journal article·2017-09-15Open access

Study on the High Temperature Interfacial Stability of Ti/Mo/Yb0.3Co4Sb12 Thermoelectric Joints

Ming Gu, Shengqiang Bai, Xugui Xia, Xiangyang Huang, Xiaoya Li, Xun Shi, Lidong Chen

Applied Sciences· Volume 7· Issue 9

Abstract

To improve the interfacial stability at high temperatures, n-type skutterudite (SKD) thermoelectric joints with sandwich structures of Ti/Mo/Yb0.3Co4Sb12 were successfully designed and fabricated. In this structure, Mo and Ti were introduced as the barrier layer with the goal of suppressing the interfacial diffusion and the buffer layer with the goal of enhancing the bonding strength, respectively. To evaluate the high temperature interfacial behavior of the Ti/Mo/Yb0.3Co4Sb12 joints, thermal shocking between 0 °C and 600 °C and isothermal aging at a temperature range of 550 °C to 650 °C were carried out in vacuum. During the isothermal aging process, Ti penetrates across the Mo layer, and finally diffuses into the Yb0.3Co4Sb12 matrix. By increasing the isothermal aging time, Ti continuously diffuses and reacts with the elements of Sb and Co in the matrix, consequently forming the multilayer-structured intermetallic compounds of Ti3Sb/Ti2Sb/TiCoSb. Diffusion kinetics was investigated and it was found that the interfacial evolution of the Ti/Mo/Yb0.3Co4Sb12 joints was a diffusion-controlling process. During the diffusion process, the formed Mo-Ti buffer layer acts as a damper, which greatly decelerates the diffusion of Ti towards the Yb0.3Co4Sb12 matrix at high temperatures. Meanwhile, it was found that the increase in the contact resistivity of the joints mainly derives from the inter-diffusion between Ti and Yb0.3Co4Sb12. As a result, the Ti/Mo/Yb0.3Co4Sb12 joint demonstrates the excellent stability of the interfacial contact resistivity. Service life prediction was made based on the stability of the contact resistivity, and it was found that the Ti/Mo/Yb0.3Co4Sb12 joint is qualified for practical applications at 550 °C.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Thermoelectric Materials and Devices · Intermetallics and Advanced Alloy Properties · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050, China

References (39)

