Properties of Rubberwood Medium-Density Fiberboard Bonded with Starch and Urea-Formaldehyde
Source abstract
Abstract
Abstract The objective of this study was to evaluate some of the properties of experimental medium-density fiberboard panels made from rubberwood (Hevea brasiliensis) using a combination of cassava (Manihot utilissima) starch and a low percentage of urea-formaldehyde (UF) resin as a binder. Experimental panels with density levels of 0.65 and 0.80 g/cm3 were made using 10 percent starch, 10 percent starch and 3 percent UF, and 10 percent UF for the control samples. The panels manufactured with 10 percent starch did not have satisfactory physical and mechanical properties based on Japanese Industrial Standards. However, average modulus of elasticity, modulus of rupture, and thickness swelling values of the sample types E and F manufactured using a combination of starch and UF were 2,044 MPa, 22.49 MPa, and 35.50 percent, respectively, which met required limits listed in Japanese Industrial Standard A-5908. The results of this study indicated that starch can be used as a viable alternative binder with limited addition of UF resin without having any significant adverse influence of bending properties of the samples. Based on formaldehyde emission tests, specimens made with 3 percent UF had an average value of 18.5 mg/100 g, while control samples having 10 percent UF resulted in 38.5 mg/100 g.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Natural Fiber Reinforced Composites · Nanocomposite Films for Food Packaging · Wood Treatment and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Akbulut, T., S.Hiziroglu, and N.Ayrilmis. 2000. Surface absorption, surface roughness, and formaldehyde emission of Turkish MDF.Forest Prod. J50 (6):45–48.
2. American National Standards Institute. 1985. Surface texture (surface roughness, waviness, and lay) B46.1. The American Society of Mechanical Engineers. New York. 43pp.
3. Chow, P., M. O.Bagby, and J. A.Youngquist. 1993. Furniture panels made from kenaf stalks, wood waste, and selected crop fiber residue.In:. Proceedings of the 5th Annual International Kenaf Conference, March 3–5, 1993, Fresno, California. California State University Press. Fresno. pp.250–255.
4. European Committee for Standardization. 1993. Wood based panels. Determination of formaldehyde content. EN 120. European Committee for Standardization. Brussels.
5. Falvey, L. 2000. Thai Agriculture. Golden Cradle of Millennia. Kasetsart University Press. Bangkok, Thailand.
6. Hiziroglu, S. 1996. Surface roughness analysis of wood composites: A stylus method.Forest Prod. J46 (7/8):67–72.
7. Hiziroglu, S., S.Jarusombuti, and V.Fueangvivat. 2004. Surface characteristics of wood composites manufactured in Thailand.J. Building Environ39:1359–1364.
8. Hong, L. T. and H. C.Sim. 1994. Rubberwood processing and utilization. Malaysian Forest Record No. 39. Forest Research Institute of Malaysia. Kepong, Kuala Lumpur.
9. Japanese Industrial Standards (JIS). 1995. Particleboards. A-5908. Japanese Standards Association. Tokyo.
10. Kim, S. and H. J.Kim. 2005. Comparison of standard methods and gas chromatography method in determination of formaldehyde emission from MDF bonded with formaldehyde-based resin.Bioresour. Technol96:1457–1464.
11. Krukanont, P. and S.Prasertsan. 2004. Geographical distribution of biomass and potential sites of rubber wood fired power plants in Southern Thailand.Biomass Bioenergy26:47–59.
12. Maloney, T. 1993. Modern Particleboard and Dry Process Fiberboard Manufacture. Miller Freeman. San Francisco.
13. Marutzky, R. 1989. Release of formaldehyde by wood products.In:Wood Adhesives—Chemistry and Technology. Vol. 2. Pizzi, A.Marcel Dekker Inc.. New York. pp.307–387.
14. Moubarik, A., A.Allal, A.Pizzi, F.Charrier, and B.Charrier. 2010a. Preparation and mechanical characterization of particleboard made from maritime pine and glued with bio-adhesives based on cornstarch and tannins.Maderas Cienc. Tecnol12 (3):189–197.
15. Moubarik, A., B.Charrier, A.Allal, F.Charrier, and A.Pizzi. 2010b. Development and optimization of a new formaldehyde-free cornstarch and tannin wood adhesive.Eur. J. Wood Wood Prod68 (2):167–177.
16. Moubarik, A., B.Charrier, F.Charrier, A.Pizzi, and A.Allal. 2009. Evaluation of decay resistance of wood products made from borax-impregnated wood and bonded with a formaldehyde-free cornstarch and tannin adhesive.Ann. Forest Sci66 (1):DOI:10.1051/forest/2008082.10.1051/forest/2008082 ↗
17. Mummery, L. 1993. Surface Texture Analysis. The Handbook. Hommelwerke. Muhlhausen, Germany. 106pp.
18. Nihat, S. C. and O.Nilgun. 2002. Use of organosolv lignin in phenol formaldehyde resin for particleboard production II. Particleboard production and properties.Int. J. Adhes. Adhes22:481–486.
19. Pichelin, F., M.Nakatanin, A.Pizzi, S.Wieland, A.Despres, and S.Rigolet. 2006. Structural beams from thick wood panels bonded industrially with formaldehyde-free tannin adhesives.Forest Prod. J56 (5):31–36.
20. Roffael, E. 1993. Formaldehyde release from particleboard and other wood based panels. Malaysian Forest Records No. 37. Forest Research Institute of Malaysia. Kepong, Kuala Lumpur.
21. Yamamoto, H., E.Makita, Y.Oki, and M.Otani. 2006. Flow characteristics and gelatinization kinetics of rice starch under strong alkali conditions.Food Hydrocoll20:9–20.
22. Yuan, L. and L.Kaichang. 2007. Development and characterization of adhesive from soy protein for bonding wood.Int. J. Adhes. Adhes27:59–67.
23. Yusoff, M. N. M. 1994. Panel products from rubberwood particleboard, blockboard and medium density fiberboard.In:Rubberwood Processing and Utilization. Malaysian Forest Records No. 39. Hong, L. T. and H. C.Sim. Forest Research Institute of Malaysia. Kepong, Kuala Lumpur.
24. Zhongli, P., A.Cathcart, and D.Wang. 2006. Properties of particleboard bond with rice bran and polymeric methylene diphenyl diisocyanate adhesives.Ind. Crops Prod23:40–45.