journal article·2014-04

The influence of magnetic heat treatment on morphology, structure, magnetic properties of Fe-Co-P alloy films

Jinwu Wei, Erxi Feng, Liang Hao, Derang Cao, Jianbo Wang, Qingfang Liu

Applied Physics A· Volume 115· Issue 1
Publisher page

Abstract

FeCoP nanocrystalline films were successfully electrodeposited on the Cu film coated silicon substrate in the bath containing Fe2+, Co2+, as well as different concentration H2PO− ions ranging from 0.001 mol/L to 0.01 mol/L. And then the samples experienced magnetic heat treatment with different heating rates. Effects of H2PO− concentration and magnetic heat treatment on morphological, structural, and magnetic properties of the films were investigated by scanning electron microscopy, X-ray diffraction, vibrating sample magnetometer, and vector network analyzer. The results suggest that the as-deposited films do not exhibit obvious in-plane uniaxial magnetic anisotropy, and interestingly after magnetic heat treatment at heating rate of 6 °C/min, the FeCoP films will possess better in-plane uniaxial magnetic anisotropy. It has been obtained that morphology and grain size play important roles in determining magnetic properties. The magnetic performance of FeCoP films with different phosphorus content can be improved by appropriate magnetic heat treatment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic properties of thin films · Metallic Glasses and Amorphous Alloys · Magnetic Properties and Synthesis of Ferrites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. G. Herzer, J. Magn. Magn. Mater. 157–158, 133–136 (1996)10.1016/0304-8853(95)01126-9 ↗
2. T. Osaka, Electrochim. Acta 45, 3311–3321 (2000)10.1016/S0013-4686(00)00407-2 ↗
3. R.H. Yu, L. Ren, S. Basu, K.M. Unruh, A. Parvizi-Majidi, J.Q. Xiao, J. Appl. Phys. 87, 5840–5842 (2000)10.1063/1.372540 ↗
4. K.S.I. Fergen, A.v.d. Weth, A. Schüppen, J. Magn. Magn. Mater. 242–245, 146–151 (2002)10.1016/S0304-8853(01)01185-4 ↗
5. K. Sundaram, V. Dhanasekaran, T. Mahalingam, Ionics 17, 835–842 (2011)10.1007/s11581-011-0580-0 ↗
6. D. Zhou, M. Zhou, M. Zhu, X. Yang, M. Yue, J. Appl. Phys. 111, 07A319 (2012)
7. I. Tabakovic, V. Inturi, S. Riemer, J. Electrochem. Soc. 149, C18–C22 (2002)10.1149/1.1421346 ↗
8. E.X. Feng, Z.K. Wang, X.Q. Zhu, Q.F. Liu, J.B. Wang, J. Electrochem. Soc. 159, H842–H845 (2012)10.1149/2.004211jes ↗
9. E.E. Kalu, J. Solid State Electrochem. 11, 1145–1156 (2007)10.1007/s10008-006-0252-6 ↗
10. C.A.C. Souza, J.E. May, A.T. Machado, A.L.R. Tachard, E.D. Bidoia, Surf. Coat. Technol. 190, 75–82 (2005)10.1016/j.surfcoat.2004.04.070 ↗
11. J.L. Fu, Z.J. Yan, Y. Xu, X.L. Fan, D.S. Xue, J. Phys. Chem. Solids 68, 2221–2226 (2007)10.1016/j.jpcs.2007.06.023 ↗
12. J.M. Barandiará, J. Herreros, A. García-Arribas, J. Non-Cryst. Solids 201, 102–109 (1996)10.1016/0022-3093(96)00139-1 ↗
13. Y. Shen, X.C. Zheng, G.P. Zheng, Metall. Mater. Trans. A 42, 211–218 (2010)10.1007/s11661-010-0437-6 ↗
14. W.Q. Huang, G.F. Huang, B. Liang, C.L. Xie, J. Magn. Magn. Mater. 321, 1177–1181 (2009)10.1016/j.jmmm.2008.10.028 ↗
15. R.L. Wang, S.L. Tang, Y.G. Shi, X.L. Fei, B. Nie, Y.W. Du, J. Appl. Phys. 103, 07D507 (2008)
16. L. Vlad, A.V. Sandu, V. Georgescu, J. Supercond. Nov. Magn. 25, 469–474 (2011)10.1007/s10948-011-1301-7 ↗
17. B. Soulestin, O. Castelein, J.P. Bonnet, P. Blanchart, Ceram. Int. 27, 517–522 (2001)10.1016/S0272-8842(00)00110-3 ↗
18. C.W.B. Bezerra, L. Zhang, H. Liu, K. Lee, A.L.B. Marques, E.P. Marques, H.J. Wang, J.J. Zhang, J. Power Sources 173, 891–908 (2007)10.1016/j.jpowsour.2007.08.028 ↗
19. C.Y. Tsay, K.S. Fan, S.H. Chen, C.H. Tsai, J. Alloys Compd. 495, 126–130 (2010)10.1016/j.jallcom.2010.01.100 ↗
20. E.T. Ferguson, J. Appl. Phys. 29, 252–253 (1958)10.1063/1.1723093 ↗
21. U. Holzwarth, N. Gibson, Nanotechnology 6, 534 (2011)
22. V. Ganesh, D. Vijayaraghavan, V. Lakshminarayanan, Appl. Surf. Sci. 240, 286–295 (2005)10.1016/j.apsusc.2004.06.139 ↗
23. H. Kockar, M. Alper, T. Sahin, O. Karaagac, J. Magn. Magn. Mater. 322, 1095–1097 (2010)10.1016/j.jmmm.2009.10.058 ↗
24. M.H. Seo, D.J. Kim, J.S. Kim, Thin Solid Films 489, 122–129 (2005)10.1016/j.tsf.2005.05.011 ↗
25. R. Angelucci, P. Negrini, S. Solmi, Appl. Phys. Lett. 49, 1468–1470 (1986)10.1063/1.97305 ↗
26. V. Bekker, K. Seemann, H. Leiste, J. Magn. Magn. Mater. 270, 327–332 (2004)10.1016/j.jmmm.2003.08.033 ↗
27. D.S. Xue, F.S. Li, X.L. Fan, F.S. Wen, Chin. Phys. Lett. 25, 4120–4123 (2008)10.1088/0256-307X/25/11/077 ↗
28. T.L. Gilbert, IEEE Trans. Magn. 40, 3443–3449 (2004)10.1109/TMAG.2004.836740 ↗