Show source-provided references
1. High efficiency segmented thermoelectric unicouple for operation between 973 and 300 K10.1016/S0196-8904(02)00109-7 ↗
2. Thierry Caillat, Efficient segmented thermoelectric unicouples for space power applications
3. Skutterudites: Thermoelectric Materials for Automotive Applications?10.1007/s11664-009-1005-y ↗
4. Optimization of thermoelectric components for automobile waste heat recovery systems10.1007/s11664-015-3912-4 ↗
5. Silk fabric-based wearable thermoelectric generator for energy harvesting from the human body10.1016/j.apenergy.2015.11.038 ↗
6. Physical, mechanical and structural properties of highly efficient nanostructured n- and p- silicides for practical thermoelectric applications10.1007/s11664-013-2848-9 ↗
7. Enhanced thermoelectric figure-of-merit in nanostructured p-type silicon germanium bulk alloys10.1021/nl8026795 ↗
8. Enhanced thermoelectric figure of merit in nanostructured n-type silicon germanium bulk alloy10.1063/1.3027060 ↗
9. Microstructure and Thermoelectric Properties of p-type Si80Ge20B0.6-SiC Nanocomposite
10. Effects of microstructural evolution effects on the thermoelectric properties of spark plasma sintered Ti0.3Zr0.35Hf0.35NiSn half-Heusler compound10.1007/s11664-012-2249-5 ↗
11. Morpholoical effects on the thermoelectric properties of Ti0.3Zr0.35Hf0.35Ni1+δSn alloys following phase separation
12. Bonding of Bi2Te3 based thermoelectric legs to metallic contacts using Bi0.82Sb0.18 alloy10.1007/s11664-015-4003-2 ↗
13. Thermoelectric properties of Bi0.5Sb1.5Te3/Ag2Te bulk composites with size- and shape-controlled Ag2Te nano-particles dispersion10.1016/j.jallcom.2015.10.160 ↗
14. Enhancement in thermoelectric figure of merit in nanostructured Bi2Te3 with semimetal nanoinclusions10.1002/aenm.201100338 ↗
15. Enhanced thermoelectric performance of n-type PbTe bulk materials fabricated by semisolid powder processing10.1016/j.jallcom.2014.04.116 ↗
16. High thermoelectric properties of PbTe-Sm2Se3 composites10.1016/j.scriptamat.2015.09.036 ↗
17. Pb1−xSnxTe Alloys—Application Considerations10.1007/s11664-010-1435-6 ↗
18. Phase morphology effects on the thermoelectric properties of Pb0.25Sn0.25Ge0.5Te10.1016/j.actamat.2012.11.027 ↗
19. Structural evolution following spinodal decomposition of the pseudo-ternary compound (Pb0.3Sn0.1Ge0.6)Te10.1007/s11664-009-0980-3 ↗
20. Hazan, E., Ben-Yehuda, O., Madar, N., and Gelbstein, Y. (2015). Functional graded germanium-lead chalcogenides-based thermoelectric module for renewable energy applications. Adv. Energy Mater., 5.10.1002/aenm.201500272 ↗
21. Chen, L., Backhaus-Ricoult, M., He, L., Li, X., Xia, X., and Zhao, D. (2012). Fabrication Method for Thermoelectric Device. (US8198116 B2), U.S. Patent.
22. Enhanced Thermoelectric Properties of BaxEuyCo4Sb12 with Very High Filling Fraction10.3724/SP.J.1077.2012.12615 ↗
23. Skutterudite unicouple characterization for energy harvesting applications10.1002/aenm.201200503 ↗
24. A thermoelectric generator based on an n-type clathrate and a p-type skutterudite unicouple10.1002/pssa.201300218 ↗
25. Conversion efficiency of skutterudite-based thermoelectric modules10.1039/C4CP01582G ↗
26. Interface Structure and Electrical Property of Yb0.3Co4Sb12/Mo-Cu Element Prepared by Welding Using Ag-Cu-Zn Solder10.15541/jim20140378 ↗
27. Joining of Mo to CoSb3 by spark plasma sintering by inserting a Ti interlayer10.1016/j.matlet.2004.07.041 ↗
28. Interfacial evolution behavior and reliability evaluation of CoSb3/Ti/Mo-Cu thermoelectric joints during accelerated thermal aging10.1016/j.jallcom.2008.10.037 ↗
29. High temperature reliability evaluation of CoSb3/electrode thermoelectric joints10.1016/j.intermet.2008.10.010 ↗
30. Microstructural evolution of the interfacial layer in the Ti-Al/Yb0.6Co4Sb12 thermoelectric joints at high temperature10.1016/j.jallcom.2014.05.087 ↗
31. Fabrication and reliability evaluation of Yb0.3Co4Sb12/Mo–Ti/Mo–Cu/Ni thermoelectric joints10.1016/j.ceramint.2015.02.083 ↗
32. Power-Generation Characteristics After Vibration and Thermal Stresses of Thermoelectric Unicouples with CoSb3/Ti/Mo(Cu) Interfaces10.1007/s11664-015-3694-8 ↗
33. Synthesis and thermoelectric properties of Sr-filled skutterudite SryCo4Sb1210.1063/1.2172705 ↗
34. Study on the interfacial stability of p-type Ti/CeyFexCo4−xSb12 thermoelectric joints at high temperature10.1016/j.jallcom.2016.02.041 ↗
35. PLANSEE (2017, August 22). Available online: https://www.plansee.com/en/materials/molybdenum.html.
36. Thermal Expansion of Copper from 20 to 800 K—Standard Reference Material 73610.1063/1.1658614 ↗
37. Density and Thermal Expansion of High Purity Nickel over the Temperature Range from 150 K to 2030 K10.1007/s10765-015-1839-x ↗
38. The growth and roughness evolution of intermetallic compounds of Sn–Ag–Cu/Cu interface during soldering reaction10.1016/j.jallcom.2007.04.047 ↗
39. Study of interfacial reactions in Sn–3.5Ag–3.0Bi and Sn–8.0Zn–3.0Bi sandwich structure solder joint with Ni(P)/Cu metallization on Cu substrate10.1016/j.jallcom.2006.07.121 ↗