Abstract

The effect of ageing at 85°C of extrusion welds of 1.5 mm-thick high-density polyethylene (HDPE) geomembrane, immersed in synthetic municipal solid waste leachate, is investigated with respect to its standard oxidative induction time (Std-OIT) and stress crack resistance (SCR). Results show that the heat-affected zones (HAZ) adjacent to the squeeze-out bead (flashing) may exhibit faster STD-OIT depletion than the sheet. Generally, individual weld SCR failure times were observed to be between that of the notched and unnotched sheet. Welds with high welding-induced geometric irregularities (WIGI), and overheated fusion and extrusion welds are shown to result in SCR failure times close to that of a notched sheet. The average time to nominal failure (taken to be when tNF = 250 h) of Cool and Good welding parameter combinations ranges between 3% and 15% shorter than the unnotched sheet. Differences in tNF were attributed to accelerated craze formation in welds with high WIGI from stress concentration. No significant difference was observed between the SCR values of fusion and extrusion welds during 40 months of immersion in MSW-L3. This paper shows that overgrind negatively impacts the SCR of welds and accelerates the degradation of SCR.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Landfill Environmental Impact Studies · Geotechnical Engineering and Soil Stabilization · High voltage insulation and dielectric phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

1 PhD student, GeoEngineering Centre at Queen's – RMC, Department of Civil Engineering, Queen's University, Kingston, Canada, E-mail: 18ma111@queensu.ca

2 Barrington Batchelor Distinguished University Professor and Canada Research Chair in Geotechnical and Geoenvironmental Engineering, GeoEngineering Centre at Queen's – RMC, Department of Civil Engineering, Queen's University, Kingston, Canada, E-mail: kerry.rowe@queensu.ca (corresponding author)

References (48)

Show source-provided references
1. Durability of three HDPE geomembranes immersed in different fluids at 85°C10.1061/(ASCE)GT.1943-5606.0001234 ↗
2. Brittle rupture of an aged HPDE geomembrane at local gravel indentations under simulated field conditions10.1680/gein.13.00031 ↗
3. Effect of leachate composition on the long-term performance of a HDPE geomembrane10.1016/j.geotexmem.2014.06.001 ↗
4. Long-term performance of a HDPE geomembrane stabilized with HALS in chlorinated water10.1016/j.geotexmem.2019.103497 ↗
5. Effect of aged geomembrane extrusion welding on antioxidant depletion. Geosynthetics: Leading the Way to a Resilient Planet
6. ASTM D1238-23
7. ASTM D3895-19
8. ASTM D5199-01
9. ASTM D5397-20
10. ASTM D5885-20
11. ASTM D6392-23
12. ASTM D6693-20
13. A comparison of geomembrane wrinkles for nine field cases10.1680/gein.12.00030 ↗
14. TCE and PCE diffusion through five geomembranes including two coextruded with an EVOH layer10.1016/j.geotexmem.2020.03.010 ↗
15. Effect of aging on the stress crack resistance of an HDPE geomembrane10.1016/j.polymdegradstab.2014.06.013 ↗
16. Degradation behaviour of HDPE geomembranes with high and low initial high-pressure oxidative induction time10.1016/j.geotexmem.2014.01.004 ↗
17. Long-term stress crack resistance of HDPE fusion seams aged at 85°c in synthetic leachate10.1139/cgj-2022-0159 ↗
18. Stress crack resistance of unaged high-density polyethylene geomembrane fusion seams10.1680/jgein.21.00027a ↗
19. Importance of thickness reduction and squeeze-out Std-OIT loss for HDPE geomembrane fusion seams10.1016/j.geotexmem.2022.09.003 ↗
20. A quantification of the short-term reliability of HDPE geomembrane seaming methods10.1680/jgein.21.00041 ↗
21. Analysis of strain concentration next to geomembrane seams10.1680/gein.2.0046 ↗
22. GRI-GM5 · 1992
23. Data base of field incidents used to establish HDPE geomembrane stress crack resistance specifications10.1016/S0266-1144(99)00018-7 ↗
24. Antioxidant depletion lifetime in high density polyethylene geomembranes10.1061/(ASCE)1090-0241(1998)124:6(532) ↗
25. Experimental evaluation of HDPE geomembrane seam strain concentrations10.1680/jgein.17.00005 ↗
26. Geomembrane landfill liners in the real world, Geological Society, London10.1144/GSL.ENG.1996.011.01.23 ↗
27. Effect of texturing on the longevity of high-density polyethylene (HDPE) geomembranes in municipal solid waste landfills10.1139/cgj-2019-0047 ↗
28. Brittle-fracture in polyethylene geomembranes
29. Effect of welding parameters on properties of HDPE geomembrane extrusion welds10.1016/j.geotexmem.2023.12.002 ↗
30. Impact on landfill liner time-temperature history on the service-life of HDPE geomembranes10.1016/j.wasman.2009.05.010 ↗
31. Durability of HDPE geomembranes10.1016/S0266-1144(02)00005-5 ↗
32. Long-term performance of high-density polyethylene (HDPE) geomembrane seams in municipal solid waste (MSW) leachate10.1139/cgj-2017-0049 ↗
33. Durability of HDPE geomembrane seams immersed in brine for three years10.1680/jgein.17.00018 ↗
34. Magnitude and significance of tensile strains in geomembrane landfill liners10.1016/j.geotexmem.2019.01.001 ↗
35. Composite liner for a lagoon after 14 years of use
36. Leachate chemical composition effects on OIT depletion in an HDPE geomembrane10.1680/gein.2008.15.2.136 ↗
37. Ageing of HDPE geomembrane exposed to air, water and leachate at different temperatures10.1016/j.geotexmem.2008.09.007 ↗
38. Effect of thickness on the ageing of HDPE geomembranes10.1061/(ASCE)GT.1943-5606.0000207 ↗
39. Antioxidant depletion from an HDPE geomembrane under simulated landfill conditions10.1061/(ASCE)GT.1943-5606.0000302 ↗
40. Representative stress crack resistance of polyolefin geomembranes used in waste management10.1016/j.wasman.2019.08.028 ↗
41. Effect of surface fluorination on diffusion through an HDPE geomembrane10.1061/(ASCE)1090-0241(2005)131:6(694) ↗
42. Scheirs · 200910.1002/9780470748213 ↗
43. Seeger · 2003 · 137
44. Quantifying geomembrane wrinkles using aerial photography and digital image processing10.1680/gein.2007.14.4.219 ↗
45. Extrusion seams – the good, the bad, and the ugly
46. Geomembrane strain observed in large-scale testing of protection layers10.1061/(ASCE)1090-0241(2000)126:12(1194) ↗
47. Geoenvironmental applications of geosynthetics, Keynote Lecture
48. Effect of welding parameters on properties of HDPE geomembrane seams10.1680/jgein.17.00011 ↗