journal article·2022Open access

Comparison of Water Resistance for Modified Medium-Density Fiberboard

Luis Molina Irribarra, Frederick A. Kamke, Scott Leavengood

Forest Products Journal· Volume 72· Issue 4

Abstract

Abstract Commercial medium-density fiberboard (MDF) products, specifically manufactured for water resistance, were evaluated over 8 days under three water exposure regimes: 90 percent relative humidity, one-sided water spray, and one-sided wet pad. A three-cycle wet-pad and drying exposure test was also performed. Rate of swelling, extent of swelling, and irreversible thickness swelling were determined. Acetylated MDF (AMDF) had the best overall performance, followed by steam-injection pressed MDF (SMDF) and polymeric methylene-diphenyl-diisocyanate–bonded moisture-resistant MDF. The fastest rate of thickness swell and linear expansion occurred with exposure to one-sided water spray and the slowest with 90 percent relative humidity exposure. While AMDF was clearly superior after 24-hour exposure, the other MDF products were nearly identical. Significant difference in thickness swell and water absorption between moisture-resistant MDF and SMDF developed after 24 hours. Regardless of the method of water exposure, the trend of best to worst MDF performance was the same.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Natural Fiber Reinforced Composites · Material Properties and Processing · Textile materials and evaluations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Ahmed, S. A., Adamopoulos, S. Li, J. and J. Kovacikova,. 2020. Prediction of mechanical performance of acetylated MDF at different humid conditions. Appl. Sci. 8712.doi:10.3390/app10238712.
2. American National Standards Institute (ANSI). 2016. Medium density fiberboard (MDF) for interior applications. ANSI A208.2-2016. Composite Panel Association, Leesburg, Virginia.
3. American National Standards Institute (ANSI). 2020 a. Engineered wood siding. ANSI A135.6-2012(R2020). Composite Panel Association, Leesburg, Virginia.
4. American National Standards Institute (ANSI). 2020 b. Engineered wood trim. ANSI A135.7-2012(R2020).Composite Panel Association, Leesburg, Virginia.
5. American Society for Testing and Materials. 2020. Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM D1037-12(R2020). ASTM International, West Conshohocken, Pennsylvania.
6. Hill, C. A. S. 2006. Wood Modification: Chemical, Thermal and Other Processes. Chichester: John Wiley & Sons.
7. Li, X., Zheng, X. and Li.H. 2011. Steam-injection pressing technology of man-made board. Key Eng. Mater. 474: 1351– 1355. doi:10.4028/www.scientific.net/KEM.474-476.1351.
8. Mai, C., Direske, M. Varel, D. and Weber.A. 2016. Light medium-density fiberboards (MDFs): Does acetylation improve the physico-mechanical properties?Eur. J. Wood Wood Prod. 75: 739– 745.
9. Passarini, L., Zelinka, S. L. Glass, S. V. and Hunt.C. G. 2017. Effect of weight percent gain and experimental method on fiber saturation point of acetylated wood determined by differential scanning calorimetry. Wood Sci. Technol. 51: 1291– 1305.
10. Popescu, C.-M., Hill, C. A. S. Curling, S. Ormondroyd, G. and Xie.Y. 2014. The water vapour sorption behaviour of acetylated birch wood: How acetylation affects the sorption isotherm and accessible hydroxyl content. J. Mater. Sci. 49: 2362– 2371.
11. Rowell, R. 2006. Acetylation of wood—A journey from analytical technique to commercial reality. Forest Prod. J. 56(9): 4– 12.
12. RStudio Team. 2019. RStudio: Integrated Development for R. http://www.rstudio.com. Accessed November 10, 2019.
13. Sebera, V., Tippner, J. Šimek, M. Šrajer, J. and Decký.K. 2014. Poisson's ratio of the MDF in respect to vertical density profile. Eur. J. Wood Wood Prod. 72: 407– 410.
14. Wolcott, M., Kamke, F. A. and Dillard.D. A. 1994. Fundamental aspects of wood deformation pertaining to manufacture of wood-based composites. Wood Fiber Sci. 26(4): 496– 511.