Passivating oxidation behavior of Ti0.12Al0.21B0.67 coatings investigated by scanning transmission electron microscopy and chemical environment dependent density functional theory simulations

Sebastian Lellig, Amir Hossein Navidi Kashani, Peter Schweizer, Marcus Hans, Ganesh K. Nayak, Johann Michler, Jochen M. Schneider

Acta Materialia· Volume 285

Abstract

The oxidation behavior of stoichiometric Ti 0.12 Al 0.21 B 0.67 coatings is investigated by scanning transmission electron microscopy (STEM) after oxidizing for 1, 4 and 8 h at 700 °C and at 800 and 900 °C. In the as deposited state, a ∼4 nm thick, native, amorphous oxide layer covers the surface of the coating, while the magnitude of incorporated O along the column boundaries decreases with depth. During oxidation, the formation of scale layers consisting predominantly of Al, O and B is observed, that appear to be amorphous at 700 °C, while after oxidation at 900 °C for 8 h, a (nano-)crystalline aluminoborate layer forms. Concurrently, within the unoxidized coating, the formation of Al- and Ti-rich boride regions, consistent with spinodal decomposition, is observed. Chemical environment dependent density functional theory (DFT) predictions of the energies required for mass transport on the metal sublattice indicate that Al diffusion is initiated before Ti diffusion. Hence, as the temperature is increased, the migration of Al is initiated first, leading to the formation of the oxide scale observed already after oxidation at 700 °C for 1 h. Below the oxidized region, the formation of Al-rich and Ti-rich regions by spinodal decomposition require the concurrent migration of Al and Ti. The fact that decomposition takes place at 900 °C and hence at larger temperatures than the Al diffusion mediated scale formation is consistent with DFT predictions as the average values of the predicted energies required for both, vacancy formation and migration for Ti, are larger than for Al.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Material properties of titanium diboride10.6028/jres.105.057 ↗
2. Evaluation of TiB2 coatings in sliding contact against aluminium10.1016/S0257-8972(01)01361-5 ↗
3. Corrosion resistance of nanostructured TiB2 films in 3% NACl solution10.1007/s11106-010-9218-4 ↗
4. Mechanical properties and microstructure of TiB2–TiC composite ceramic cutting tool material10.1016/j.ijrmhm.2012.02.011 ↗
5. A numerical approach to the heat transfer in monolithic and SiC reinforced HfB2, ZrB2 and TiB2 ceramic cutting tools10.1016/j.ceramint.2019.05.095 ↗
6. The study of radius end mills with TiB2 coating when milling a nickel alloy10.3390/ma16062535 ↗
7. Shaw · 2005
8. Hypervelocity impact of TiB2-based composites as front bumpers for space shield applications10.1016/j.matdes.2016.02.126 ↗
9. Ballistic studies on TiB 2-Ti functionally graded armor ceramics10.14429/dsj.62.2666 ↗
10. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
11. Self-organized nanocolumnar structure in superhard TiB 2 thin films10.1063/1.1887824 ↗
12. Thermal stability and self-arrangement of nanocrystalline hard coatings
13. Evaluation of magnetron-sputtered TiB2 intended for tribological applications10.1016/S0257-8972(99)00638-6 ↗
14. Microstructure-driven strengthening of TiB2 coatings deposited by pulsed magnetron sputtering10.1016/j.surfcoat.2019.04.042 ↗
15. Wettable TiB2 cathode for aluminum electrolysis: a review10.1007/s40831-022-00526-8 ↗
16. Research progress in TiB 2 wettable cathode for aluminum reduction10.1007/s11837-008-0104-1 ↗
17. Use of TiB2 cathode material: demonstrated energy conservation in VSS cells
