Wafer-level SLID bonding for MEMS encapsulation
Source abstract
Abstract
Hermetic packaging is often an essential requirement to enable proper functionality throughout the device's lifetime and ensure the optimal performance of a micro electronic mechanical system (MEMS) device. Solid-liquid interdiffusion (SLID) bonding is a novel and attractive way to encapsulate MEMS devices at a wafer level. SLID bonding utilizes a low-melting-point metal to reduce the bonding process temperature; and metallic seal rings take out less of the valuable surface area and have a lower gas permeability compared to polymer or glass-based sealing materials. In addition, ductile metals can adopt mechanical and thermo-mechanical stresses during their service lifetime, which improves their reliability. In this study, the principles of Au-Sn and Cu-Sn SLID bonding are presented, which are meant to be used for wafer-level hermetic sealing of MEMS resonators. Seal rings in 15.24 cm silicon wafers were bonded at a width of 60 µm, electroplated, and used with Au-Sn and Cu-Sn layer structures. The wafer bonding temperature varied between 300 °C and 350 °C, and the bonding force was 3.5 kN under the ambient pressure, that is, it was less than 0.1 Pa. A shear test was used to compare the mechanical properties of the interconnections between both material systems. In addition, important factors pertaining to bond ring design are discussed according to their effects on the failure mechanisms. The results show that the design of metal structures can significantly affect the reliability of bond rings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Adhesion, Friction, and Surface Interactions · 3D IC and TSV technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Suhir E, Lee YC, Wong CP (2007) Micro- and optoelectronic materials and structures: physics, mechanics, design, reliability, packaging. Springer, New York10.1007/0-387-32989-7 ↗
2. Tummala RR, Swaminathan M (2008) Introduction to system-on-package: miniaturization of the entire system. McGraw-Hill, New York
3. Hartzell AL, Silva MG, Shea HR (2010) MEMS reliability. Springer, Brookline
4. Bernstein L (1966) Semiconductor joining by the solid-liquid-interdiffusion (SLID) process: I. The systems Ag-In, Au-In, and Cu-In. J Electrochem Soc 113(12):1282–128810.1149/1.2423806 ↗
5. Li JF, Agyakwa PA, Johnson CM (2010) Kinetics of Ag3Sn growth in Ag-Sn-Ag system during transient liquid phase soldering process. Acta Mater 58(9):3429–344310.1016/j.actamat.2010.02.018 ↗
6. Tollefsen TA, Larsson A, Løvvik OM et al (2012) Au-Sn SLID bonding—properties and possibilities. Metall Mater Trans B 43(2):397–40510.1007/s11663-011-9609-z ↗
7. Matijasevic GS, Lee CC, Wang CY (1993) AuSn alloy phase diagram and properties related to its use as a bonding medium. Thin Solid Films 223(2):276–28710.1016/0040-6090(93)90533-U ↗
8. Lee CL, Wang YW, Matijasevic G (1993) Advances in bonding technology for electronic packaging. J Electron Packag 115(2):201–20710.1115/1.2909318 ↗
9. Johnson WR, Wang CQ, Liu Y et al (2007) Power device packaging technologies for extreme environments. IEEE Trans Electron Packag Manuf 30(3):182–19310.1109/TEPM.2007.899158 ↗
10. Wang K, Aasmundtveit K, Jakobsen H (2008) Surface evolution and bonding properties of electroplated Au/Sn/Au. In: Electronics system-integration technology conference, Greenwich, 1–4 Sept 2008, pp 1131–113410.1109/ESTC.2008.4684511 ↗
11. Bartels F, Morris JW, Dalke G et al (1994) Intermetallic phase formation in thin solid-liquid diffusion couples. J Eletron Mater 23(8):787–79010.1007/BF02651374 ↗
12. Bosco NS, Zok FW (2005) Strength of joints produced by transient liquid phase bonding in the Cu-Sn system. Acta Mater 53(7):2019–202710.1016/j.actamat.2005.01.013 ↗
13. Agarwal R, Zhang W, Limaye P et al (2009) High density Cu-Sn TLP bonding for 3D integration. In: Electronic components and technology conference (ECTC 2009. 59th), San Diego, CA, 26–29 May 2009, pp 345–349
14. Welch W, Chae J, Lee SH et al (2005) Transient liquid phase (TLP) bonding for microsystem packaging applications. The 13th international conference on solid-state sensors, actuators and microsystems. doi: 10.1109/SENSOR.2005.149733110.1109/SENSOR.2005.1497331 ↗
15. Esashi M (2008) Wafer level packaging of MEMS. J Micromech Microeng 18(7):07300110.1088/0960-1317/18/7/073001 ↗
