperforming cells employing commercial carbonate electrolytes (capacity retention rate: 56.9% after 125 cycles). Thus, the developed quasi‐localized high‐concentration solvation structure can effectively stabilize the electrode interface, greatly enhancing the cycling performance of phosphate‐based flame‐retardant electrolytes.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Supercapacitor Materials and Fabrication

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Metallurgy and Environment Central South University Changsha Hunan 410083 China

Engineering Research Centre of Advanced Battery Materials The Ministry of Education Changsha Hunan 410083 China

National Energy Metal Resources and New Materials Key Laboratory Changsha Hunan 410083 China

National Engineering Research Center of Advanced Energy Storage Materials Changsha Hunan 410083 China

Department of Chemical Engineering Swansea University Swansea SA1 8EN UK

Department of Chemical Engineering Imperial College London London SW7 2AZ UK

Hunan Province Key Laboratory of Nonferrous Value‐Added Metallurgy Central South University Changsha Hunan 410083 China

Funding

National Natural Science Foundation of China · Fundamental Research Funds for Central Universities of the Central South University

References (39)

Show source-provided references
1. 10.1016/j.esci.2021.12.00310.1016/j.esci.2021.12.003 ↗
2. Wang Y. · Adv. Funct. Mater. · 2024 · 34
3. 10.1038/s44286-024-00103-810.1038/s44286-024-00103-8 ↗
4. 10.1016/j.ensm.2020.07.01810.1016/j.ensm.2020.07.018 ↗
5. 10.1002/aenm.20220277910.1002/aenm.202202779 ↗
6. 10.1002/smsc.20210005810.1002/smsc.202100058 ↗
7. 10.1002/cey2.60410.1002/cey2.604 ↗
8. 10.1038/s41893-024-01275-010.1038/s41893-024-01275-0 ↗
9. 10.1016/j.electacta.2012.09.06510.1016/j.electacta.2012.09.065 ↗
10. 10.3390/batteries501001910.3390/batteries5010019 ↗
11. 10.1002/aenm.20230025910.1002/aenm.202300259 ↗
12. 10.1016/j.jechem.2023.08.05310.1016/j.jechem.2023.08.053 ↗
13. 10.1016/j.ensm.2023.10309810.1016/j.ensm.2023.103098 ↗
14. 10.1038/s41586-022-05627-810.1038/s41586-022-05627-8 ↗
15. 10.1002/inf2.1208910.1002/inf2.12089 ↗
16. 10.1021/acsnano.3c1282310.1021/acsnano.3c12823 ↗
17. 10.1016/j.isci.2018.11.02010.1016/j.isci.2018.11.020 ↗
18. 10.1002/adma.20210840010.1002/adma.202108400 ↗
19. Chen S. · Angew. Chem., Int. Ed. · 2024
20. 10.31635/ccschem.024.20240412010.31635/ccschem.024.202404120 ↗
21. 10.1002/anie.20240771710.1002/anie.202407717 ↗
22. 10.1002/adfm.20240786710.1002/adfm.202407867 ↗
23. 10.1016/j.ensm.2022.12.04410.1016/j.ensm.2022.12.044 ↗
24. 10.1021/acsaem.1c0050310.1021/acsaem.1c00503 ↗
25. 10.1016/j.nanoen.2019.10388110.1016/j.nanoen.2019.103881 ↗
26. 10.1039/C7CP08511G10.1039/C7CP08511G ↗
27. 10.1021/acs.jpcc.7b0691010.1021/acs.jpcc.7b06910 ↗
28. Wang Z. · Angew. Chem., Int. Ed. · 2022 · 61
29. 10.1016/j.nanoen.2022.10726510.1016/j.nanoen.2022.107265 ↗
30. 10.1016/j.ensm.2020.05.02010.1016/j.ensm.2020.05.020 ↗
31. 10.1002/anie.20220668210.1002/anie.202206682 ↗
32. 10.1039/D3CP01236K10.1039/D3CP01236K ↗
33. 10.1021/acs.jpcc.5b0369410.1021/acs.jpcc.5b03694 ↗
34. 10.1002/adfm.20230366710.1002/adfm.202303667 ↗
35. 10.1002/anie.20200973810.1002/anie.202009738 ↗
36. 10.1016/j.electacta.2010.05.07210.1016/j.electacta.2010.05.072 ↗
37. 10.1016/j.ensm.2022.12.04410.1016/j.ensm.2022.12.044 ↗
38. 10.1021/acsenergylett.3c0050410.1021/acsenergylett.3c00504 ↗
39. 10.1038/s41565-018-0284-y10.1038/s41565-018-0284-y ↗