Y-junction carbon nanotubes, grown through thermal pyrolysis of acetylene over nanocrystalline Ni-P deposited SiC whiskers, were investigated by transmission electron microscopy. The pyrolysis temperature, which ranged from 800 °C to 1000 °C, was found to be crucial for the growth of different Y-junction carbon nanotubes. At pyrolysis temperatures below the partial melting point of the Ni-P alloy catalyst, only single-junction nanotubes could be synthesized. Whereas, due to partial melting of the alloy catalyst at higher pyrolysis temperatures, liquid-assisted growth of multiple Y-junction nanotubes could occur.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Carbon Nanotubes in Composites · Silicon Carbide Semiconductor Technologies · Graphene research and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. M. Menon, D. Srivastava: Phys. Rev. Lett. 79, 4453 (1997)10.1103/PhysRevLett.79.4453 ↗
2. A.N. Andriotis, M. Menon, D. Srivastava, L. Chernozatonskii: Phys. Rev. B 65, 165416 (2002)10.1103/PhysRevB.65.165416 ↗
3. C. Papadopoulos, A. Rakitin, J. Li, A.S. Vedeneev, J.M. Xu: Phys. Rev. Lett. 85, 3476 (2000)10.1103/PhysRevLett.85.3476 ↗
4. P. Nagy, R. Ehlich, L.P. Biró, J. Gyulai: Appl. Phys. A 70, 481 (2000)10.1007/s003390051072 ↗
5. B. C Satishkumar, P.J. Thomas, A. Govindaraj: C.N.R. Rao: Appl. Phys. Lett. 77, 2530 (2000)
6. D. Zhou, S. Seraphin: Chem. Phys. Lett. 238, 286 (1995)10.1016/0009-2614(95)00406-T ↗
7. J. Li, C. Papadopoulos, J. Xu: Nature 402, 254 (1999)10.1038/46509 ↗
8. B. Gan, J. Ahn, Q. Zhang, Rusli, S.F. Yoon, J. Yu, Q.-F. Huang, K. Chew, V.A. Ligatchev, X.-B. Zhang, W.-Z. Li: Chem. Phys. Lett. 333, 23 (2001)10.1016/S0009-2614(00)01336-1 ↗
9. H.W. Zhu, L.J. Ci, C.L. Xu, J. Liang, D.H. Wu: Diamond Relat. Mater. 11, 1349 (2002)10.1016/S0925-9635(01)00745-2 ↗
10. W.Z. Li, J.G. Wen, Z.F. Ren: Appl. Phys. Lett. 79, 1879 (2001)10.1063/1.1404400 ↗
11. F.L. Deepak, A. Govindaraj, C.N.R. Rao: Chem. Phys. Lett. 345, 5 (2001)10.1016/S0009-2614(01)00849-1 ↗
12. M. Terrones, M.F. Banhart, N. Grobert, J.-C. Charlier, H. Terrones, P.M. Ajayan: Phys. Rev. Lett. 89, 75505 (2002)10.1103/PhysRevLett.89.075505 ↗
13. D. Srivastava, M. Menon, P.M. Ajayan: J. Nanoparticle Res. 5, 395 (2003)10.1023/A:1025579730847 ↗
14. D.Y. Ding, J.N. Wang, Z.L. Cao, J.H. Dai, F. Yu: Chem. Phys. Lett. 371, 333 (2003)10.1016/S0009-2614(03)00292-6 ↗
15. K.L. Lin, Y.L. Chang, C.C. Huang, F.I. Li, J.C. Hsu: Appl. Surf. Sci. 181, 166 (2001)10.1016/S0169-4332(01)00387-7 ↗
16. K. Lu, J.T. Wang, W.D. Wei: J. Phys. D 25, 808 (1992)10.1088/0022-3727/25/5/010 ↗
17. T.B. Massalski: Binary Phase Diagrams (American Society for Metals, Metals Park 1986)
18. H.X. Li, W.J. Wang, H. Li, J.F. Deng: J. Catal. 194, 211 (2000)10.1006/jcat.2000.2944 ↗
19. E.F. Kukovitsky, S. G. L’vov, N.A. Sainov, V.A. Shustov, L.A. Chernozatonskii: Chem. Phys. Lett. 355, 497 (2002)10.1016/S0009-2614(02)00283-X ↗
20. E.F. Kukovitsky, S. G. L’vov, N.A. Sainov: Chem. Phys. Lett. 317, 65 (2000)10.1016/S0009-2614(99)01299-3 ↗
21. S.H. Tsai, C.T. Siu, W.J. Jong, H.C. Shih: Carbon 38, 1899 (2000)10.1016/S0008-6223(00)00150-0 ↗