Micromorphology change and microstructure of Cu-P based amorphous filler during heating process

XiangPing Xu, QiuJie Ma, ChunZhi Xia

Abstract

Abstract The changes that occur in the microstructure of crystalline and amorphous Cu-P-Sn-Ni filler metals during the heating process were studied by high-temperature microscopy, and the composition of solders at certain temperatures were analyzed by scanning electron microscopy and X-ray diffraction. The amorphous solder was observed to transform from amorphic to crystalline during the process of heating and distinct surface morphology changes were apparent, while the internal structure of the crystalline brazing filler metal was found to be relatively stable. During the heating process, the amorphous brazing filler metal formed a ϒ -Cu solid solution with a small amount of Cu 3 P compounds, Cu 88 Sn 22 and (Cu, Ni) 3 P phase compounds, ultimately forming the Cu 88 Sn 22 + Ni 12 P 5 + (Cu, Ni) 3 P 3 three-element eutectic structure.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Electronic Packaging and Soldering Technologies · Electrical and Thermal Properties of Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Provincial Key Lab of Advanced Welding Technology, Jiangsu University of Science and Technology , Zhenjiang 212003 , China

References (18)

Show source-provided references
1. L. Tian, W. H. Li, M.X. Chen, and B. Fang, Hot Work Technol., 15 (2015) 158-161.
2. C.Z. Xia, J. Yang, X.P. Xu, and J.S. Zou, High Temp Mater.Process., 36 (2017) 477-483.10.1515/htmp-2015-0258 ↗
3. A. G. Tiagunov, V. S. Tsepelev, and G. V. Tiagunov, Mater. Sci. Forum., 870 (2016) 108-213.10.4028/www.scientific.net/MSF.870.26 ↗
4. F. Wang, S. Yin, and Z. Wang, Spec. Cast. Nonferrous Alloys., 2 (2015) 335-340.
5. C.Z. Xia, W.W. Sun, and M.J. Zhao, Mater. Process. Technol., 259 (2018) 15-22.10.1016/j.jmatprotec.2018.04.01810.1016/j.jmatprotec.2018.04.018 ↗
6. A.A. Ivannikov, V.T. Fedotov, O.N. Sevryukov, B.A. Kalin, A.N. Suchkov, I.S. Logvenchev, et al., Weld.Int., 27 (2013) 660-664.10.1080/09507116.2012.75327110.1080/09507116.2012.753271 ↗
7. C. Peng, Y.D. Yuan, and W.H. Li, Hot.Work.Technol., 21 (2016) 162-165.
8. P.I. Burak, A.V. Serov, and R.A. Latypov, Weld. Int., 26 (2012) 1-5.10.1080/09507116.2011.58135010.1080/09507116.2011.653168 ↗
9. W.Y. Yu, X.D. Chen,W.J. Lu, Rare Met.Mater. Eng., 38 (2009) 1627-1629.
10. C.Z. Xia,W.W. Sun, Y.J. Zhou, and X. Xu, Alloys Compd., 741 (2018) 155-160.10.1016/j.jallcom.2018.01.15110.1016/j.jallcom.2018.01.151 ↗
11. Y.H. Liu, J.D. Hu, P. Shen, X.H. Han, and J.C. Li, Mater. Des., 47 (2013) 281-286.10.1016/j.matdes.2012.12.02310.1016/j.matdes.2012.12.023 ↗
12. O.N. Sevryukov, A.N. Suchkov, and E.V. Guseva, Non-Ferrous Met., 1 (2015) 45-49.
13. R.W. Hua, H.W. Zuo, and J.S. Zou, Weld.Technol., 40 (2011) 9-12.
14. X.Z. Wang, Steel Res., 04 (1991) 86-92.
15. A. Rabinkin, E. Wenski, and A. Ribaudo, Weld. J., 77 (1998) 66-75.
16. X.P. Xu, Q.M. Liu, C.Z. Xia, and J.S. Zou, High Temp Mater. Process., 37(6) (2018) 597-602.10.1515/htmp-2016-018310.1515/htmp-2016-0183 ↗
17. P. He, J.H. Zhang, R.L. Zhou, X.Q. Li, Mater. Charact.. 43(5) (1999) 289-292.10.1016/S1044-5803(99)00008-X ↗
18. W.Y. Yu, X.D. Chen, W.L. Lu, Rare Metal Mat Eng., 38(9) (2009) 1626- 1629.