Accelerated Weathering of Recycled Polypropylene Packaging Bag Composites Reinforced with Wheat Straw Fibers
Source abstract
Abstract
Abstract In this study, there were two kinds of recycled polypropylene (RPP) packaging bags, RPP disposable packaging bags (RPP-DB) and RPP woven bags (RPP-WB), used as matrix reinforced with wheat straw fiber (WSF). The aim of this study was to investigate the relative degradation behavior of WSF/RPP composites with two RPP matrices under weathering conditions. The RPP packaging bags were blended with WSF by a two-roll mill mixer and then molded by a compression molding machine. The effects of accelerated weathering on the surface morphology, surface color, surface chemistry, thermal properties, and mechanical properties were evaluated after distinct periods; the total time of exposure of the composites in a QUV-accelerated weathering tester was 1,200 hours. The weathering degradation process of WS/RPP-DB was gradual from surface to interior, whereas the internal collapse aggravated the performance reduction of WS/RPP-WB. The weathering resulted in significant discoloration. The photobleaching of WS/RPP-DB was faster than of WS/RPP-WB. The Fourier-transform infrared spectrum suggested that the color change was closely related to the formation of carbonyl groups and degradation of lignin. After weathering, the thermal properties of WS/RPP-DB and WS/RPP-WB were both decreased. The flexural strength and modulus of WS/RPP strongly decreased with exposure time and was related to the surface crack of composites. The utilization of RPP packaging bags as matrix could be a good candidate of wood–plastic composites for applications in the future.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Natural Fiber Reinforced Composites · Advanced Cellulose Research Studies · Mechanical Behavior of Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Abdel-Bary, E. (Ed.). 2003. Handbook of Plastic Films. Smithers Rapra Publishing, Shawbury, Shrewsbury, Shropshire, UK.
2. Abu-Sharkh, B. and H. Hamid. 2004. Degradation study of date palm fibre/polypropylene composites in natural and artificial weathering: mechanical and thermal analysis. Polym. Degrad. Stab. 85(3):967–973.
3. Achilias, D., E. Antonakou, C. Roupakias, P. Megalokonomos, and A. Lappas. 2008. Recycling techniques of polyolefins from plastic wastes. Global Nest J. 10(1):114–122.
4. Alvarez, V. and A. Vázquez. 2004. Thermal degradation of cellulose derivatives/starch blends and sisal fibre biocomposites. Polym. Degrad. Stab. 84(1):13–21.
5. Assarar, M., D. Scida, A. El Mahi, C. Poilâne, and R. Ayad. 2011. Influence of water ageing on mechanical properties and damage events of two reinforced composite materials: Flax–fibres and glass–fibres. Mater. Des. 32(2):788–795.
6. ASTM International. 2015. Standard practice for calculation of color tolerances and color differences from instrumentally measured color coordinates. ASTM D2244‐15a. ASTM International, West Conshohocken, Pennsylvania.
7. Athijayamani, A., M. Thiruchitrambalam, U. Natarajan, and B. Pazhanivel. 2009. Effect of moisture absorption on the mechanical properties of randomly oriented natural fibers/polyester hybrid composite. Mater. Sci. Eng. A517(1):344–353.
8. Azwa, Z., B. Yousif, A. Manalo, and W. Karunasena. 2013. A review on the degradability of polymeric composites based on natural fibres. Mater. Des. 47:424–442.
9. Beg, M. D. H. and K. L. Pickering. 2008. Accelerated weathering of unbleached and bleached Kraft wood fibre reinforced polypropylene composites. Polym. Degrad. Stab. 93(10):1939–1946.
10. Butylina, S., M. Hyvärinen, and T. Kärki. 2012a. Accelerated weathering of wood–polypropylene composites containing minerals. Compos. A Appl. Sci. Manuf. 43(11):2087–2094.
11. Butylina, S., M. Hyvärinen, and T. Kärki. 2012b. A study of surface changes of wood–polypropylene composites as the result of exterior weathering. Polym. Degrad. Stab. 97(3):337–345.
12. Fabiyi, J. S., A. G. McDonald, and D. McIlroy. 2009. Wood modification effects on weathering of HDPE-based wood plastic composites. J. Polym. Environ. 17(1):34–48.
13. Fabiyi, J. S., A. G. McDonald, M. P. Wolcott, and P. R. Griffiths. 2008. Wood–plastic composites weathering: Visual appearance and chemical changes. Polym. Degrad. Stab. 93(8):1405–1414.
14. George, J., M. Sreekala, and S. Thomas. 2001. A review on interface modification and characterization of natural fiber reinforced plastic composites. Polym. Eng. Sci. 41(9):1471–1485.
15. Hawkins, G. 2001. Plastic bags: Living with rubbish. Int. J. Cult. Stud. 4(1):5–23.
16. He, H. 2010. The effects of an environmental policy on consumers: Lessons from the Chinese plastic bag regulation. Environment & Development Economics17(453).
17. Homkhiew, C., T. Ratanawilai, and W. Thongruang. 2014. Effects of natural weathering on the properties of recycled polypropylene composites reinforced with rubberwood flour. Ind. Crops Prod. 56:52–59.
18. Hon, D. N.-S. and N. Shiraishi. 2000. Wood and Cellulosic Chemistry, Revised, and Expanded, CRC Press, Boca Raton, Florida.
19. Hopewell, J., R. Dvorak, and E. Kosior. 2009. Plastics recycling: Challenges and opportunities. Phil. Trans. R. Soc. B Biol. Sci. 364(1526):2115–2126.
20. Hosseinaei, O., S. Wang, A. A. Enayati, and T. G. Rials. 2012. Effects of hemicellulose extraction on properties of wood flour and wood–plastic composites. Compos. A Appl. Sci. Manuf. 43(4):686–694.
