Binderless Particleboard Resistance to Termite Attack
Source abstract
Abstract
Abstract Three particleboard types, including urea-formaldehyde (UF), melamine-formaldehyde (MF), and binderless, were made from three wood species, sengon (Paraserianthes falcataria), gmelina (Gmelina arborea), and mindi (Melia azedarach). Wood particle sizes of 10 to 20 mesh were manufactured for the 30 by 30 by 0.7-cm (length by width by thickness) boards, with 0.75 g/cm3 as the density target. Binderless particleboards were made through particle activation with hydrogen peroxide and ferrous sulfate as the catalyst, and the boards were hot pressed at 180°C for 12 minutes. For the purpose of comparison, conventional particleboards were made with UF and MF, with the resin level at 10 percent and the boards hot pressed at 120°C for 7 minutes. All particleboards were conditioned for 8 months prior to testing against the subterranean termite (Coptotermes curvignathus Holmgren) in laboratory and field tests, and against the dry wood termite (Cryptotermes cynocephalus Light) in laboratory tests. Results showed that wood species affected particleboard resistance in both of the subterranean termite tests and that the type of particleboard affected board resistance in field tests. Particleboard from sengon wood had the lowest resistance in both tests, followed by from gmelina and mindi woods, and particleboards with UF and MF resins had better resistance than binderless particleboard in field tests. Particleboard type and wood species did not affect board resistance to dry wood termite attack.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Insect and Arachnid Ecology and Behavior · Forest Insect Ecology and Management · Insect and Pesticide Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Arango, R. A., F. Green, K. Hintz, P. K. Lebow, and R. B. Miller. 2006. Natural durability of tropical and native woods against termite damage by Reticulitermes flavipes (Kollar). Int. Biodeterior. Biodegrad. 57:146–150.
2. Hadi, Y. S., E. Fajriani, D. Hermawan, M. Y. Massijaya, and N. Hadjib. 2011. Resistance of particleboard made from fast growing species to subterranean termite attack. In:Proceedings of the 8th Conference of the Pacific Rim Termite Research Group, February 28–March 1, 2011,Bangkok, Thailand; Pacific Rim Termite Research Group. pp. 142–145.
3. Hadi, Y. S., T. Nurhayati, and J. Jasni. 2010. Smoked wood as an alternative for wood protection against termites. Forest Prod. J. 60(6):496–500.
4. Hashim, R., N. Said, J. Lamaming, M. Baskaran, O. Sulaiman, M. Sato, S. Hiziroglu, and T. Sugimoto. 2011. Influence of press temperature on the properties of binderless particleboard made from oil palm trunk. J. Mater. Design32:2520–2525.
5. Japanese Standards Association (JSA). 2003. Particleboards. Japanese Industrial Standard (JIS) A 5908‐2003. JSA, Tokyo.
6. Karlsson, O. and U. Westermark. 2002. Resin-free particleboard by oxidation of wood. In:Proceedings of the 6th Pacific Rim Bio-Based Composites Symposium and Workshop on the Chemical Modification of Cellulosics, November 10–13, 2002,Portland, Oregon; Oregon State University. pp. 149–153.
7. Lukmandaru, G. and K. Takahashi. 2008. Variation in the natural termite resistance of teak (Tectona grandis Linn. Fil) wood as a function of tree age. Ann. Forest Sci. 65(7):708.
8. Martawijaya, A., I. Kartasujana, Y. I. Mandang, S. A. Prawira, and K. Kadir. 1989. Indonesian Wood Atlas. Vol. 2. Forestry Research and Development Agency, Forestry Ministry, Bogor, Indonesia.
9. Ministry of Forestry. 2010. Statistik 2009. Directorate of Natural Forest Development, Directorate General Forest Products. Ministry of Forestry, Jakarta, Indonesia.
10. Nandika, D., Y. Rismayadi, and F. Diba. 2003. Termite: Behavior and Control. Muhammadiyah University Press, Surakarta, Indonesia.
11. Pablo, M. R. S. and C. M. Garcia. 1997. Natural durability of anahau (Livistona rotundifolia Lam. Mart.). Forest Prod. Res. Develop. Inst. J. 23:69–76.
12. Standar Nasional Indonesia (SNI). 2006a. Particleboard. SNI 03‐2105‐2006. National Standardization Bureau, Jakarta, Indonesia.
13. Standar Nasional Indonesia (SNI). 2006b. Wood and wood products resistance test to wood destroying organisms. SNI 01.7207‐2006. National Standardization Bureau, Jakarta, Indonesia.
14. Suhasman, M., Y. Massijaya, Y. S. Hadi, and A. Santoso, 2010. Hydrogen peroxide and ferrous sulfate activated wood particles for binderless particleboard. J. Trop. Wood Sci. Technol. 8(1):1–8.
15. Suhasman, M., Y. Massijaya, Y. S. Hadi, and A. Santoso. 2011. Particle oxidation time for the manufacture of binderless particleboard. Wood Res. J. 2(1):9–18.
16. Weaver, F. W. and N. L. Owen. 1992. The isocyanate-wood adhesive bond. In:Proceedings of the Pacific Rim Bio-Based Composites Symposium, November 9–13, 1992,Rotorua, New Zealand; New Zealand Forest Research Institute.
17. Widsten, P., P. Qvintus-Leino, S. Tuominen, and J. E. Laine. 2003. Manufacture of fiberboard from wood fibers activated with Fenton's reagent (H2O2/FeSO4). Holzforschung57:447–452.
18. Widsten, P., S. Tuominen, P. Qvintus-Leino, and J. E. Laine. 2004. The influence of high defibration temperature on the properties of medium-density fiberboard (MDF) made from laccase-treated softwood fibers. Wood Sci. Technol. 38:521–528.
19. Widyorini, R., T. Higashihara, J. Xu, T. Watanabe, and S. Kawai. 2005. Self-bonding characteristics of binderless kenaf core composites. J. Wood Sci. 39:651–662.