Abstract This paper presents the results of an extensive experimental study on the compressive and splitting tensile strength of high-strength concrete with and without polypropylene (PP) fibers after heating to 600 °C. Mixtures were prepared with water to cementitious materials ratios of 0.40, 0.35, and 0.30 containing silica fume at 0%, 6%, and 10% cement replacement and polypropylene fibers content of 0, 1, 2, and 3 kg/m3. A severe strength loss was observed for all of the concretes after exposure to 600 °C, particularly the concretes containing silica fume despite their good mechanical properties at room temperature. The range of 300–600 °C was more critical for concrete having higher strength. The relative compressive strengths of concretes containing PP fibers were higher than those of concretes without PP fibers. The splitting tensile strength of concrete was more sensitive to high temperatures than the compressive strength. Furthermore, the presence of PP fibers was more effective for compressive strength than splitting tensile strength above 200 °C. Based on the test results, it can be concluded that the addition of 2 kg/m3 PP fibers can significantly promote the residual mechanical properties of HSC during heating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fire effects on concrete materials · Innovative concrete reinforcement materials · Structural Behavior of Reinforced Concrete
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Effect of temperature on some of the properties of material
2. Effect of temperature on compressive strength of concrete10.1680/macr.1956.8.23.85 ↗
3. Abrams · 1971
4. Comparison of the strength and durability performance of normal and high-strength pozzolanic concretes at elevated temperatures10.1016/S0008-8846(01)00580-4 ↗
5. Elevated temperature effects on HSC residual strength
6. Fire behavior of high-performance concrete made with silica fume at various moisture contents
7. Stress-strain cures for high-strength concrete at elevated temperatures10.1061/(ASCE)0899-1561(2004)16:1(84) ↗
8. A. Behnood, Effects of high temperatures on the high-strength concretes incorporating copper slag as coarse aggregate, in: Seventh International Symposium on Utilization of High-Strength/Performance Concrete, SP-228-66, American Concrete Institute, Washington, 2005, pp. 1063–1075.
9. Effects of test conditions and mixture proportions on behaviour of high-strength concrete exposed to high temperatures
10. Effect of transient high temperature on high-strength concrete
11. U. Diederiches, U.M. Jumppanen, U. Schneider, High temperature properties and spalling behavior of high strength concrete. In: Proceedings of the Fourth Weimar Workshop on High Strength Concrete: Materials Properties and Design, Germany, 1995, pp. 237–254.
12. Material and environmental factors influencing the compressive strength of unsealed cement paste and concrete at high temperatures10.1680/macr.1993.45.162.51 ↗
13. Effects of high temperature on the residual compressive strength of high-strength siliceous concretes
14. R.B. Williams, A.I. Rashed, Comparison of ASTM E 119 fire endurance exposure of two EMSAC concretes with similar conventional concretes, Report No. UCB FRG 87-1, Fire Research Laboratory, University of California, Berkeley, 1987, pp. 22–87.
15. S.T. Shirley, R.G. Burg, A.E. Fiorato, Fire endurance of high-strength concrete slabs, Report, Construction Technology Laboratories, Skokie, 1987, p. 27.
16. Fibers, percolation, and spalling of high-performance concrete
17. Effect of temperature on the hydration of the main clinker phases in portland cements: Part 1, Neat Cements10.1016/S0008-8846(98)00107-0 ↗
18. Design of reinforced concrete beams under fire exposure conditions10.1680/macr.1998.50.1.75 ↗
19. Concrete strength estimation at early ages: modification of the method of equivalent age
20. Influence of elevated temperatures on the mechanical properties of blended cement concretes prepared with limestone and siliceous aggregates10.1016/j.cemconcomp.2004.02.013 ↗
21. Temperature distribution and mechanical properties of high-strength silica fume concrete at elevated temperature up to 200°C
22. Effects of minor components and heating rates on the fine textures of alite in portland cement clinker10.1016/S0008-8846(97)00103-8 ↗
23. T.A. Hammer, High-strength concrete Phase 3, compressive strength and e-modulus at elevated temperatures, Report 6.1, SINTEF Structures and Concretes, STF 70 A 95023, 1995.
24. Effect of silica fume addition and water to cement ratio on the properties of high-strength concrete after exposure to high temperatures10.1016/j.cemconcomp.2007.06.003 ↗
25. Mechanical properties of high-strength concrete after fire10.1016/j.cemconres.2003.11.007 ↗
26. Residual strength of hybrid-fiber-reinforced high-strength concrete after exposure to high temperatures10.1016/j.cemconres.2003.11.010 ↗
27. The chunnel fire: chemoplastic softening in rapidly heated concrete10.1061/(ASCE)0733-9399(1999)125:3(272) ↗
28. Ahmed · 1997
29. Bazant · 1996
30. How do polypropylene fibers improve the spalling behavior of in-situ concrete?10.1016/j.cemconres.2005.12.018 ↗
31. G.R. Consolazio, M.C. McVay, J.W. Rish, Measurement and prediction of pore pressure in cement mortar subjected to elevated temperature. In: Proceedings of International Workshop of Fire Performance of High-Strength Concrete, NIST, Gaithersburg, Maryland, 1997, pp. 125–148.
32. Spalling of concrete for tunnel linings10.1002/best.200200860 ↗
33. Measurement and prediction of pore pressure in saturated cement mortar subjected to radiant heating
34. High-temperature behavior of HPC with polypropylene fibers from spalling to microstructure10.1016/S0008-8846(01)00596-8 ↗
35. Thermal degradation of polypropylene fibers in cement composites
36. Soroushian · 1993
37. Shrinkage cracking of fiber reinforced concrete
38. Hannant · 1987
39. Compressive behavior of fiber reinforced high-performance concrete subjected to elevated temperatures10.1016/j.cemconres.2004.02.011 ↗
40. Compressive strength and pore structure of high-performance concrete after exposure to high temperature up to 800°C10.1016/S0008-8846(99)00240-9 ↗
41. Modeling of hygro-thermal behavior of concrete at high temperature with thermo-chemical and mechanical material degradation10.1016/S0045-7825(03)00200-7 ↗
42. Towards prediction of the thermal spalling risk through a multi-phase porous media model of concrete10.1016/j.cma.2005.10.021 ↗
43. A numerical model for predicting the fire resistance of reinforced concrete beams10.1016/j.cemconcomp.2007.08.012 ↗
44. Lankard · 1971
45. Residual fracture toughness of normal-and high-strength gravel concrete after heating to 600°C
46. Microstructures of fire-damaged concrete
47. Chen · 1982
48. Properties of high-strength concrete subjecting to short-term loads
49. ACI 363R-84, State-of-the-Art Report on High-Strength Concrete, ACI Manuals of Concrete Practice, Part 1, American Concrete Institute, Detroit, 1993, pp. 364–411.
50. Fracture toughness of micro-fiber reinforced cement composites10.1016/0958-9465(95)00030-5 ↗
51. Bonding in polypropylene fiber reinforced concretes10.1016/0262-5075(89)90087-0 ↗
52. Microstructure, interfacial effects and micromechanics of cementitious composites
53. Petzold · 1970
54. Do fibers increase the tensile strength of cement-based matrixes?
55. Pore structures, permeabilities, and compressive strengths of concrete at temperatures up to 800°C
56. Effect of heating and cooling regimes on residual strength and microstructure of normal and high-performance concrete10.1016/S0008-8846(99)00264-1 ↗