18. High-temperature wetting and interfacial interaction between liquid Al and TiB 2 ceramic10.1007/s10853-015-8814-6 ↗
19. Anti-corrosion and conductivity of titanium diboride coating on metallic bipolar plates10.1016/j.corsci.2020.108646 ↗
20. The corrosion behaviour of titanium diboride in neutral chloride solution10.1016/S0010-938X(00)00120-7 ↗
21. Microstructure and corrosion resistance of TC2 Ti alloy by laser cladding with Ti/TiC/TiB2 powders10.1016/j.apsusc.2015.04.030 ↗
22. Unmasking the anomalous rapid oxidation of refractory TiB2 at low temperatures10.1016/j.jeurceramsoc.2021.04.011 ↗
23. Revisiting the origins of super-hardness in TiB2+z thin films – Impact of growth conditions and anisotropy10.1016/j.surfcoat.2022.128806 ↗
24. Oxidation of monolithic TiB2 and of Al2O3-TiB2 composite10.1007/BF01151240 ↗
25. Improving the high-temperature oxidation resistance of TiB2 thin films by alloying with Al10.1016/j.actamat.2020.07.025 ↗
26. High-temperature oxidation of titanium diboride of different purity10.1007/BF01061928 ↗
27. Navidi Kashani · 2022
28. Oxidation resistance and mechanical properties of sputter-deposited Ti0. 9Al0. 1B2-y thin films10.1016/j.surfcoat.2022.128187 ↗
29. Effect of aluminium ion implantation on the oxidation resistance of DC magnetron sputter-deposited TiB2 thin films10.1016/j.surfcoat.2003.06.027 ↗
30. Microstructure of Al-containing magnetron sputtered TiB2 thin films10.1016/j.tsf.2019.06.011 ↗
31. Influence of the Al concentration in Ti-Al-B coatings on microstructure and mechanical properties using combinatorial sputtering from a segmented TiB2/AlB2 target10.1016/j.surfcoat.2019.02.060 ↗
32. Age hardening in (Ti1-xAlx) B2+ Delta thin films10.1016/j.scriptamat.2016.09.021 ↗
33. Morphology, mechanical properties, and oxidation behavior of stoichiometric Ti0.33-xAlxB0.67 coatings (x = 0.04, 0.15, 0.21, and 0.28)10.1016/j.actamat.2024.119829 ↗
34. Probing the onset of wurtzite phase formation in (V, Al) N thin films by transmission electron microscopy and atom probe tomography10.1016/j.surfcoat.2022.128235 ↗
35. On correlations between local chemistry, distortions and kinetics in high entropy nitrides: an ab initio study10.1016/j.actamat.2023.118951 ↗
36. Three-dimensional atom mapping of dopants in Si nanostructures10.1063/1.2005368 ↗
37. Electronic properties of random alloys: special quasirandom structures10.1103/PhysRevB.42.9622 ↗
38. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
39. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
40. Restoring the density-gradient expansion for exchange in solids and surfaces10.1103/PhysRevLett.100.136406 ↗
41. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
42. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
43. High-precision sampling for Brillouin-zone integration in metals10.1103/PhysRevB.40.3616 ↗
44. Optimization methods for finding minimum energy paths10.1063/1.2841941 ↗
45. Pressure- and temperature-dependent diffusion from first-principles: a case study of V and Ti in a TiN matrix10.1016/j.surfcoat.2021.127491 ↗
46. Gottstein · 2004
47. Structure of diborides of titanium, zirconium, columbium, tantalum and vanadium10.1007/BF03398932 ↗
48. Sokolova · 1978
49. The preparation of aluminum diboride, AlB2110.1021/ja01604a003 ↗
50. Structures and transformation mechanisms of the η, γ and θ transition aluminas10.1107/S0108768191002719 ↗
51. Crystal structure of κ-alumina: an X-ray powder diffraction, TEM and NMR study10.1039/a700054e ↗
52. Temporally-resolved decomposition of Ti0. 12Al0. 21B0. 67 thin films at 1000°C10.1016/j.surfcoat.2024.131026 ↗