Nanoarchitectured Co–Cr–Mo orthopedic implant alloys: Nitrogen-enhanced nanostructural evolution and its effect on phase stability
Source abstract
Abstract
Our previous studies indicate that nitrogen addition suppresses the athermal γ (face-centered cubic, fcc)→ε (hexagonal close-packed, hcp) martensitic transformation of biomedical Co-Cr-Mo alloys and ultimately offers large elongation to failure while maintaining high strength. In the present study, structural evolution and dislocation slip as an elementary process in the martensitic transformation in Co-Cr-Mo alloys were investigated to reveal the origin of their enhanced γ phase stability due to nitrogen addition. Alloy specimens with and without nitrogen addition were prepared. The N-doped alloys had a single-phase γ matrix, whereas the N-free alloys had a γ/ε duplex microstructure. Irrespective of the nitrogen content, dislocations frequently dissociated into Shockley partial dislocations with stacking faults. This indicates that nitrogen has little effect on the stability of the γ phase, which is also predicted by thermodynamic calculations. We discovered short-range ordering (SRO) or nanoscale Cr2N precipitates in the γ matrix of the N-containing alloy specimens, and it was revealed that both SRO and nanoprecipitates function as obstacles to the glide of partial dislocations and consequently significantly affect the kinetics of the γ→ε martensitic transformation. Since the formation of ε martensite plays a crucial role in plastic deformation and wear behavior, the developed nanostructural modification associated with nitrogen addition must be a promising strategy for highly durable orthopedic implants.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Recent metallic materials for biomedical applications10.1007/s11661-002-0109-2 ↗
2. Review of wear mechanisms in hip implants: I – General10.1016/j.matdes.2003.11.010 ↗
3. Pin-on-disk wear behavior in a like-on-like configuration in a biological environment of high carbon cast and low carbon forged Co–29Cr–6Mo alloys10.1016/j.actamat.2006.10.005 ↗
4. Microstructural effects on the wear resistance of wrought and as-cast Co–Cr–Mo–C implant alloys10.1002/jbm.a.30392 ↗
5. Influence of metal carbides on dissolution behavior of biomedical CoCrMo alloy: SEM, TEM and AFM studies10.1016/j.electacta.2011.08.028 ↗
6. New insights into hard phases of CoCrMo metal-on-metal hip replacements10.1016/j.jmbbm.2012.03.013 ↗
7. Deformation mode in biomedical Co–27% Cr–5% Mo alloy consisting of a single hexagonal close-packed structure10.1016/j.scriptamat.2010.08.006 ↗
8. Ultrafine grain refinement of biomedical Co–29Cr–6Mo alloy during conventional hot-compression deformation10.1007/s11661-009-9879-0 ↗
9. Origin of significant grain refinement of biomedical Co–29Cr–6Mo alloy without severe plastic deformation10.1007/s11661-012-1303-5 ↗
10. Mechanical properties of as-forged Ni-free Co–29Cr–6Mo alloys with ultrafine-grained microstructure10.1016/j.msea.2011.04.027 ↗
11. Enhanced mechanical properties of as-forged Co–Cr–Mo–N alloys with ultrafine-grained structures10.1007/s11661-012-1288-0 ↗
12. Evolution of cold-rolled microstructures of biomedical Co–Cr–Mo alloys with and without N doping10.1016/j.msea.2010.09.002 ↗
13. Microstructures and mechanical properties of biomedical Co–Cr–Mo alloys processed by hot rolling10.1007/s11661-012-1156-y ↗
14. Significant improvement in mechanical properties of biomedical Co–Cr–Mo alloys with a combination of N addition and Cr enrichment10.2320/matertrans.MRA2007220 ↗
15. Effect of nitrogen on the microstructure and mechanical properties of a Co–Cr–Mo alloy10.1016/S0261-3069(96)00036-2 ↗
16. Wear properties of Co–Cr–Mo–N plasma-melted surgical implant alloys10.1016/S0924-0136(03)00077-3 ↗
17. The effects of nitrogen additions to a cobalt-chromium surgical implant alloy, Part 1: Processing and microstructure10.1007/BF01160770 ↗
18. Deformation behavior of low-carbon Co–Cr–Mo alloys for low-friction implant applications10.1002/(SICI)1097-4636(199607)31:3<409::AID-JBM16>3.0.CO;2-D ↗
19. Mani A, Salinas-Rodriguez, López HF. Deformation induced FCC to HCP transformation in a Co–27Cr–5Mo–0.05C alloy. Mater Sci Eng A 2011;528:3037–3043.10.1016/j.msea.2010.12.024 ↗
20. Isothermal phase transformation in biomedical Co–29Cr–6Mo alloy without addition of carbon or nitrogen10.1007/s11661-010-0273-8 ↗
21. High work-hardening rate and deformation twinning of Co–Ni-based superalloy at elevated temperatures10.1080/01418619908210378 ↗
