Abstract
Abstract Cyclic degradation in flexible electronic inks remains a key challenge while their deployment in life critical applications is ongoing. The origin of electrical degradation of a screen-printed stretchable conductive ink with silver flakes embedded in a polyurethane binder is investigated under uniaxial monotonic and cyclic stretching, using in-situ confocal microscopy and scanning electron microscopy experiments, for varying ink thickness (1, 2, and 3 layers, each layer around 8–10 μ m) and trace width (0.5, 1, and 2 mm). Cracks form under monotonic stretching, and the evolution of crack pattern (density, length and width) with applied strain is affected by ink thickness such that the 3-layer ink exhibits larger normalized resistance but slightly lower resistance than the 1-layer ink up to strains of 125%. For cyclic stretching, the crack density and length do not evolve with cycling. However, the cracks widen and deepen, leading to an increase in resistance with cycling. There exists a strong correlation between fatigue life, i.e. the number of cycles until a normalized resistance of 100 is reached, and the strain amplitude. The normalized resistance increase rate with respect to cycling is also found to scale with strain amplitude. The rate of change in resistance with cycling decreases with ink thickness and trace width. For practical applications, thicker ( ⩾ 25 μ m) and wider (⩾2 mm) inks should be used to lower resistance increases with repeated deformation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Sensor and Energy Harvesting Materials · Conducting polymers and applications · Nanomaterials and Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Fully integrated wearable sensor arrays for multiplexed in situ perspiration analysis10.1038/nature16521 ↗
2. A wearable chemical–electrophysiological hybrid biosensing system for real-time health and fitness monitoring10.1038/ncomms11650 ↗
3. A graphene-based electrochemical device with thermoresponsive microneedles for diabetes monitoring and therapy10.1038/nnano.2016.38 ↗
4. Flexible polymer transistors with high pressure sensitivity for application in electronic skin and health monitoring10.1038/ncomms2832 ↗
5. Garment embedded sweat-activated batteries in wearable electronics for continuous sweat monitoring10.1038/s41528-022-00144-0 ↗
6. Advances in healthcare wearable devices10.1038/s41528-021-00107-x ↗
7. Towards flexible solid-state supercapacitors for smart and wearable electronics10.1039/c7cs00505a ↗
8. Nanocarbon‐based materials for flexible all‐solid‐state supercapacitors10.1002/adma.201705489 ↗
9. Energy autonomous electronic skin10.1038/s41528-018-0045-x ↗
10. Ultra-thin chips for high-performance flexible electronics10.1038/s41528-018-0021-5 ↗
11. Low‐power flexible organic light‐emitting diode display device10.1002/adma.201101066 ↗
12. Paper-like electronic displays: large-area rubber-stamped plastic sheets of electronics and microencapsulated electrophoretic inks10.1073/pnas.091588098 ↗
13. Stretchable active-matrix organic light-emitting diode display using printable elastic conductors10.1038/nmat2459 ↗
14. 2021 Skin-like low-noise elastomeric organic photodiodes10.1126/sciadv.abj6565 ↗
15. Flexible inorganic bioelectronics10.1038/s41528-020-0065-1 ↗
16. Flexible quantum dot light-emitting diodes for next-generation displays10.1038/s41528-018-0023-3 ↗
17. A compact polymer–inorganic hybrid gas barrier nanolayer for flexible organic light-emitting diode displays10.1038/s41528-022-00154-y ↗
18. Wearable and implantable devices for cardiovascular healthcare: from monitoring to therapy based on flexible and stretchable electronics10.1002/adfm.201808247 ↗
19. Materials for multifunctional balloon catheters with capabilities in cardiac electrophysiological mapping and ablation therapy10.1038/nmat2971 ↗
20. Study of wearables with embedded electronics through experiments and simulations
21. Wearables in medicine10.1002/adma.201706910 ↗
22. Deformation behavior of thin copper films on deformable substrates10.1016/S1359-6454(01)00293-2 ↗
23. X-ray diffraction as a tool to study the mechanical behaviour of thin films10.1016/S0921-5093(00)00876-5 ↗
