Influence of Specimen Size on Accelerated Weathering of Laminated Veneer Lumber
Source abstract
Abstract
Abstract Moisture intrusion can be significantly higher along specimen edges, particularly at edges where longitudinal grain is exposed, which is referred to as the edge effect. The influence of edge effects on moisture durability are assumed to decrease as the edge area to total-surface-area ratio decreases. Moisture durability assessment of laminated veneer lumber (LVL) is commonly evaluated using accelerated weathering (AW) and outdoor exposure methods, where small specimens are analyzed. The influence of specimen size (i.e., edge effect) on moisture durability evaluation of LVL was investigated in this study. To vary specimen size, three widths with constant length and thickness were evaluated. In addition, three AW methods were used to characterize how the method of inflicting degradation influenced edge effects. No consistent trends in mechanical property loss were found across AW methods, indicating that the influence of specimen size varied with AW method. The greatest influence of specimen size occurred when cyclic vacuum-soak-dry was included, where water absorption decreased significantly with increasing width, and three of four mechanical properties evaluated displayed an influence of specimen size. The smallest influence of specimen size occurred when a single soak-dry procedure was included, where only one of four mechanical properties evaluated displayed an influence of specimen size. Results from this study provide evidence that edge effects may occur during LVL moisture durability assessment but that the severity is dependent on AW conditions.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Cultural Heritage Materials Analysis · Material Properties and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Alexopoulos, J. 1992. Accelerated aging and outdoor weathering of aspen waferboard. Forest Prod. J. 44(2):15–22.
2. American Wood Council (AWC). 2015. General dowel equations for calculating lateral connection values. Technical Report 12. AWC, Leesburg, Virginia.
3. APA—The Engineered Wood Association. 2010. Engineered wood construction guide. Form No. E30. APA, Tacoma, Washington.
4. APA—The Engineered Wood Association. 2011. PS 2-10: Performance standard for wood-based structural-use panels. APA, Tacoma, Washington
5. ASTM International. 2012. Standard test methods for evaluating properties of wood-base fiber and particle panel materials. ASTM-D1037. ASTM International, West Conshohocken, Pennsylvania.
6. ASTM International. 2013. Standard test methods of static tests of lumber in structural sizes. ASTM-D198. ASTM International, West Conshohocken, Pennsylvania.
7. ASTM International. 2014. Standard specification for evaluation of structural composite lumber products. ASTM-D5456. ASTM International, West Conshohocken, Pennsylvania.
8. ASTM International. 2016. Standard test methods for direct moisture content measurement of wood and wood-based materials. ASTM-D4442. ASTM International, West Conshohocken, Pennsylvania.
9. Baker, A. J. and R. H. Gillespie. 1978. Accelerated aging of phenolic-bonded flakeboards. General Technical Report WO-5. USDA Forest Service, Washington D.C.
10. Bodig, J. and J. Fyie. 1986. Performance requirements for exterior laminated veneer lumber. Forest Prod. J. 36(2):49–54.
11. Breyer, D., K. Cobeen, K. Fridley, and D. Pollock. 2015. Design of Wood Structures—ASD/LRFD. 7th ed. McGraw Hill Education, New York.
12. Chen, G. W., R. C. Tang, and E. W. Price. 1989. Effect of environmental conditions on the flexural properties of wood composite I-beams and lumber. Forest Prod. J. 39(2):17–22.
13. Glass, S. V. and S. L. Zelinka. 2010. Chapter 4: Wood moisture relations and physical properties of wood. In:Wood Handbook. Wood as an Engineering Material. General Technical Report No. FPL-GTR-190. USDA Forest Products Laboratory, Madison, Wisconsin. 509pp.
14. Hayashi, T., A. Miyatake, and M. Harada. 2002. Outdoor exposure tests of structural laminated veneer lumber 1: Evaluation of the physical properties after six years. J. Wood Sci. 48:69–74.
15. Kamke, F. A. and J. E. Winandy. 2008. Issues and concepts for making durable composites. In: Proceedings 104th annual meeting of the American Wood Protection Association, Portland, Oregon; American Wood Protection Association, Birmingham, Alabama. pp. 116–124.
16. King, D., A. Sinha, and J. J. Morrell. 2014. Effects of outdoor exposure on properties of I-joists. Wood Fiber Sci. 46(3):394–400.
17. Kojima, Y., H. Norita, and S. Suzuki. 2009. Evaluating the durability of wood-based panels using thickness swelling results from accelerated aging treatments. Forest Prod. J. 59(5):35–41.
18. Kojima, Y., T. Shimoda, and S. Suzuki. 2011. Evaluation of the weathering intensity of wood-based panels under outdoor exposure. J. Wood Sci. 57(5):408–414.