21. Hu, R.-H., M.-y. Sun, and J.-K. Lim. 2010. Moisture absorption, tensile strength and microstructure evolution of short jute fiber/polylactide composite in hygrothermal environment. Mater. Des. 31(7):3167–3173.
22. Joseph, P., M. S. Rabello, L. Mattoso, K. Joseph, and S. Thomas. 2002. Environmental effects on the degradation behaviour of sisal fibre-reinforced polypropylene composites. Compos. Sci. Technol. 62(10):1357–1372.
23. Karian, H. 2003. Handbook of Polypropylene and Polypropylene Composites, Revised and Expanded. CRC Press, Boca Raton, Florida.
24. Kazemi Najafi, S. 2013. Use of recycled plastics in wood–plastic composites—A review. Waste Manag. 33(9):1898–1905.
25. Kiguchi, M., Y. Kataoka, H. Matsunaga, K. Yamamoto, and P. D. Evans. 2007. Surface deterioration of wood-flour polypropylene composites by weathering trials. J. Wood Sci. 53(3):234–238.
26. Lin, P., G. Engling, and J. Yu. 2010. Humic-like substances in fresh emissions of rice straw burning and in ambient aerosols in the Pearl River Delta Region, China. Atmos. Chem. Phys. 10(14):6487–6500.
27. Lopez, J., M. Sain, and P. Cooper. 2006. Performance of natural-fiber–plastic composites under stress for outdoor applications: Effect of moisture, temperature, and ultraviolet light exposure. J. Appl. Polym. Sci. 99(5):2570–2577.
28. Lujia, H., Y. Qiaojuan, L. Xiangyang, and H. Jinyou. 2002. Straw resources and their utilization in China. Trans. Chin. Soc. Agric. Eng. 3:022.
29. Matuana, L. M., S. Jin, and N. M. Stark. 2011. Ultraviolet weathering of HDPE/wood-flour composites coextruded with a clear HDPE cap layer. Polym. Degrad. Stab. 96(1):97–106.
30. Meran, C., O. Ozturk, and M. Yuksel. 2008. Examination of the possibility of recycling and utilizing recycled polyethylene and polypropylene. Mater. Des. 29(3):701–705.
31. Michel, A. and S. Billington. 2012. Characterization of poly-hydroxybutyrate films and hemp fiber-reinforced composites exposed to accelerated weathering. Polym. Degrad. Stab. 97(6):870–878.
32. Mukhopadhyay, S. and R. Srikanta. 2008. Effect of ageing of sisal fibres on properties of sisal–polypropylene composites. Polym. Degrad. Stab. 93(11):2048–2051.
33. Peng, Y., R. Liu, J. Cao, and Y. Chen. 2014. Effects of UV weathering on surface properties of polypropylene composites reinforced with wood flour, lignin, and cellulose. Appl. Surf. Sci. 317:385–392.
34. Rajakumar, K., V. Sarasvathy, A. T. Chelvan, R. Chitra, and C. Vijayakumar. 2009. Natural weathering studies of polypropylene. J. Polym. Environ. 17(3):191–202.
35. Reddy, C. R., A. P. Sardashti, and L. C. Simon. 2010. Preparation and characterization of polypropylene–wheat straw–clay composites. Compos. Sci. Technol. 70(12):1674–1680.
36. Standardization Administration of the People's Republic of China (SAC). 2008a. Plastic—Determination of flexural properties. GB/T 9341‐2008. SAC, Beijing.
37. Standardization Administration of the People's Republic of China (SAC). 2008b. Plastic—Determination of charpy impact strength of rigid materials. GB/T 1043‐2008. SAC, Beijing.
38. Stark, N. M. and L. M. Matuana. 2003. Ultraviolet weathering of photostabilized wood-flour-filled high-density polyethylene composites. J. Appl. Polym. Sci. 90(10):2609–2617.
39. Stark, N. M. and L. M. Matuana. 2004 a. Surface chemistry and mechanical property changes of wood-flour/high-density-polyethylene composites after accelerated weathering. J. Appl. Polym. Sci. 94(6):2263–2273.
40. Stark, N. M. and L. M. Matuana. 2004 b. Surface chemistry changes of weathered HDPE/wood-flour composites studied by XPS and FTIR spectroscopy. Polym. Degrad. Stab. 86(1):1–9.
41. Stark, N. M. and L. M. Matuana. 2006. Influence of photostabilizers on wood flour–HDPE composites exposed to xenon-arc radiation with and without water spray. Polym. Degrad. Stab. 91(12):3048–3056.
42. Winandy, J. E., N. M. Stark, and C. M. Clemons. 2004. Considerations in recycling of wood–plastic composites. In:Proceedings of the 5th Global Wood and Natural Fibre Composites Symposium, April 27–28, 2004, Kassel, Germany.
43. Wypych, G. 2003. Handbook of Material Weathering. ChemTec Publishing, Ontario, Canada.
44. Xing, X. 2009. Study on the ban on free plastic bags in China. J. Sust. Dev. 2(1):P156.
45. Zhang, D., Y. Shen, and G. A. Somorjai. 1997. Studies of surface structures and compositions of polyethylene and polypropylene by IR+ visible sum frequency vibrational spectroscopy. Chem. Phys. Lett. 281(4):394–400.
46. Zhang, Y., H. Dou, B. Chang, Z. Wei, W. Qiu, S. Liu, W. Liu, and S. Tao. 2008. Emission of polycyclic aromatic hydrocarbons from indoor straw burning and emission inventory updating in China. Ann. N. Y. Acad. Sci. 1140(1):218–227.