Abstract

Waste dolomite powder (WDP) is being actively investigated as the additive of Portland cement (PC) for lowering the energy consumption and carbon emission of PC. In this work, 1H low-field nuclear magnetic resonance (1H NMR) was used to analyze the impacts of WDP on the hydration and pore structure of PC pastes at the early age. Meanwhile, the compressive strengths of blended cements containing 5–20% WDP were also measured. The results show that the T2 average value and evaporable water content of all the pastes decrease dramatically from 0 to 24 h, and the reduction rate slows down after 24 h. Adding 5% WDP can decrease further the T2 average value and evaporable water content attributed to its nucleating and filler effect, resulting in the compacted pore structure and the higher strength. However, adding more than 5% WDP degrades the pore structure and lowers the compressive strength.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Innovative concrete reinforcement materials · Recycled Aggregate Concrete Performance

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechanics and Engineering Science, Shanghai University, Shanghai, PR China

School of Civil Engineering, Suzhou University of Science and Technology, Suzhou, PR China

Suzhou Niumag Analytical Instrument Corporation, Suzhou, PR China

Suzhou Testniumag Corporation Co. Ltd, Suzhou, PR China

References (34)

Show source-provided references
1. 10.1016/j.jclepro.2022.13349210.1016/j.jclepro.2022.133492 ↗
2. 10.1016/j.jclepro.2020.12355810.1016/j.jclepro.2020.123558 ↗
3. 10.1016/j.cemconres.2010.12.00110.1016/j.cemconres.2010.12.001 ↗
4. 10.1016/j.jclepro.2015.12.11510.1016/j.jclepro.2015.12.115 ↗
5. 10.1016/j.cemconres.2019.05.00810.1016/j.cemconres.2019.05.008 ↗
6. Chen D. · Rev. Rom. Mater. · 2021 · 51 · 116
7. 10.1016/j.jhazmat.2018.03.06310.1016/j.jhazmat.2018.03.063 ↗
8. 10.1617/s11527-007-9284-310.1617/s11527-007-9284-3 ↗
9. 10.1016/j.conbuildmat.2007.03.00610.1016/j.conbuildmat.2007.03.006 ↗
10. 10.1016/j.cemconres.2011.03.01910.1016/j.cemconres.2011.03.019 ↗
11. 10.1016/j.conbuildmat.2011.03.01810.1016/j.conbuildmat.2011.03.018 ↗
12. Chen D. · Rev. Rom. Mater. · 2021 · 51 · 395
13. 10.1016/j.conbuildmat.2017.11.14810.1016/j.conbuildmat.2017.11.148 ↗
14. 10.1016/j.conbuildmat.2022.12894210.1016/j.conbuildmat.2022.128942 ↗
15. 10.1016/j.conbuildmat.2021.12394810.1016/j.conbuildmat.2021.123948 ↗
16. 10.1016/j.cemconres.2014.07.00210.1016/j.cemconres.2014.07.002 ↗
17. 10.1016/j.conbuildmat.2020.12137510.1016/j.conbuildmat.2020.121375 ↗
18. 10.14062/j.issn.0454-5648.2017.02.1410.14062/j.issn.0454-5648.2017.02.14 ↗
19. 10.1016/j.jmro.2021.10001210.1016/j.jmro.2021.100012 ↗
20. 10.1016/j.conbuildmat.2022.12898810.1016/j.conbuildmat.2022.128988 ↗
21. 10.1016/j.cemconres.2020.10632910.1016/j.cemconres.2020.106329 ↗
22. 10.1016/j.conbuildmat.2020.12158310.1016/j.conbuildmat.2020.121583 ↗
23. Chen D. · Rev. Rom. Mater. · 2022 · 52 · 203
24. 10.1016/j.conbuildmat.2020.11878810.1016/j.conbuildmat.2020.118788 ↗
25. 10.1016/j.conbuildmat.2021.12463110.1016/j.conbuildmat.2021.124631 ↗
26. 10.1016/j.cemconres.2015.04.00510.1016/j.cemconres.2015.04.005 ↗
27. 10.1080/1536383X.2021.191755410.1080/1536383X.2021.1917554 ↗
28. 10.1016/j.cemconres.2017.11.00110.1016/j.cemconres.2017.11.001 ↗
29. 10.1016/j.cemconres.2017.02.02710.1016/j.cemconres.2017.02.027 ↗
30. Chinese Standards GB/T 17671-1999 · 1999
31. 10.1016/j.apsusc.2022.15571310.1016/j.apsusc.2022.155713 ↗
32. Mehta P. K. · 2006
33. 10.1080/1536383X.2022.203536310.1080/1536383X.2022.2035363 ↗
34. 10.1080/1536383X.2022.208168410.1080/1536383X.2022.2081684 ↗