Silicon nitridation at different nitrogen pressures
Source abstract
Abstract
The mass change of silicon samples with different initial density, apparent density, ultimate strength and phase composition during nitridation in the nitrogen pressure range 0.002 – 18 MPa is followed. It is shown that rate of the reaction of nitrogen and silicon increases up to nitrogen pressure 1.5 MPa; at higher nitrogen pressures the growth of the reaction rate slows down. Ceramic with relative density 90% and ultimate bending strength 540 MPa was obtained at kilning temperature 1710°C. Ceramic parts serviceable under the actual operating conditions of a real motor have been fabricated for internal combustion engines.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Material Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (4)
Show source-provided references
1. E. A. Anikin, V. I. Snop, I. Ya. Guzman, and E. B. Bendovskii, “Inventor’s Certificate No. 1344516,” Byul. Izobr. Polez. Modeli, No. 38 (1987).
2. R. A. Andrievskii and I. I. Spivak, Silicon Nitride and Materials Based on It [in Russian], Metallurgiya, Moscow (1984).
3. I. Ya. Guzman, Reactive Sintering and Its Use in Ceramics and Refractories Technology, Teaching Notes [in Russian], RKhTU im. D. I. Mendeleeva, Moscow (1996).
4. E. B. Bendovskii and I. Ya. Guzman, “Particulars of silicon nitridation,” Steklo Keram., No. 11, 22 – 26 (2003); E. B. Bendovskii and I. Ya. Guzman, “Specifics of silicon nitration,” Glass Ceram., 63(11 – 12), 374–378 (2003).