Selected Physical and Mechanical Properties of Microwave Heat Treated Rubberwood (Hevea brasiliensis)
Source abstract
Abstract
The objectives of this study were to evaluate some of physical and mechanical properties of rubberwood (Hevea brasiliensis) as function of microwave heat treatment process. The specimens were heat treated at three temperature levels of 150 °C, 180 °C, and 220 °C for 20 min in a small microwave oven connected to a computer. Bending characteristics, namely modulus of elasticity (MOE), modulus of rupture (MOR) as well as hardness of the samples were tested. Dimensional stability in the form of swelling and water absorption of the specimens were also determined. Based on the findings in this work it appears that microwave can be used successfully for heat treatment of rubberwood. Overall mechanical properties of the samples were adversely influenced by the treatment. MOE, MOR and hardness values of the samples treated at a temperature of 220 °C had 2.37, 3.69, and 2.12 times reduced than those of control samples, respectively. Dimensional stability of the heat treated samples as a result of 2-h and 24-h water soaking improved. Micrographs take from scanning electron microscope (SEM) and transmission electron microscope (TEM) revealed that certain amount of damage took place in the cellwall of the treated specimens. Overall discoloration on the samples due to microwave heat treatment was found insignificant.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Plant Pathogens and Fungal Diseases · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Science and Industrial Technology, Prince of Songkla University, Surat Thani Campus, Surat Thani 84000, Thailand;aujchariya.c@psu.ac.th (A.C.)
Faculty of Wood Engineering, Transilvania University of Brasov, Universitatii Street, 1, 500068 Brasov, Romania
Department of Natural Resource Ecology & Management, Oklahoma State University, Stillwater, OK 74078-6013, USA
References (32)
Show source-provided references
1. Changes in the chemical structure of thermally treated wood10.15376/biores.5.3.1936-1944 ↗
2. Pore size diameter, shrinkage and specific gravity evolution during the heat treatment of wood
3. Shear strength of heat-treated solid wood bonded with polyvinyl-acetate reinforced by nanowollastonite10.37763/wr.1336-4561/65.2.183194 ↗
4. Effect of thermal treatment on the chemical composition and mechanical properties of birch and aspen10.15376/biores.3.2.517-537 ↗
5. Control of wood thermal and its effects on decay resistance: A review10.1007/s13595-016-0541-x ↗
6. Mechanical and chemical behavior of spruce wood modified by heat10.1016/j.buildenv.2005.07.017 ↗
7. Effect of high temperature treatment on the mechanical properties of birch10.1007/s00226-006-0082-9 ↗
8. Chemical analysis of heat treated softwoods10.1007/s00107-005-0078-4 ↗
9. Hiziroglu, S. (2019). Fundamental aspects of heat treated wood. Fact Sheet, 2. Available online: www.fapc.biz.
10. Bonding strength of heat treated compressed Eastern redcedar wood10.1016/j.matdes.2012.05.050 ↗
11. Mechanical behaviour of Québec wood species heat-treated using ThermoWood process10.1007/s00107-007-0173-9 ↗
12. Effects of heat treatment and surface roughness on bonding strength10.1016/j.conbuildmat.2012.01.008 ↗
13. Wood modification by heat treatment: A review10.15376/biores.4.1.Esteves ↗
14. The effects of heat treatment on technological properties in red-bud maple (Acer trautvetteri Medw.) wood10.1016/j.biortech.2007.04.021 ↗
15. Mechanical behaviour of Eucalyptus wood modified by heat10.1007/s002260050006 ↗
16. Hill, C. (2006). Wood Modification: Chemical, Thermal and Other Processes, John Wiley & Sons, Ltd.10.1002/0470021748 ↗
17. Properties of some thermally modified wood.species10.1016/j.matdes.2012.06.054 ↗
18. Properties of thermally treated yellow poplar, Southern pine, and Eastern redcedar10.15376/biores.13.4.7726-7737 ↗
19. Effect of high temperature on the change in dimensional stability and mechanical properties of spruce wood10.1515/HF.2003.080 ↗
20. Strength properties of thermally modified softwoods and its relation to polymeric structural wood constituents10.1051/forest:2007048 ↗
21. Effect of heat treatment on the mechanical properties of North American Jack pine: Thermogravimetric study10.1007/s10853-009-3985-7 ↗
22. González-Peña, M., Breese, M., and Hill, C. (2004, January 22–24). Hygroscopicity in heat-treated wood: Effect of extractives. Proceedings of the International Conference on Environmentally Compatible Forest Products (ICECFOP), Oporto, Portugal.
23. Microwave wood modification technology and its.applications
24. High-intensity microwave wood modification for increasing permeability
25. Microwave Pretreatment of Backsawn Messmate Boards to Improve Drying Quality: Part 110.1080/07373930801944770 ↗
26. Effect of heat treatment on the machining and other properties of rubberwood. European10.1007/s00107-011-0587-2 ↗
27. Assessment of the properties, utilization, and preservation of rubberwood (Hevea brasiliensis): A case study in Malaysia10.1007/s10086-011-1173-2 ↗
28. ASTM D 143–14 (2010). Standard Test Methods for Small Clear Specimens of Timber, Street.
29. Characterization of heat treated wood species10.1016/j.matdes.2012.12.067 ↗
30. Measurement of dimensional stability of heat treated southern red oak (Quercus falcata Michx.)10.1016/j.measurement.2016.02.064 ↗
31. Dimensional stability and color change of heat treated young teak wood10.1080/20426445.2019.1679430 ↗
32. Dimensional stability of wood through warm pressure treatment10.1007/BF02608498 ↗