Abstract
The electrical properties of a (Ba[Formula: see text]SrxCay)TiO3-based positive temperature coefficient (PTC) thermistor were determined by measuring resistivity with increasing temperature, and its thermal properties were measured with a cartridge heater made of a (Ba[Formula: see text]Sr[Formula: see text]Ca[Formula: see text])TiO3-based PTC thermistor. The (Ba[Formula: see text]SrxCay)TiO3-based PTC thermistor were fabricated by a conventional solid-state reaction method with Sb2O3, BaTiO3, SrTiO3, SiO2, and CaTiO3. Their electrical properties were determined by room temperature resistivity ([Formula: see text]C), minimum resistivity ([Formula: see text]), maximum resistivity ([Formula: see text]), resistivity jump rate (log [Formula: see text]/[Formula: see text]), Curie temperature ([Formula: see text]), and withstanding voltage. The effect of the microstructure on the electrical properties was investigated to improve the withstand voltage. The cartridge heater was fabricated with the (Ba[Formula: see text]Sr[Formula: see text]Ca[Formula: see text])TiO3-based PTC thermistor and its thermal properties were determined by the temperature of light oil in a 100 cc beaker. The temperature of light oil was maintained at 60[Formula: see text]C without fluctuations in temperature after reaching 60[Formula: see text]C at 220[Formula: see text]V, and thus (Ba[Formula: see text]SrxCay)TiO3-based PTC thermistor was able to operate as a self-regulating heater element for preheating light oil.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Electrical and Thermal Properties of Materials · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Separation and Conversion Materials Laboratory, Korea Institute of Energy and Research, 152, Gajeong-ro, Yuseong-gu, Dajeon 34129, The Republic of Korea
References (24)
Show source-provided references
1. Kurian R. M. · IRJET · 2015 · 2 · 581
2. 10.1038/156717a010.1038/156717a0 ↗
3. Jaffe B. · 1971
4. Andrich E. · Electron. Appl. · 1965 · 26 · 123
5. 10.1143/JJAP.34.530910.1143/JJAP.34.5309 ↗
6. 10.1016/S0955-2219(99)00010-210.1016/S0955-2219(99)00010-2 ↗
7. 10.1109/TIA.1972.34976510.1109/TIA.1972.349765 ↗
8. Humphrey T. · IJVD. · 1985 · 6 · 469
9. Meier K. · Appliance · 2001 · 58 · 64
10. Musta R. · IFIP AICT · 2010 · 314 · 461
11. 10.20965/ijat.2014.p072310.20965/ijat.2014.p0723 ↗
12. Kim J. · HT-HP · 2016 · 45 · 451
13. 10.1143/JJAP.18.73510.1143/JJAP.18.735 ↗
14. Niwa N. · JSAE Rev · 1985 · 95
15. Matuo Y. · Ceram. Bull. · 1968 · 47 · 292
16. Eastman C. · Proc. British Ceram. Soc. · 1970 · 18 · 77
17. 10.1111/j.1151-2916.1971.tb12391.x10.1111/j.1151-2916.1971.tb12391.x ↗
18. 10.1111/j.1151-2916.1976.tb09430.x10.1111/j.1151-2916.1976.tb09430.x ↗
19. 10.1143/JJAP.18.73510.1143/JJAP.18.735 ↗
20. Howng W. Y. · Ceram. Bull. · 1983 · 62 · 231
21. 10.1016/S0955-2219(00)00061-310.1016/S0955-2219(00)00061-3 ↗
22. 10.1016/j.jeurceramsoc.2005.03.17810.1016/j.jeurceramsoc.2005.03.178 ↗
23. Huang M. · Adv. Mat. Res. · 2013 · 760 · 767
24. 10.1179/1743676111Y.000000000110.1179/1743676111Y.0000000001 ↗