journal article·2015-09

Application of Near-Infrared Spectroscopy to Determine the Juvenile–Mature Wood Transition in Black Spruce

Guillaume Giroud, Maurice Defo, Jean Bégin, Chhun-Huor Ung

Forest Products Journal· Volume 65· Issue 3-4
Publisher page

Abstract

Abstract The potential of near-infrared spectroscopy (NIRS) to determine the transition from juvenile to mature wood in black spruce (Picea mariana (Mill.) B.S.P.) was assessed. In total, 127 wood samples were harvested from 50 sites located across the black spruce–moss domain in the province of Québec, Canada. Mechanical wood properties were determined by SilviScan. NIR spectra were collected on the transverse face of the samples. Good to excellent calibration statistics (R2, ratio of performance to deviation) were obtained for basic density (0.85, 1.8), microfibril angle (0.79, 2.2), and modulus of elasticity (0.88, 2.9). Two-segment linear regressions were applied to microfibril angle profiles to determine the transition age and then calculate the juvenile and mature wood properties. The values obtained using SilviScan data were compared with those obtained using NIRS predicted data. Using SilviScan data, the average transition age was 23 years, with a standard deviation of 7 years. The correlation was moderate for the transition age (r = 0.592, P < 0.0001), which was slightly underestimated by NIRS with a mean prediction error (and 95% limits of agreement) of −2.2 ± 6.3 years (−14.6/10.1). These results suggest that the transition age from juvenile to mature wood could be predicted by NIRS. This article makes some recommendations to improve method accuracy for operational use.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Wood and Agarwood Research · Forest ecology and management

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The authors are, respectively, PhD Scholar, Researcher, and Professor, Dépt. des Sci. du bois et de la forêt, Faculté de foresterie, de géographie et de géomatique, Univ. Laval, Québec, Canada (Guillaume.Giroud@mffp.gouv.qc.ca [corresponding author], Maurice.Defo@sbf.ulaval.ca, Jean.Begin@sbf.ulaval.ca); and Retired Researcher, Natural Resources Canada, Canadian Forest Serv., Canadian Wood Fibre Centre, Québec, Canada (chhunhuorung@gmail.com). This paper was received for publication in April 2014....

References (36)