22. Nickel essentiality, toxicity, and carcinogenicity10.1016/S1040-8428(01)00214-1 ↗
23. Characterization of air-formed surface oxide film on a Co–Ni–Cr–Mo alloy (MP35N) and its change in Hanks’ solution10.1016/j.apsusc.2012.02.057 ↗
24. Fatigue and life prediction for cobalt–chromium stents: a fracture mechanics analysis10.1016/j.biomaterials.2005.10.012 ↗
25. Role of nitrogen addition in stabilizing the γ phase of Co–29Cr–6Mo alloy10.1016/j.matchemphys.2011.12.081 ↗
26. Change in the electron structure caused by C, N and H atoms in iron and its effect on their interaction with dislocations10.1016/j.actamat.2005.07.028 ↗
27. On the correlation between electron structure and short range atomic order in iron-based alloys10.1016/S1359-6454(00)00192-0 ↗
28. X-ray absorption fine structure analysis of interstitial (C, N)–substitutional (Cr) complexes in austenitic stainless steels10.2355/isijinternational.30.625 ↗
29. Nadutov VM, Bulavin LA, Garamus VM. Analysis of small-angle neutron scattering from Fe–18Cr–10Mn–16Ni–0.5N and Fe–21Cr–10Mn–17Ni–0.5C austenites. Mater Sci Eng A 1999;264:286–290.10.1016/S0921-5093(98)01101-0 ↗
30. The combined effect of molybdenum and nitrogen on the fatigued microstructure of 316 type austenitic stainless steel10.1016/S1359-6462(99)00194-3 ↗
31. Work hardening mechanism in high nitrogen austenitic steel studied byin situneutron diffraction andin situelectron backscattering diffraction10.1016/j.msea.2009.07.066 ↗
32. Microstructural evolution of Cr–Mn–N austenitic steels during cold work hardening10.1016/j.msea.2006.04.020 ↗
33. Electron microscopic study of Cr2N formation in thermally aged 316LN austenitic stainless steels10.1007/BF02649856 ↗
34. Nitrogen strengthening of a stable austenitic stainless steel10.1016/0001-6160(87)90131-3 ↗
35. Effect of nitrogen addition on strain rate dependence of flow stress in austenitic stainless steels10.2320/jinstmet.69.867 ↗
36. Work-hardening behaviour of nitrogen-alloyed austenitic stainless steels10.1016/0921-5093(91)90655-7 ↗
37. Unusual strainrate dependence of low temperature fracture behavior in high nitrogen bearing austenitic steels10.1016/S1359-6454(98)00005-6 ↗
38. Formation of shear bands and strain-induced martensite during plastic deformation of metastable austenitic stainless steels10.1016/j.actamat.2007.07.015 ↗
39. Hardening due to pre-existing ε-martensite in an Fe–30Mn–1Si alloy single crystal10.1016/0001-6160(82)90030-X ↗
40. On the crystal structure of Cr2N precipitates in high-nitrogen austenitic stainless steel10.1107/S0108768104033919 ↗
41. Fultz · 2009
42. Grain refinement of biomedical Co–27Cr–5Mo–0.16N alloy by reverse transformation10.1016/j.matlet.2009.10.001 ↗
43. Odahara T, Matsumoto H, Chiba A. Mechanical properties of biomedical Co–33Cr–5Mo–0.3N alloy at elevated temperatures. Mater Trans 2008;49:1963–1969.10.2320/matertrans.MAW200816 ↗
44. Thermally-activated deformation of BCC metals and alloys10.1016/0079-6425(92)90004-Q ↗
45. Enhanced solid solution effects on the strength of nanocrystalline alloys10.1016/j.actamat.2010.11.026 ↗
46. Suzuki T. In: Rosenfield AR, Hahn GT, Bement Jr AL, Jaffee RI, editors. Dislocation dynamics. New York: McGraw-Hill Book Company; 1968.
47. Nano-sized twins induce high rate sensitivity of flow stress in pure copper10.1016/j.actamat.2005.01.031 ↗
48. Grain size dependence of the plastic deformation kinetics in Cu10.1016/S0921-5093(02)00238-1 ↗
49. Effect of nanocrystalline and ultrafine grain sizes on the strain rate sensitivity and activation volume: fcc versus bcc metals10.1016/j.msea.2004.03.064 ↗
50. Influence of stacking fault energy and short-range ordering on dynamic recovery and work hardening behavior of copper alloys10.1016/j.scriptamat.2010.01.031 ↗
51. Dynamic strain aging in biomedical Co–Cr–Mo alloys with nitrogen addition10.4028/www.scientific.net/KEM.508.141 ↗
52. Nitrogen-induced dynamic strain aging in a biomedical-grade Co–Cr–Mo alloy10.1016/j.msea.2012.05.003 ↗
53. Olson GB, Cohen M. A general mechanism of martensitic nucleation: Part 1. General concepts and the FCC→HCP transformation. Metall Trans A 1976;7A:1897–1904.10.1007/BF02659822 ↗
54. Allain A, Chateau JP, Bouaziz O, Migot S, Guelton N. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys. Mater Sci Eng A 2004;387–389:158–162.10.1016/j.msea.2004.01.059 ↗
55. Effect of nitrogen on generalized stacking fault energy and stacking fault widths in high nitrogen steels10.1016/j.actamat.2006.02.048 ↗