The promotion effect of uniaxial strain on hydrogen aggregation in tungsten
Source abstract
Abstract
The aggregation behavior of hydrogen (H) isotopes after low-energy plasma irradiation is particularly important for tungsten (W) in future fusion devices. Here, using the first-principles calculation, we demonstrated an interesting strain effect that may drive the planar aggregation of interstitial H atoms in W. Although there are attractive interactions between H atoms, the spontaneous nucleation of these platelet-like H clusters in strain-free W appears impossible even at high H concentrations (up to 0.1 at.%) because of the extremely low configurational entropy. However, applied uniaxial strain significantly increased the binding energy of H platelets and enabled planar H clusters to form. These results suggest that uniaxial strain enhances the nucleation and growth of H platelets in W, regardless of whether it is a compressive or tensile strain. Moreover, the binding energy of one-layer H clusters was lower than that of parallel H platelets, implying that the formation of multi-layer H clusters in W and their stability is also promoted by uniaxial strain. Meanwhile, the presence of planar H clusters dramatically reduced the vacancy formation energy in W, which in turn provided an extra trapping site to accommodate excessive H atoms. These results provide an important reference for understanding the H evolution in W-PFMs.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Depth distribution of deuterium in single- and polycrystalline tungsten up to depths of several micrometers10.1016/j.jnucmat.2004.10.082 ↗
2. Temperature dependence of surface morphology and deuterium retention in polycrystalline ITER-grade tungsten exposed to low-energy, high-flux D plasma10.1016/j.jnucmat.2011.11.003 ↗
3. Trapping of hydrogen and helium at dislocations in tungsten: An ab initio study10.1088/1741-4326/aa7965 ↗
4. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
5. Nucleation mechanism of intra-granular blisters in tungsten exposed to hydrogen plasma10.1016/j.scriptamat.2020.06.024 ↗
6. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
7. Handbook of surface science10.1016/S1573-4331(96)80012-6 ↗
8. Multiscale modelling of the interaction of hydrogen with interstitial defects and dislocations in BCC tungsten10.1088/1741-4326/aa8e0c ↗
9. Hydrogen diffusion and vacancies formation in tungsten: Density Functional Theory calculations and statistical models10.1016/j.actamat.2015.04.052 ↗
10. Solution and diffusion of hydrogen in tungsten10.1116/1.1492699 ↗
11. Deuterium supersaturation in low-energy plasma-loaded tungsten surfaces10.1088/0029-5515/57/1/016026 ↗
12. Hydrogen atom-ion synergy in surface lattice modification at sub-threshold energy10.1016/j.actamat.2020.09.065 ↗
13. H trapping and mobility in nanostructured tungsten grain boundaries: A combined experimental and theoretical approach10.1088/0029-5515/55/11/113009 ↗
14. Hydrogen interaction with point defects in tungsten10.1103/PhysRevB.82.094102 ↗
15. Difference in formation of hydrogen and helium clusters in tungsten10.1063/1.2103390 ↗
16. Hydrogen supersaturated layers in H/D plasma-loaded tungsten: A global model based on thermodynamics, kinetics and density functional theory data10.1103/PhysRevMaterials.2.093802 ↗
17. Stress-dependent solute energetics in W-Re alloys from first-principles calculations10.1016/j.actamat.2014.07.028 ↗
18. Hydrogen clustering in bcc metals: Atomic origin and strong stress anisotropy10.1016/j.actamat.2020.09.048 ↗
19. Hydrogen bubble nucleation by self-clustering: Density functional theory and statistical model studies using tungsten as a model system10.1088/1741-4326/aacdb6 ↗
20. Predictive model of hydrogen trapping and bubbling in nanovoids in bcc metals10.1038/s41563-019-0422-4 ↗
21. First-principles study of vacancy, interstitial, noble gas atom interstitial and vacancy clusters in bcc-W10.1016/j.commatsci.2016.06.022 ↗
