Growth Directions of Primary Phases in Directionally Solidified Ti-45Al-7Nb Alloys
Source abstract
Abstract
Abstract Ti-45Al-7Nb alloys are produced by liquid-metal-cooling (LMC) directional solidification (DS) furnace with different temperature gradients (G) at a range of 40–80 K/cm. The growth directions of primary β phases and the deflection angles relative to the 〈100〉 β direction were investigated. The solidification pathway of alloy is: Liq. → Liq. + β → β → β + α → α + γ → lamella (α 2 + γ) + B2. Primary dendrite arm spacing λ reduced from 611.4 µm to 508.7 µm when G increased from 40 K cm −1 to 80 K cm −1 . Grains with lamellar orientation aligned at the angles of 12–15° and 55° to growth direction were favored for various G. The orientations of the γ lamellas in steady-state regions were identified by the electron backscattered diffraction analysis (EBSD). The results indicated that the growth directions of primary bcc-β dendrites were 〈211〉 β and 〈110〉 β at 40 K/cm, 〈210〉 β and 〈211〉 β at 50 K/cm and 〈211〉 β at 80 K/cm, the deflection angle of 〈211〉 β relative to 〈100〉 β direction is 35.3°.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Metallic Glasses and Amorphous Alloys · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Aerospace Advanced Materials and Performance of Ministry of Education, School of Materials Science and Engineering, Beihang University, Beijing, 100191
References
Reference metadata was not supplied for this record.