19. Kojima, Y., T. Shoji, T. Aoki, H. Kobori, and S. Suzuki. 2017. Effect of starting time and test specimen size on the deterioration of particleboard in an outdoor exposure test. Forest Prod. J. 67(7/8):448–454.
20. Kojima, Y. and S. Suzuki. 2011. Evaluation of wood-based panel durability using bending properties after accelerated aging treatments. J. Wood Sci. 57(1):126–133.
21. Kuehl, R. 2000 a. Chapter 6: Factorial treatment designs. In: Design of Experiments: Statistical Principles of Research Design and Analysis. Brooks/Cole, Belmont, California. pp. 175–231.
22. Kuehl, R., 2000 b. Chapter 3: Treatment comparisons. In: Design of Experiments: Statistical Principles of Research Design and Analysis. Brooks/Cole, Belmont, California. pp. 73–122.
23. Laleicke, P. 2015. Non-destructive detection and monitoring of durability issues in wood panels under accelerated-weathering. PhD thesis. Oregon State University, Corvallis. 114pp.
24. Laufenberg, T. 1982. Exposure effects upon performance of laminated veneer lumber and glulam materials. Forest Prod. J. 32(5):42–48.
25. Lenth, R.V. 2016. Least-squares means: The R package lsmeans. J. Stat. Softw. 69(1):1–33.
26. Mirzaei, B., A. Sinha, and J. A. Nairn. 2015. Using crack propagation fracture toughness to characterize the durability of wood and wood composites. Mater. & Des. 87:586–592.
27. Mirzaei, B., A. Sinha, and J. A. Nairn. 2016. Assessing the role of adhesives in durability of laminated veneer lumber (LVL) by fracture mechanics. Holzforschung70(8):763–771.
28. Mohammad, M.A. and I. Smith. 1996. Effects of multi-phase moisture conditioning on stiffness of nailed OSB-to-lumber connections. Forest Prod. J. 46(4):76–83.
29. Nelson, S. 1997. Chapter 6: Structural composite lumber. In: Engineered Wood Products: A Guide for Specifiers, Designers, and Users. PFS Research Foundation, Madison, Wisconsin. pp. 147–152.
30. Northcott, P. L. and H. G. M. Colbeck. 1960. Prediction of plywood bond durability. Forest Prod. J. 10(8):403–408.
31. Okkonen, A. E. and B. H. River. 1996. Outdoor aging of wood-based panels and correlation with laboratory aging: Part 2. Forest Prod. J. 46(3):68–74.
32. Olek, W., P. Perré, and J. Weres. 2005. Inverse analysis of the transient bound water diffusion in wood. Holzforschung59(1):38–45.
33. Paridah, M., A. Zaidon, T. Chuo, A. Zakiah, and U. Anwar. 2012. Accelerated and outdoor ageings of laminated veneer lumber and their correlations with strength and stiffness. J. Trop. Forest Sci. 24(4):465–473.
34. Pinheiro, J., D. Bates, S. DebRoy, and D. Sarkar. 2017. nlme: Linear and nonlinear mixed effects models. R package version 3.1–131. https://cran.r-project.org/web/packages/nlme/nlme.pdf. Accessed October 21, 2018.
35. Pizzi, A., 2003. Phenolic resin adhesives. In: Handbook of Adhesive Technology. A. Pizziand K. L. Mittal (Eds.). Marcel Dekker, New York. pp. 541–572.
36. R Core Team, 2015. A Language and Environment for Statistical Computing. R Foundation for Statistical Computing, Vienna.
37. Ramsey, F. L. and D. W. Schafer. 2012. Chapter 2: Inference using t-distributions. In: The Statistical Sleuth: A Course in Methods of Data Analysis. Brooks/Cole, Boston. pp. 28–57.
38. River, B. H. 1994. Outdoor aging of wood-based panels and correlation with laboratory aging. Forest Prod. J. 44(11/12):55–65.
39. Saad, S., H. Kobori, Y. Kojima, and S. Suzuki. 2016. Performance evaluation of wood-based panels under a mild accelerated aging treatment. J. Wood Sci. 62(4):324–331.
40. Siau, J. S. 1995. Chapter 6: Steady-state moisture diffusion. In: Wood: Influence of Moisture on Physical Properties. Department of Wood Science and Forest Products, Virginia Polytechnic Institute and State University, Blacksburg, Virginia. 112pp.
41. Sonderegger, W., S. Hering, D. Mannes, P. Vontobel, E. Lehmann, and P. Niemz. 2010. Quantitative determination of bound water diffusion in multilayer boards by means of neutron imaging. Eur. J. Wood Prod. 68(3):341–350.
42. Way, D., F. A. Kamke, and A. Sinha. 2018. Influence of specimen size during accelerated weathering of wood-based structural panels. Wood Mater. Sci. Eng. DOI: 10.1080/17480272.2018.145983610.1080/17480272.2018.1459836 ↗