Show source-provided references
1. Alteyrac, J., A. Cloutier, and S. Y.Zhang. 2006. Characterization of juvenile wood to mature wood transition age in black spruce (Picea mariana (Mill.) B.S.P.) at different stand densities and sampling heights. Wood Sci. Technol. 40(2):124–138.
2. Barnett, J. R.and V. A.Bonham. 2004. Cellulose microfibril angle in the cell wall of wood fibres. Biol. Rev. 79(2):461–472.
3. Bhat, K. M., P. B. Priya, and P.Rugmini. 2001. Characterisation of juvenile wood in teak. Wood Sci. Technol. 34(6):517–532.
4. Bland, J. M.and D. G.Altman. 1995. Comparing methods of measurement: Why plotting difference against standard method is misleading. Lancet346(8982):1085–1087.
5. Briggs, D. 2010. Enhancing forest value productivity through fiber quality. J. Forestry108(4):174–182.
6. Cieszewski, C. J., M. Strub, F. Antony, P. Bettinger, J. Dahlen, and R. C.Lowe. 2013. Wood quality assessment of tree trunk from the tree branch sample and auxiliary data based on NIR spectroscopy and SilviScan. Math. Comput. Forestry Nat.-Res. Sci. 5(26):86–111.
7. Clark, A., III, R. F. Daniels, and L.Jordan. 2006. Juvenile/mature wood transition in loblolly pine as defined by annual ring specific gravity, proportion of latewood, and microfibril angle. Wood Fiber Sci. 38(2):292–299.
8. Donaldson, L. 2008. Microfibril angle: Measurement, variation and relationships—A review. IAWA J. 29(4):345–386.
9. Evans, R. 1999. A variance approach to the X-ray diffractometric estimation of microfibril angle in wood. Appita J. 52(4):283–289.
10. Evans, R., S. Stringer, and R.Kibblewhite. 2000. Variation of microfibril angle, density and fibre orientation in twenty-nine Eucalyptus nitens trees. Appita J. 53(6):450–457.
11. Hein, P., B. Clair, L. Brancheriau, and G.Chaix. 2010. Predicting microfibril angle in Eucalyptus wood from different wood faces and surface qualities using near infrared spectra. J. Near Infrared Spectrosc. 18(6):455–464.
12. Jessome, A. P. 1995. Strength and related properties of woods grown in Canada. SP-514F. Forintek Canada Corp., Ottawa, Ontario. 37pp.
13. Jones, P. D., L. R. Schimleck, G. F. Peter, R. F. Daniels, and ClarkA.III. 2005. Nondestructive estimation of Pinus taeda L. wood properties for samples from a wide range of sites in Georgia. Can. J. Forest Res. 35(1):85–92.
14. Jozsa, L. A.and G. R.Middleton. 1994. A discussion of wood quality attributes and their practical implications. SP-34. Forintek Canada Corp., Vancouver, British Columbia. 42pp.
15. Lessard, E. 2013. Modeling and mapping wood fiber attributes using environmental and forest inventory data: Case of Newfoundland's boreal forest. Master's thesis in geographic sciences. Université de Sherbrooke, Québec, Canada. 103pp. (In French.)
16. Lessard, E., R. A. Fournier, J. E. Luther, M. J. Mazerolle, and O. R.Van Lier. 2014. Modeling wood fiber attributes using forest inventory and environmental data for Newfoundland's boreal forest. Forest Ecol. Manag. 313:307–318.
17. Meder, R., T. Trung, and L.Schimleck. 2010. Guest editorial: Seeing the wood in the trees: Unleashing the secrets of wood via near infrared spectroscopy. J. Near Infrared Spectrosc. 18(6):v–vii.
18. Panshin, A. J.and C.De Zeeuw. 1980. Textbook of Wood Technology: Structure, Identification, Properties, and Uses of the Commercial Woods of the United States and Canada. 4th ed. McGraw-Hill, New York. 722pp.
19. Pérez-Marín, D., A. Garrido-Varo, and J. E.Guerrero. 2007. Non-linear regression methods in NIRS quantitative analysis. Talanta72(1):28–42.
20. Ryan, S. E.and L. S.Porth. 2007. A tutorial on the piecewise regression approach applied to bedload transport data. General Technical Report RMRS-GTR-189. USDA Forest Service, Rocky Mountain Research Station, Fort Collins, Colorado. 41pp.
21. Schimleck, L. R.and R.Evans. 2002. Estimation of microfibril angle of increment cores by near infrared spectroscopy. IAWA J. 23(3):225–234.
22. Schimleck, L. R., R. Evans, and J.Ilic. 2001. Estimation of Eucalyptus delegatensis wood properties by near infrared spectroscopy. Can. J. Forest Res. 31(10):1671–1675.
23. Schimleck, L. R., P. D. Jones, Clark A. III, R. F. Daniels, and G. F.Peter. 2005 a. Near infrared spectroscopy for the nondestructive estimation of clear wood properties of Pinus taeda L. from the southern United States. Forest Prod. J. 55(12):21–28.
24. Schimleck, L. R., R. Stürzenbecher, C. Mora, P. D. Jones, and R. F.Daniels. 2005 b. Comparison of Pinus taeda L. wood property calibrations based on NIR spectra from the radial-longitudinal and radial-transverse faces of wooden strips. Holzforschung59(2):214–218.
25. Siau, J. F. 1995. Wood: Influence of moisture on physical properties. Department of Wood Science and Forest Products, Virginia Polytechnic Institute and State University, Blacksburg. 227pp.
26. Siesler, H. W., Y. Ozaki, S. Kawata, and H. M.Heise. 2002. Near-Infrared Spectroscopy: Principles, Instruments, Applications. Wiley-VCH, Weinheim, Germany. 348pp.
27. So, C.-L., J. H. Myszewski, T. Elder, and L. H.Groom. 2013. Rapid analysis of the microfibril angle of loblolly pine from two test sites using near-infrared analysis. Forestry Chron. 89(5):639–645.
28. Tsuchikawa, S. 2007. A review of recent near infrared research for wood and paper. Appl. Spectrosc. Rev. 42(1):43–71.
29. Via, B. 2010. Prediction of oriented strand board wood strand density by near infrared and Fourier transform infrared reflectance spectroscopy. J. Near Infrared Spectrosc. 18(6):491–498.
30. Via, B. K., T. F. Shupe, L. H. Groom, M. Stine, and C.-L.So. 2003. Multivariate modelling of density, strength and stiffness from near infrared spectra for mature, juvenile and pith wood of longleaf pine (Pinus palustris). J. Near Infrared Spectrosc. 11(5):365–378.
31. Via, B. K., C. L. So, T. F. Shupe, L. H. Groom, and J.Wikaira. 2009. Mechanical response of longleaf pine to variation in microfibril angle, chemistry associated wavelengths, density, and radial position. Compos. Part A40(1):60–66.
32. Viereck, L. A.and W. F.Johnston. 1990. Picea mariana (Mill.) B.S.P.—Black spruce. In:Silvics of North America. Vol. 1. Conifers. Agricultural Handbook 654. BurnsR. M.and HonkalaB. H.(Eds.). USDA Forest Service, Washington, D.C. pp. 227–237.
33. Wang, M.and J. D.Stewart. 2012. Determining the transition from juvenile to mature wood microfibril angle in lodgepole pine: A comparison of six different two-segment models. Ann. Forest Sci. 69(8):927–937.
34. Williams, P. C.and D. C.Sobering. 1993. Comparison of commercial near infrared transmittance and reflectance instruments for analysis of whole grains and seeds. J. Near Infrared Spectrosc. 1(1):25–32.
35. Xu, Q., M. Qin, Y. Ni, M. Defo, B. Dalpke, and G.Sherson. 2011. Predictions of wood density and module of elasticity of balsam fir (Abies balsamea) and black spruce (Picea mariana) from near infrared spectral analyses. Can. J. Forest Res. 41(2):352–358.
36. Yang, K. C.and G.Hazenberg. 1994. Impact of spacing on tracheid length, relative density, and growth rate of juvenile wood and mature wood in Picea mariana. Can. J. Forest Res. 24(5):996–1007.