24. Stretchable gold conductors on elastomeric substrates10.1063/1.1565683 ↗
25. Giant stretchability of thin gold films on rough elastomeric substrates10.1016/j.actamat.2012.10.001 ↗
26. Thickness dependent critical strain in submicron Cu films adherent to polymer substrate10.1063/1.2722684 ↗
27. High ductility of a metal film adherent on a polymer substrate10.1063/1.2108110 ↗
28. The yield strength of thin copper films on Kapton10.1063/1.1644634 ↗
29. Materials engineering for flexible metallic thin film applications10.3390/ma15030926 ↗
30. Electrical and mechanical behaviour of metal thin films with deformation-induced cracks predicted by computational homogenisation10.1007/s10704-021-00582-3 ↗
31. Effects of stretching and cycling on the fatigue behavior of polymer-supported Ag thin films10.1016/j.msea.2013.03.043 ↗
32. Fatigue of polymer-supported Ag thin films10.1016/j.scriptamat.2012.02.030 ↗
33. In-operando fatigue behavior of gold metallization lines on polyimide substrate10.1016/j.scriptamat.2020.04.021 ↗
34. The role of strain localization on the electrical behavior of flexible and stretchable screen printed silver inks on polymer substrates10.1016/j.mtla.2020.100642 ↗
35. The characterization of electrically conductive silver ink patterns on flexible substrates10.1016/j.microrel.2009.04.004 ↗
36. Performance characterization of screen printed radio frequency identification antennas with silver nanopaste10.1016/j.tsf.2009.05.019 ↗
37. Effect of printing parameters on gravure patterning with conductive silver ink10.1088/0960-1317/25/4/045004 ↗
38. Scaling and optimization of gravure-printed silver nanoparticle lines for printed electronics10.1109/TCAPT.2009.2021464 ↗
39. Mechanical behavior of strain sensors based on PEDOT: PSS and silver nanoparticles inks deposited on polymer substrate by inkjet printing10.1016/j.sna.2016.03.021 ↗
40. Surface energy patterning for ink-independent process optimization of inkjet-printed electronics10.1088/2058-8585/abcc79 ↗
41. Understanding effects of printhead geometry in aerosol jet printing10.1088/2058-8585/aba2bb ↗
42. Inkjet printing of narrow conductive tracks on untreated polymeric substrates10.1002/adma.200701876 ↗
43. One-pot synthesis of a stable and cost-effective silver particle-free ink for inkjet-printed flexible electronics10.1039/D0TC03864D ↗
44. Measurement and analysis on failure lifetime of serpentine interconnects for e-textiles under cyclic large deformation10.1088/2058-8585/abfe4c ↗
45. Reliability of R2R-printed, flexible electrodes for e-clothing applications10.1038/s41528-020-0076-y ↗
46. Buckling in serpentine microstructures and applications in elastomer-supported ultra-stretchable electronics with high areal coverage10.1039/c3sm51360b ↗
47. Electrical performance evolution and fatigue mechanisms of silver-filled polymer ink under uniaxial cyclic stretch10.1088/2058-8585/ac1243 ↗
48. Trace width effects on electrical performance of screen-printed silver inks on elastomeric substrates under uniaxial stretch10.1063/5.0056117 ↗
49. Ncorr: open-source 2D digital image correlation matlab software10.1007/s11340-015-0009-1 ↗
50. Thickness effect on the fracture and delamination of titanium films10.1016/j.tsf.2015.05.021 ↗
51. Monotonic and cyclic mechanical reliability of metallization lines on polymer substrates10.1557/jmr.2017.121 ↗
52. On the limits of the interfacial yield model for fragmentation testing of brittle films on polymer substrates10.1080/14786435.2012.723145 ↗
53. Mixed mode cracking in layered materials10.1016/S0065-2156(08)70164-9 ↗
54. Thin film cracking and the roles of substrate and interface10.1016/0020-7683(92)90227-K ↗
55. Channel cracking in thin films on substrates of finite thickness10.1023/A:1024962825938 ↗
56. Explicit relationship between electrical and topological degradation of polymer-supported metal films subjected to mechanical loading10.1063/1.4982802 ↗
57. Linking through-thickness cracks in metallic thin films to in-situ electrical resistance peak broadening10.1016/j.scriptamat.2022.114550 ↗
58. Fracture and delamination of chromium thin films on polymer substrates10.1007/s11661-009-9988-9 ↗