journal article·2014-09

Effect of Si/Al ratio on engineering properties of alkali-activated GGBS pastes

Mohammed Nadeem Qureshi, Somnath Ghosh

Green Materials· Volume 2· Issue 3
Publisher page

Abstract

The effect of synthesis parameter, silicon/aluminum molar ratio, on the engineering properties of alkali-activated blast-furnace paste has been investigated. The article presents the study of the compressive strength and microstructure of alkali-activated blast-furnace slag paste specimens prepared using sodium silicate and potassium hydroxide solution as activators. The experimental results have indicated that the compressive strength, bulk density, apparent porosity, water absorption and microstructure of the specimens are significantly affected by the silicon/aluminum molar ratio of alkali-activated ground granulated blast-furnace slag (AAS) paste. The compressive strength at 28 d of 44·90–46·30 MPa was obtained for silicon/aluminum ratios of 2·03–2·26. Increasing silicon/aluminum ratio beyond 2·26 resulted in a decrease in compressive strength of AAS paste due to delayed precipitation of calcium silicate hydrate products. The microstructural changes of hardened AAS paste were studied using scanning electron microscopy/energy-dispersive X-ray spectroscopy, and mineralogical characterization was studied with X-ray diffraction and Fourier transform infrared spectroscopy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Recycling and utilization of industrial and municipal waste in materials production · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Senior Lecturer, Government Polytechnic, Khamgaon, Maharashtra, India

Research Scholar, Department of Civil Engineering, Jadavpur University, Kolkata, India

Professor, Department of Civil Engineering, Jadavpur University, Kolkata, India

References (33)

Show source-provided references
1. Davidovits J. · World Resource Review · 1994 · 6 · 263
2. 10.1680/coma.2007.160.3.9910.1680/coma.2007.160.3.99 ↗
3. Mehta P. K. · 1989 · 1
4. ACI Committee 233. Ground Granulated Blast Furnace Slag as a Cementitious Constituent in Concrete, 2000, American Concrete Institute, Michigan, 1–18, ACI Manual of Concrete Practice, 233R-95.
5. 10.1016/0008-8846(94)90026-410.1016/0008-8846(94)90026-4 ↗
6. 10.1016/S0008-8846(98)00170-710.1016/S0008-8846(98)00170-7 ↗
7. 10.1016/j.conbuildmat.2007.10.01210.1016/j.conbuildmat.2007.10.012 ↗
8. 10.1016/S0008-8846(01)00717-710.1016/S0008-8846(01)00717-7 ↗
9. 10.1016/j.cemconres.2011.08.00510.1016/j.cemconres.2011.08.005 ↗
10. 10.1680/adcr.2000.12.4.16310.1680/adcr.2000.12.4.163 ↗
11. 10.1680/adcr.2000.12.2.6510.1680/adcr.2000.12.2.65 ↗
12. 10.1680/coma.10.0001610.1680/coma.10.00016 ↗
13. Qureshi M. N. · International Journal of Engineering and Science Invention · 2013 · 2 · 24
14. 10.1680/adcr.2005.17.4.16110.1680/adcr.2005.17.4.161 ↗
15. Qureshi M. N. · International Journal of Applied Engineering Research · 2013 · 8 · 141
16. 10.1680/adcr.2006.18.3.11910.1680/adcr.2006.18.3.119 ↗
17. 10.1007/s10853-012-6353-y10.1007/s10853-012-6353-y ↗
18. Qureshi M. N. · Global Journal of Researches in Engineering · 2013 · 13 · 11
19. ASTM Standards · 2007
20. ASTM Standards · 2008
21. 10.1520/ACEM2012002910.1520/ACEM20120029 ↗
22. ASTM Standards · 2002
23. Qureshi M. N. · The Arabian Journal for Science and Engineering
24. 10.4324/978020339067210.4324/9780203390672 ↗
25. 10.1016/j.conbuildmat.2009.02.02210.1016/j.conbuildmat.2009.02.022 ↗
26. Astutiningsih S. · 2005 · 69
27. 10.1016/S0022-3093(99)00555-410.1016/S0022-3093(99)00555-4 ↗
28. 10.1021/es00018a02410.1021/es00018a024 ↗
29. Allahverdi A. · Ceramics Silikaty · 2011 · 55 · 68
30. Najafikani E. · Ceramics Silikaty · 2009 · 53 · 195
31. Soleimani M. A. · Ceramics Silikaty · 2013 · 57 · 33
32. 10.1016/S0008-8846(03)00254-010.1016/S0008-8846(03)00254-0 ↗
33. Wu Z. · 2004