16. Dimcic B, Messemaeker JD, Zhang W et al (2012) Phase formation in Cu/Ni/Sn thin film systems. In: Electronics system integration technologies conference (ESTC). doi: 10.1109/ESTC.2012.654213710.1109/ESTC.2012.6542137 ↗
17. Zhang W, Dimcic B, Limaye P et al (2011) Ni/Cu/Sn bumping scheme for fine-pitch micro-bump connections. In: Electronic components and technology (ECTC), Lake Buena Vista, FL, May 31–June 3 2011, pp 109–11310.1109/ECTC.2011.5898499 ↗
18. Brem F, Liu C, Raik D (2012) Influence of Cu joining partner in transient liquid phase bonding. In: Electronics system integration technologies conference (ESTC). doi: 10.1109/ESTC.2012.654213510.1109/ESTC.2012.6542135 ↗
19. Liu H, Salomonsen G, Wang K et al (2011) Wafer-level Cu/Sn to Cu/Sn SLID-bonded interconnects with increased strength. IEEE Trans Comput Packag Manuf 1(9):1350–135810.1109/TCPMT.2011.2156793 ↗
20. Klumpp A, Merkel R, Ramm P et al (2004) Vertical system integration by using inter-chip vias and solid-liquid interdiffusion bonding. Jpn J Appl Phys 43(7A):L829–L83010.1143/JJAP.43.L829 ↗
21. Wieland R, Bonfert D, Klumpp A et al (2005) 3D integration of CMOS transistors with ICV-SLID technology. Microelectron Eng 82(3/4):529–53310.1016/j.mee.2005.07.052 ↗
22. Pouranvari M, Ekrami A, Kokabi AH (2009) Effect of bonding temperature on microstructure development during TLP bonding of a nickel base superalloy. J Alloy Compd 469(1/2):270–27510.1016/j.jallcom.2008.01.101 ↗
23. Gale WF (1999) Applying TLP bonding to the joining of structural intermetallic compounds. JOM 51(2):49–5210.1007/s11837-999-0210-8 ↗
24. Tollefsen TA, Taklo MMV, Aasmundtveit KE et al (2012) Reliable HT electronic packaging—optimization of a Au-Sn SLID joint. In: Electronics system integration technologies conference (ESTC). doi: 10.1109/ESTC.2012.654213810.1109/ESTC.2012.6542138 ↗
25. Welch WC, Najafi K (2007) Nickel-tin transient liquid phase (TLP) wafer bonding for MEMS vacuum packaging. In: Solid-state sensors, actuators and microsystems conference. doi: 10.1109/SENSOR.2007.430038510.1109/SENSOR.2007.4300385 ↗
26. Welch WC, Najafi K (2008) Gold-indium transient liquid phase (TLP) wafer bonding for MEMS vacuum packaging. In: Micro electro mechanical systems (MEMS 2008), Tucson, AZ, 13–17 Jan 2008, pp 806–809
27. Welch WC, Junseok C, Najafi K (2005) Transfer of metal MEMS packages using a wafer-level solder transfer technique. IEEE Trans Adv Packag 28(4):643–64910.1109/TADVP.2005.859356 ↗
28. Vivek C, Ho BY, Gao S (2012) Development of metallic hermetic sealing for MEMS packaging for harsh environment applications. J Eletron Mater 41(8):2256–226610.1007/s11664-012-2107-5 ↗
29. Marauska S, Claus M, Lisec T et al (2012) Low temperature transient liquid phase bonding of Au/Sn and Cu/Sn electroplated material systems for MEMS wafer-level packaging. Microsyst Technol 19(8):1119–113010.1007/s00542-012-1708-5 ↗
30. Zhou Y, Gale WF, North TH (1995) Modelling of transient liquid phase bonding. Int Mater Rev 40(5):181–19610.1179/095066095790151160 ↗
31. Okamoto H (2007) Au-Sn (gold-tin). J Phase Equilib Diffus 28(5):49010.1007/s11669-007-9147-1 ↗
32. Fürtauer S, Li D, Cupid D et al (2013) The Cu-Sn phase diagram, part I: new experimental results. Intermetallics 34:142–14710.1016/j.intermet.2012.10.004 ↗
33. Lueck MR, Reed JD, Gregory CW et al (2012) High-density large-area-array interconnects formed by low-temperature Cu/Sn-Cu bonding for three-dimensional integrated circuits. IEEE Trans Electron Dev 59(7):1941–194710.1109/TED.2012.2193404 ↗
34. MacDonald WD, Eagar TW (1992) Transient liquid phase bonding. Annu Rev Mater Sci 22:23–4610.1146/annurev.ms.22.080192.000323 ↗
35. Bader S, Gust W, Hieber H (1995) Rapid formation of intermetallic compounds interdiffusion in the Cu-Sn and Ni-Sn systems. Acta Metall Mater 43(1):329–337
36. Song JM, Shen YL, Su CW et al (2009) Strain rate dependence on nanoindentation responses of interfacial intermetallic compounds in electronic solder joints with Cu and Ag substrates. Mater Trans 50(5):1231–123410.2320/matertrans.M2009016 ↗
37. Balakrisnan B, Chum CC, Li M et al (2003) Fracture toughness of Cu-Sn intermetallic thin films. J Electron Mater 32(3):166–17110.1007/s11664-003-0188-x ↗
38. Ghosh G (2004) Elastic properties, hardness, and indentation fracture toughness of intermetallics relevant to electronic packaging. J Mater Res 19(5):1439–145410.1557/JMR.2004.0193 ↗