22. Subsurface deuterium bubble formation in W due to low-energy high flux deuterium plasma exposure10.1088/1741-4326/57/3/034003 ↗
23. Super-saturated hydrogen effects on radiation damages in tungsten under the high-flux divertor plasma irradiation10.1088/0029-5515/55/8/083019 ↗
24. Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation. I. Theoretical background10.1016/j.actamat.2007.05.047 ↗
25. Solid solution softening and hardening by mobile solute atoms with special focus on hydrogen10.1016/j.scriptamat.2012.07.022 ↗
26. Hydrogen and helium trapping in tungsten under simultaneous irradiations10.1016/j.jnucmat.2007.01.111 ↗
27. Behaviors of transmutation elements Re and Os and their effects on energetics and clustering of vacancy and self-interstitial atoms in W10.1088/1741-4326/aa5893 ↗
28. Strain dependence of energetics and kinetics of vacancy in tungsten10.3390/ma13153375 ↗
29. Chapter 4: Power and particle control10.1088/0029-5515/47/6/s04 ↗
30. Hydrogen induced vacancy formation in tungsten10.1016/j.jnucmat.2014.02.014 ↗
31. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
32. A review of recent experiments on W and high Z materials as plasma-facing components in magnetic fusion devices10.1016/S0022-3115(97)80042-6 ↗
33. The solubility of hydrogen in molybdenum10.1016/0036-9748(72)90201-3 ↗
34. Deuterium retention in tungsten in dependence of the surface conditions10.1016/S0022-3115(02)01375-2 ↗
35. Generalized gradient approximation made simple10.1103/physrevlett.77.3865 ↗
36. Modelling deuterium release during thermal desorption of D+-irradiated tungsten10.1016/j.jnucmat.2007.09.028 ↗
37. Effect of post-D+-irradiation time delay and pre-TDS heating on D retention in single crystal tungsten10.1016/j.jnucmat.2006.07.012 ↗
38. Characterization of the energetics and configurations of hydrogen in vacancy clusters in tungsten10.1088/1741-4326/ab36a4 ↗
39. Recent analysis of key plasma wall interactions issues for ITER10.1016/j.jnucmat.2009.01.037 ↗
40. First-principles calculation on free energy of precipitate nucleation10.1016/j.calphad.2004.07.003 ↗
41. Recent findings on blistering and deuterium retention in tungsten exposed to high-fluence deuterium plasma10.1016/j.jnucmat.2008.12.129 ↗
42. Blister bursting and deuterium bursting release from tungsten exposed to high fluences of high flux and low energy deuterium plasma10.1088/0029-5515/47/3/006 ↗
43. Stress-induced hydrogen self-trapping in tungsten10.1088/1741-4326/aae2c7 ↗
44. Synergy of plastic deformation and gas retention in tungsten10.1088/0029-5515/55/1/013007 ↗
45. Effect of plastic deformation on deuterium retention and release in tungsten10.1063/1.4913478 ↗
46. Dislocations mediate hydrogen retention in tungsten10.1088/0029-5515/54/4/042004 ↗
47. Blister formation and deuterium retention on tungsten exposed to low energy and high flux deuterium plasma10.1016/j.jnucmat.2004.10.137 ↗
48. Effect of strain on solution energy of hydrogen in alpha-zirconium from first-principle calculations10.1016/j.ijhydene.2020.04.244 ↗
49. In situ observation of structural change of nanostructured tungsten during annealing10.1016/j.jnucmat.2014.02.027 ↗
50. First-principles simulation of h interacting with transition elements in molybdenum for nuclear material application10.1016/j.jnucmat.2020.152437 ↗
51. First-principles study of the effect of lattice vibrations on Cu nucleation free energy in Fe-Cu alloys10.1103/PhysRevB.72.174201 ↗
52. Surface blistering and deuterium retention behaviors in pure and ZrC-doped tungsten exposed to deuterium plasma10.1088/1741-4326/abdfda ↗
53. Anisotropic strain enhanced hydrogen solubility in bcc metals: The independence on the sign of strain10.1103/PhysRevLett.109.135502 ↗
54. Deuterium trapping and surface modification of polycrystalline tungsten exposed to a high-flux plasma at high fluences10.1088/1741-4326/aa5898 ↗